Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eastman Eastar GN120 Copolyester

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer Eastman Chemical
Trade Name Eastar
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman Eastar GN120 Copolyester.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Applications:AppliancesConsumer electronicsPersonal care and cosmeticsStationary suppliesKey Attributes:High clarity and transparencyHigh flow copolyesterToughProduct Description: Eastar GN120 Copolyester is a high flow product and contains a mold release. Other outstanding features of Eastar GN120 are easily maintained such as excellent appearance and clarity, good physical properties, chemical resistance, and easy processing. Eastar GN120 is for sale only in Asia as a high-flow formulation.Information provided by Eastman.
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 107
107
ASTM D785
Tensile Strength at Break 24.0 MPa
3480 psi
ASTM D638
Tensile Strength, Yield 48.0 MPa
6960 psi
ASTM D638
Elongation at Break 75 %
75 %
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Flexural Strength 66.0 MPa
9570 psi
ASTM D790
Flexural Modulus 1.90 GPa
276 ksi
ASTM D790
Izod Impact, Notched 0.460 J/cm

@Temperature -40.0 °C
0.862 ft-lb/in

@Temperature -40.0 °F
ASTM D256
0.840 J/cm

@Temperature 23.0 °C
1.57 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ASTM D4812
NB

@Temperature -40.0 °C
NB

@Temperature -40.0 °F
ASTM D4812
Puncture Energy 35.0 J

@Temperature 23.0 °C
25.8 ft-lb

@Temperature 73.4 °F
At Max load; ASTM D3763
44.0 J

@Temperature -40.0 °C
32.5 ft-lb

@Temperature -40.0 °F
At Max load; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 68.0 °C
154 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ASTM D648
Optical Properties Metric English Comments
Haze 0.40 %
0.40 %
ASTM D1003
Transmission, Visible 91 %
91 %
Total; ASTM D1003
Processing Properties Metric English Comments
Melt Temperature 249 - 271 °C
480 - 520 °F
Mold Temperature 16.0 - 38.0 °C
60.8 - 100 °F
Drying Temperature 71.0 °C
160 °F
Dry Time 6 hour
6 hour