Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 200 - 235 °C | 392 - 455 °F | |
SABIC F04660 High Density Polyethylene for Blown Film Applications Product Description: F04660 is a homopolymer HDPE film grade with excellent processability and high stiffness. It has good moisture barrier properties and can be blended with LDPE and LLDPE to imp.. |
|||
Melt Temperature | 200 - 235 °C | 392 - 455 °F | |
SABIC FJ00952 High Density Polyethylene for Blown Film Product Description: FJ00952 is a TNPP additive free, high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, .. |
|||
Melt Temperature | 225 - 235 °C | 437 - 455 °F | Extrusion |
DuPont Performance Polymers Hytrel® HTR8730 BK320 TPC-ET
(Unverified Data**) Hytrel® HTR8730 BK320 is a high viscosity thermoplastic polyester elastomer designed for blow molding. It has excellent mechanical properties at elevated temperatures and very good resistance to mo.. |
|||
Melt Temperature | 225 - 235 °C | 437 - 455 °F | |
NOVA Chemicals Sclair® 14B3 Butene LMDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, good clarity, heat resistance and barrier properties.Applications: Lamination, co-extrusion.Data provided by the manufacturer. |
|||
Melt Temperature | 205 - 235 °C | 401 - 455 °F | Injection Molding |
LG Chemical KEYFLEX BT 3038D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Melt Temperature | 220 - 235 °C | 428 - 455 °F | Recommended for Injection |
Kolon DIAMAT® EH Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Melt Temperature | 220 - 235 °C | 428 - 455 °F | Recommended for Injection |
Kolon DIAMAT® IH Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Melt Temperature | 220 - 235 °C | 428 - 455 °F | |
Lavergne VYTEEN ABS 2904 Acrylonitrile Butadiene Styrene Vyteen ABS 2904 is a black recycled ABS high impact flow terpolymer with balanced impact/stiffness properties designed for injection molding applications.Features: -Excellent resilience -Good proc.. |
|||
Melt Temperature | 225 - 235 °C | 437 - 455 °F | |
Borealis Borcoat™ BB700E-7032 Polypropylene Compound for Steel Pipe Coating Applications Borcoat BB700E-7032 is a grey colored high impact polypropylene. This product is especially designed for direct extrusion of syntactic PP with high thermal insulations capacity and high compression.. |
|||
Melt Temperature | 225 - 235 °C | 437 - 455 °F | |
Borealis Borcoat™ GA700E-7032 Syntactic Polypropylene for Steel Pipe Coating Borcoat GA700E-7032 is a grey colored syntactic, high impact polypropylene with high thermal insulation capacity and high compressive strength.Borcoat GA700E-7032 is recommended as thermal insulatio.. |
|||
Melt Temperature | 225 - 235 °C | 437 - 455 °F | |
Covestro Desmopan® 481 Polyurethane injection molding gradefree from plasticizersgrease and oil-resistantlow compression sethigh elasticitygood heat resistanceEasy releaseApplicationRoller coatingSealsmembranesAutomotive engineeringPr.. |
|||
Melt Temperature | 215 - 235 °C | 419 - 455 °F | |
Covestro Desmopan® DP 3660DU Polyurethane Extrusion- and injection molding gradetransparent up to 6 mm wall thicknesshydrolysis-stabilisedwith special UV stabilizerswith release agentgood wear resistanceApplicationSports shoe solesHosesnon-.. |
|||
Melt Temperature | 210 - 235 °C | 410 - 455 °F | Extrusion Coating |
DuPont™ Appeel® 11D888 Ethylene Vinyl Acetate Appeel®11D888 is a developmental modified ethylene vinyl acetate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a .. |
|||
Melt Temperature | 185 - 235 °C | 365 - 455 °F | Cast Film/Sheet Processing |
DuPont™ Appeel® 72D811 Sealing Resin DuPont™ Appeel® 72D811 resin is designed to be a sealing layer to film or sheet lidding applications. It provides a peelable seal to a number of materials including HDPE, LLDPE, LDPE, EVA, and Ion.. |
|||
Melt Temperature | 210 - 235 °C | 410 - 455 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 21E533 Anhydride Modified Ethylene Acrylate BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i.. |
|||
Melt Temperature | 210 - 235 °C | 410 - 455 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 21E781 Anhydride Modified Ethylene Acrylate BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i.. |
|||
Melt Temperature | 210 - 235 °C | 410 - 455 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 21E810 Anhydride Modified Ethylene Acrylate BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester that allows them to be functional in high temperature coextrusions. They are avail.. |
|||
Melt Temperature | 210 - 235 °C | 410 - 455 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 21E830 Anhydride Modified Ethylene Acrylate BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i.. |
|||
Melt Temperature | 210 - 235 °C | 410 - 455 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 22E804 Modified Ethylene Acrylate BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f.. |
|||
Melt Temperature | 210 - 235 °C | 410 - 455 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 41E710 Anhydride Modified LLDPE BYNEL® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Melt Temperature | 210 - 235 °C | 410 - 455 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 41E865 Anhydride Modified LLDPE BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext.. |
|||
Melt Temperature | 210 - 235 °C | 410 - 455 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 41E871 Anhydride Modified LLDPE BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext.. |
|||
Melt Temperature | 210 - 235 °C | 410 - 455 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 50E662 Anhydride Modified Polypropylene BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen.. |
|||
Melt Temperature | 210 - 235 °C | 410 - 455 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 50E739 Anhydride Modified Polypropylene BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen.. |
|||
Melt Temperature | 185 - 235 °C | 365 - 455 °F | Extrusion Coating |
DuPont™ Elvaloy® AC 15024S Ethylene Methyl Acrylate Elvaloy® AC 15024S is a copolymer of ethylene and methyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins. Elvaloy®.. |
|||
Melt Temperature | 225 - 235 °C | 437 - 455 °F | |
NOVA Chemicals Sclair® 14B1 Butene LMDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, good clarity, heat resistance and barrier properties.Applications: Lamination, co-extrusion.Data provided by the manufacturer. |