Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 204 - 315 °C | 399 - 599 °F | Recommended oven temperature |
NOVA Chemicals Novapol® TR-0535-UI Hexene MDPE Rotational Molding Resin TR-0530-UI complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. TR-0530-UI is su.. |
|||
Melt Temperature | 204 - 315 °C | 399 - 599 °F | |
NOVA Chemicals Novapol® TR-0535-U Hexene MDPE Rotational Molding Resin
(discontinued **) Molded Plaque Properties. Features: Hexene Copolymer, excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer. |
|||
Melt Temperature | 170 - 315 °C | 338 - 599 °F | Average value: 231 °C Grade Count:7 |
Overview of materials for Medium Density Polyethylene (MDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Molded". Each property range of values reported is minimum and maxim.. |
|||
Melt Temperature | 70.0 - 315 °C | 158 - 599 °F | Average value: 290 °C Grade Count:33 |
Overview of materials for Nylon 66, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Melt Temperature | 295 - 315 °C | 563 - 599 °F | Injection Molding |
LG Chemical LUPOY SC2202 PC+GF20%, High Impact Description: Injection Molding, PC+GF20%, Good Toughness, Good Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical |
|||
Melt Temperature | 295 - 315 °C | 563 - 599 °F | |
Lavergne VYTEEN PCGF10BK PC 10% Glass Reinforced Vyteen PCGF10BK is a 10% fiberglass reinforced general purpose Polycarbonate grade.Features: - Good processabilityTypical Applications: - Laptop computer docking - Laser printer gear - Toner car.. |
|||
Melt Temperature | 290 - 315 °C | 554 - 599 °F | |
Styron EMERGEâ„¢ 4202-15 MFR Polycarbonate EMERGEâ„¢ PC 4202-15 advanced resin is 20% glass reinforced polycarbonate containing mold release for optimal processing. This resin exhibits high modulus and excellent dimensional stability. A.. |
|||
Melt Temperature | 290 - 315 °C | 554 - 599 °F | |
Styron EMERGEâ„¢ 4202-8 MFR Polycarbonate EMERGEâ„¢ PC 4202-8 advanced resin is 20% glass reinforced polycarbonate containing mold release for optimal processing. This resin exhibits high modulus and excellent dimensional stability. Ap.. |
|||
Melt Temperature | 260 - 315 °C | 500 - 599 °F | flat die equipment |
DuPont Nucrel® 0609HSA Ethylene-Methacrylic Acid Copolymer Resin for Film and Extrusion Coating/Laminating 6.5 wt% Methacrylic Acid.Nucrel® 0609HSA is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment.. |
|||
Melt Temperature | 260 - 315 °C | 500 - 599 °F | flat die equipment |
DuPont Nucrel® 407 Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating 4 wt% Methacrylic Acid.Nucrel® 0407 is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment desi.. |
|||
Melt Temperature | 270 - 315 °C | 518 - 599 °F | |
Ecomass® 3011ZD86 Tungsten Filled Polycarbonate Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsHigh Specific GravityTungsten Filled Polycarbonate (PC) CompoundGood ToughnessInformation provided by Tech.. |
|||
Melt Temperature | 288 - 315 °C | 550 - 599 °F | Extrusion Coating Processability |
Dow AFFINITY™ PT 1450G1 Ethylene alpha-olefin resin AFFINITY™ PT 1450G1 Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. The resin is for monolayer and co-extrusion coating that offers excellent low temperature seal initiation, ult.. |
|||
Melt Temperature | 204 - 315 °C | 399 - 599 °F | Varies with the mold shape and construction. Oven will also affect process time. |
NOVA Chemicals Sclair® TD-7915-U Hexene MDPE Rotational Molding Resin
(discontinued **) Excellent low temperature impact properties, Excellent ESCR, Wide process window, NSF listing for Stds. 14, 24, and 61 pending, Retention of impact at long cook timesApplications: IBCs, Toys, Genera.. |
|||
Melt Temperature | 131 - 315 °C | 268 - 599 °F | Average value: 208 °C Grade Count:13 |
Overview of materials for Medium Density Polyethylene (MDPE), Rotational Molded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Rotational Molded". Each property range of values reported is minimu.. |
|||
Melt Temperature | 175 - 315 °C | 347 - 599 °F | Average value: 220 °C Grade Count:9 |
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Film Grade". Each property range of values reported is minimum and m.. |
|||
Melt Temperature | 220 - 315 °C | 428 - 599 °F | Average value: 278 °C Grade Count:8 |
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Coating Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Coating Grade". Each property range of values reported is minimum an.. |
|||
Melt Temperature | 204 - 315 °C | 399 - 599 °F | |
NOVA Chemicals Novapol® TR-0535-UG Hexene MDPE Rotational Molding Resin
(discontinued **) Molded Plaque Properties. Features: excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer. |
|||
Melt Temperature | 204 - 315 °C | 399 - 599 °F | |
NOVA Chemicals Novapol® PR-0636-U Butene MDPE Rotational Molding Resin
(discontinued **) Very good processability, Very good ESCR, Good impact properties, NSF listed for Stds. 14, 24, and 61Applications: Toys, General purpose custom molding, Carts, Playground equipmentAdditives: Process.. |
|||
Melt Temperature | 260 - 315 °C | 500 - 599 °F | flat die equipment |
DuPont Nucrel® 0609HS Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating
(discontinue 6 wt% Methacrylic Acid.Nucrel® 0609HS* (High-Speed) is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminatin.. |