Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 188 - 204 °C | 370 - 399 °F | |
PolyOne Geon™ Vinyl Rigid Extrusion 87350 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Melt Temperature | 199 - 204 °C | 390 - 399 °F | |
PolyOne Geon™ Vinyl Rigid Molding M4885 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Melt Temperature | 199 - 204 °C | 390 - 399 °F | |
PolyOne Geon™ Vinyl Rigid Molding MR200 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Melt Temperature | 199 - 204 °C | 390 - 399 °F | |
PolyOne Geon™ Vinyl Rigid Molding MR201 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Melt Temperature | 163 - 204 °C | 325 - 399 °F | |
PolyOne Gravi-Tech™ GRV-TE1-060-W-NAT Styrene Isoprene Styrene Block Copolymer (SIS) Information provided by PolyOne |
|||
Melt Temperature | 199 - 204 °C | 390 - 399 °F | |
PolyOne Novablend™ 6602 Polyvinyl Chloride, Rigid (PVC, Rigid) Novablend 6602 is a rigid, opaque PVC for molding compounds. This product has high impact, excellent indoor/outdoor weathering, high flow, and good processing characteristics.Applications includes: .. |
|||
Melt Temperature | 182 - 204 °C | 360 - 399 °F | |
PolyOne Versaflex™ HC MT222 Thermoplastic Elastomer (TPE) Versaflex™ HC MT222 is an exceptionally clear, high performance TPE developed for medical tubing for healthcare. Versaflex™ HC MT222 has been specially formulated without the use of any plasticize.. |
|||
Melt Temperature | 182 - 204 °C | 360 - 399 °F | |
PolyOne Versaflex™ HC MT317 Thermoplastic Elastomer (TPE) Versaflex™ HC MT317 is an extrudable, sterilizable TPE developed for medical tubing applications in healthcare. - Autoclavable sterilizable - Flexible - Kink Resistant New product. Commercial speci.. |
|||
Melt Temperature | 193 - 204 °C | 379 - 399 °F | |
PolyOne Versaflex™ HC MT555 Thermoplastic Elastomer (TPE) Versaflex™ HC MT555 is an easy processing material designed for applications where FDA compliance and medical testing is required. - Excellent Colorability - Soft TouchRear: 340 - 360F Center: 380 .. |
|||
Melt Temperature | 191 - 204 °C | 376 - 399 °F | |
PolyOne Geon™ Vinyl Dry Blend E6530 Polyvinyl Chloride, Rigid (PVC, Rigid) Interior application for thick & thin gauge profile application.Information provided by PolyOne |
|||
Melt Temperature | 193 - 204 °C | 379 - 399 °F | |
PolyOne Geon™ Vinyl Flexible A4D02 Polyvinyl Chloride, Flexible (PVC, Flexible) A flexible transparent PVC Compound designed primarily for indoor mats.Information provided by PolyOne |
|||
Melt Temperature | 193 - 204 °C | 379 - 399 °F | |
PolyOne Geon™ Vinyl Flexible A5DM0 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Melt Temperature | 193 - 204 °C | 379 - 399 °F | |
PolyOne Geon™ Vinyl Flexible B6D00 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 193 - 204 °C | 379 - 399 °F | |
PolyOne Geon™ Vinyl Flexible B9WF1 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 193 - 204 °C | 379 - 399 °F | |
PolyOne Geon™ Vinyl Flexible R132BE Polyvinyl Chloride + NBR (PVC+NBR) Information provided by PolyOne |
|||
Melt Temperature | 193 - 204 °C | 379 - 399 °F | |
PolyOne Geon™ Vinyl Flexible R8570A Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 193 - 204 °C | 379 - 399 °F | |
PolyOne Geon™ Vinyl Flexible R999A Black Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 193 - 204 °C | 379 - 399 °F | |
PolyOne Geon™ Vinyl Flexible A80U0 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Melt Temperature | 193 - 204 °C | 379 - 399 °F | |
PolyOne Geon™ Vinyl Flexible B9000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 193 - 204 °C | 379 - 399 °F | |
PolyOne Geon™ Vinyl Flexible P512 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 193 - 204 °C | 379 - 399 °F | |
PolyOne Geon™ Vinyl Flexible R279AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 193 - 204 °C | 379 - 399 °F | |
PolyOne Geon™ Vinyl Flexible R352AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 193 - 204 °C | 379 - 399 °F | |
Huntsman PE1753 EVA Film Extrusion
(discontinued **) 7.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Yields film with good clarity and excellent impact strength.Applications: Film extrusion: icebags, liquid packaging, lamination film, and .. |
|||
Melt Temperature | 188 - 204 °C | 370 - 399 °F | Molding |
Lubrizol Estane® 2103-80AEN Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: NSF Standard 61 certified, FDA complianceAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane produ.. |
|||
Melt Temperature | 188 - 204 °C | 370 - 399 °F | Molding |
Lubrizol Estane® 2103-80PF Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Film and profile resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in.. |
|||
Melt Temperature | 188 - 204 °C | 370 - 399 °F | Extrusion |
Lubrizol Estane® 2103-90AEFH Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Film resin for injection blow moldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product .. |
|||
Melt Temperature | 193 - 204 °C | 379 - 399 °F | |
PolyOne Geon™ Vinyl Flexible R350AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 190 - 204 °C | 374 - 399 °F | |
Huntsman PE1201 EVA Film Extrusion
(discontinued **) 2% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Good optical, medium impact strength, and good processability.Applications: Film extrusion: heavy duty packaging.FDA Notes: Conforms to FDA .. |
|||
Melt Temperature | 163 - 204 °C | 325 - 399 °F | |
PolyOne Gravi-Tech™ GRV-TP-050-CU-NAT Styrene Butadiene Block Copolymer (SBC) Information provided by PolyOne |