| Category | Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Geon™ Vinyl Rigid Extrusion L7005 Polyvinyl Chloride, Rigid (PVC, Rigid).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.46 g/cc | 1.46 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 80 | 80 | 15 sec; ASTM D2240 |
| Tensile Strength, Yield | 43.2 MPa | 6270 psi | Type I, 5.1 mm/min; ASTM D638 |
| Tensile Modulus | 2.85 GPa | 413 ksi | Type I, 5.1 mm/min; ASTM D638 |
| Flexural Strength | 84.8 MPa | 12300 psi | ASTM D790 |
| Flexural Modulus | 2.96 GPa | 429 ksi | ASTM D790 |
| Izod Impact, Notched | 5.90 J/cm <br>@Thickness 3.18 mm,<br> Temperature 23.0 °C |
11.1 ft-lb/in <br>@Thickness 0.125 in,<br> Temperature 73.4 °F |
Compression Molded; ASTM D256A |
| Dart Drop Total Energy | 73.4 J/cm <br>@Temperature 23.0 °C |
0.138 ft-lb/mil <br>@Temperature 73.4 °F |
Procedure A, C.125; ASTM D4226 |
| >= 178 J/cm <br>@Temperature 23.0 °C |
>= 0.333 ft-lb/mil <br>@Temperature 73.4 °F |
Procedure B, C.125; ASTM D4226 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 64.0 µm/m-°C | 35.6 µin/in-°F | ASTM D696 |
| Deflection Temperature at 0.46 MPa (66 psi) | 73.9 °C <br>@Treatment Temp. 50.0 °C,<br> Thickness 3.18 mm |
165 °F <br>@Treatment Temp. 122 °F,<br> Thickness 0.125 in |
Annealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 71.1 °C <br>@Thickness 3.18 mm |
160 °F <br>@Thickness 0.125 in |
Compression Molded, Annealed at 50 deg.C; ASTM D648 |
| 74.4 °C <br>@Thickness 3.18 mm |
166 °F <br>@Thickness 0.125 in |
Compression Molded, Annealed at 60 deg.C; ASTM D648 | |
| Flammability, UL94 | V-0 <br>@Thickness 0.749 mm |
V-0 <br>@Thickness 0.0295 in |
ALL; UL 94 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 182 - 193 °C | 360 - 379 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Ease of Sizing | Acceptable | |
| Features | Good Impact Resistance | |
| Good Weather Resistance | ||
| Forms | Cube | |
| Generic Material | PVC, Rigid | |
| Generic Name | Polyvinyl Chloride, Rigid (PVC, Rigid) | |
| Processing Method | Extrusion | |
| PVC Cell Classification | 1-42434-33 | ASTM D4216 |
| 15354 | ASTM D1784 | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Outdoor Applications | |
| Profiles | ||
| Windows & Doors |