Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 370 - 395 °C | 698 - 743 °F | |
Parker Chomerics PREMIER™ PEI-140 High Temperature Conductive Plastic for EMI Shielding PEI-140 can provide up to a 65% cost reduction by eliminating secondary operations such as assembly, machining, painting/plating and the logistics that accompany these processes. The shielding effec.. |
|||
Melt Temperature | 370 - 390 °C | 698 - 734 °F | |
LATI LARPEEK 10 G/50 50% Glass Reinforced Polyetheretherketone (PEEK)
(Unverified Data**) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Melt Temperature | 370 - 390 °C | 698 - 734 °F | |
LATI LARPEEK 10 K/40 40% Carbon Fiber Reinforced Polyetheretherketone (PEEK)
(Unverified Data**) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Melt Temperature | 370 - 390 °C | 698 - 734 °F | |
LATI LARPEEK 50 G/30 30% Glass Reinforced Polyetheretherketone (PEEK)
(Unverified Data**) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Melt Temperature | 370 - 395 °C | 698 - 743 °F | |
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical chemic.. |
|||
Melt Temperature | 370 - 416 °C | 698 - 780 °F | Average value: 392 °C Grade Count:5 |
Overview of materials for Thermoplastic Polyimide, Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyimide, Carbon Fiber". Each property range of values reported is minimum and maximum va.. |
|||
Melt Temperature | 370 - 400 °C | 698 - 752 °F | |
LATI Larpeek 10 G/50 PEEK, 50% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Melt Temperature | 370 - 400 °C | 698 - 752 °F | |
LATI Larpeek 10 K/30 PEEK, 30% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Melt Temperature | 370 - 400 °C | 698 - 752 °F | |
LATI Larpeek 10 K/40 PEEK, 40% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Melt Temperature | 370 - 400 °C | 698 - 752 °F | |
LATI Larpeek 50 G/30 PEEK, 30% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Melt Temperature | 370 - 400 °C | 698 - 752 °F | |
LATI Larpeek 50 K/30 PEEK, 30% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Melt Temperature | 370 - 400 °C | 698 - 752 °F | |
LATI Larpeek 10 G/15 PEEK, 15% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Melt Temperature | 370 - 400 °C | 698 - 752 °F | |
LATI Larpeek 10 G/30 PEEK, 30% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Melt Temperature | 370 - 400 °C | 698 - 752 °F | |
LATI Larpeek 10 G/40 PEEK, 40% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Melt Temperature | 370 - 400 °C | 698 - 752 °F | |
LATI Larpeek 10 G/60 PEEK, 60% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Melt Temperature | 370 - 400 °C | 698 - 752 °F | |
LATI Larpeek 10 K/20 PEEK, 20% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Melt Temperature | 370 - 400 °C | 698 - 752 °F | |
LATI Larpeek 10 K/40 HM PEEK, 40% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af.. |
|||
Melt Temperature | 370 - 395 °C | 698 - 743 °F | |
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK), 40% Glass Fiber AvaSpire® AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical ch.. |
|||
Melt Temperature | 370 °C | 698 °F | Optimal |
BASF Ultrason® E 2010 C6 30% Carbon Filled Carbon fibers and Ultrason® two partners with good properties. The combination of carbon fibers with the amorphous high-temperature plastic Ultrason® guarantees mechanical properties for temperatu.. |
|||
Melt Temperature | 370 °C | 698 °F | Optimal |
BASF Ultrason® E 2010 G4 MR SW 15102 20% Glass Filled PESU Information provided by BASF |
|||
Melt Temperature | 370 °C | 698 °F | Optimal |
BASF Ultrason® E 3010 MR UN PESU Description: Unreinforced, higher viscosity injection molding and extrusion grade with improved toughness and chemical resistance (stress crack resistance); demolding optimized. Abbreviated designat.. |
|||
Melt Temperature | 370 °C | 698 °F | Optimal |
BASF Ultrason® P 3010 MR SW 10101 PPSU Description: Unreinforced, higher viscosity injection molding grade, flame retardant and with improved chemical resistance. This grade is black colored and demolding optimized. Abbreviated designati.. |
|||
Melt Temperature | 370 °C | 698 °F | Optimal |
BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE Description: Compound based on PES with 30 % filler. The filler system, a mixture of carbon fibers, graphite and PTFE powder, considerably improves Ultrason’s tribological properties. In addition, .. |
|||
Melt Temperature | 370 - 390 °C | 698 - 734 °F | |
LATI LARPEEK 50 G/20 20% Glass Reinforced Polyetheretherketone (PEEK)
(discontinued **) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Melt Temperature | 370 - 400 °C | 698 - 752 °F | |
LATI Latilub 88/10-15T G/30 PEEK, 30% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyetheretherketone (PEEK). PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Melt Temperature | 370 - 400 °C | 698 - 752 °F | |
LATI Latilub 88/10-15T K/30 PEEK, 30% Carbon Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyetheretherketone (PEEK). PTFE. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Melt Temperature | 370 - 400 °C | 698 - 752 °F | |
LATI Latilub 88/50-20GRT K/10 PEEK, 10% Carbon Fiber Reinforced, Graphite/PTFE Filled Self-lubricating product based on Polyetheretherketone (PEEK). Graphite / PTFE. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provid.. |