Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 249 - 271 °C | 480 - 520 °F | |
PolyOne Versaflex™ OM 6059-9 Thermoplastic Elastomer (TPE) Versaflex™ OM 6059-9 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except.. |
|||
Melt Temperature | 249 - 260 °C | 480 - 500 °F | ASTM D789 |
Niche Polymer PA66MIN Nylon 66, Medium Impact Information provided by Niche Polymer |
|||
Melt Temperature | 249 - 268 °C | 480 - 515 °F | |
Polymer Resources NY6-G13 Nylon 6, 13% Glass Reinforced Nylon 6, 13% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Melt Temperature | 249 - 288 °C | 480 - 550 °F | |
Huntsman PE5080 Extrusion Coating Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Excellent draw down, low neck-in, and excellent adhesion.Applications: Extrusion: coating grade and thin coatings.FDA Notes: Conforms to FDA regulation 21 CFR.. |
|||
Melt Temperature | 249 - 260 °C | 480 - 500 °F | |
Firestone CLM200-001 Nylon 6 Used for monofiliament extrusion. Natural color. Not heat stabilized or modified. Lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone |
|||
Melt Temperature | 249 - 260 °C | 480 - 500 °F | |
MTI ThermoStran® PP-40G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Melt Temperature | 249 - 271 °C | 480 - 520 °F | |
Eastman Eastar 5011 Copolyester Eastar Copolyester 5011 is a glycol modified polyethylene terephthalate(PET). The modification is made by adding a second glycol, cyclohexanedimethanol (CHDM) during the polymerization stages. The s.. |
|||
Melt Temperature | 249 - 271 °C | 480 - 520 °F | |
Eastman Eastar GN120 Copolyester Applications:AppliancesConsumer electronicsPersonal care and cosmeticsStationary suppliesKey Attributes:High clarity and transparencyHigh flow copolyesterToughProduct Description: Eastar GN120 Cop.. |
|||
Melt Temperature | 249 - 277 °C | 480 - 530 °F | |
Clariant Renol 60G33HSL Nylon 6, 33% Glass Fiber Reinforced, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Melt Temperature | 249 - 282 °C | 480 - 540 °F | |
Clariant Renol BR2065 Nylon 66, Mineral/Glass Reinforced Data provided by Clariant Masterbatches |
|||
Melt Temperature | 249 - 277 °C | 480 - 530 °F | |
Clariant Renol PA233HT Nylon 6, Improved Processability, Easily Colorable, Highly Toughened Data provided by Clariant Masterbatches |
|||
Melt Temperature | 249 - 277 °C | 480 - 530 °F | |
Clariant Renol R60G33HSL Nylon 6, 33% Glass Fiber, Heat Stabilized, Lubricated, Economy Data provided by Clariant Masterbatches |
|||
Melt Temperature | 249 - 288 °C | 480 - 550 °F | |
Ecomass® 705ZD70 Tungsten Filled ABS Nontoxic Alternative to Lead (Pb) for radiation shielding applicationsHigh specific GravityTungsten Filled ABS compoundRigidGood ToughnessInformation provided by Technical Polymers |