Westlake EF418 Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Westlake Chemical Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake EF418 Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
WESTLAKE polyethylene EF418 is a LDPE formula with excellent optical properties suggested by light and medium duty packaging.Application/UsesLight and medium duty produce bagsClarity packagingGeneral purpose packagingFDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All information provided by Westlake Chemical
Physical Properties Metric English Comments
Density 0.9235 g/cc
0.03336 lb/in³
ASTM D1505
Thickness 31.8 microns
1.25 mil
Melt Flow 1.25 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.25 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 250 %
250 %
ASTM D882
Film Elongation at Break, TD 650 %
650 %
ASTM D882
Dart Drop 4.33 g/micron
110 g/mil
ASTM D1709
Film Tensile Strength at Break, MD 26.2 MPa
3800 psi
ASTM D882
Film Tensile Strength at Break, TD 18.6 MPa
2700 psi
ASTM D882
1% Secant Modulus, MD 207 MPa
30000 psi
ASTM D882
1% Secant Modulus, TD 241 MPa
35000 psi
ASTM D882
Optical Properties Metric English Comments
Haze 5.0 %
5.0 %
ASTM D1003
Gloss 70 %
70 %
at 45º; ASTM D2457
Processing Properties Metric English Comments
Melt Temperature 182 - 199 °C
360 - 390 °F
with BUR of 1.5:1 or higher
Blow-up Ratio (BUR) 2.5
2.5
Descriptive Properties Value Comments
Process Film