Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 246 - 274 °C | 475 - 525 °F | |
Polymer Resources PC/ABS-FR1 Flame Retardant PC/ABS Alloy PC/ABS Alloy, Flame Retardant, Standard FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided.. |
|||
Melt Temperature | 246 - 274 °C | 475 - 525 °F | |
Polymer Resources PC/ABS-FR1-[color]-3 PC Blend, Flame Retardant, Standard Flow, UV Stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Temperature | 246 - 274 °C | 475 - 525 °F | |
Polymer Resources PC/ABS-FR1-[color]-WR Flame Retardant PC/ABS Alloy, Wear Resistant PC/ABS Alloy, Flame Retardant, Standard Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Info.. |
|||
Melt Temperature | 246 - 274 °C | 475 - 525 °F | |
Polymer Resources PC/ABS-FR2 Flame Retardant PC/ABS Alloy, High Flow PC/ABS Alloy, Flame Retardant, Higher FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b.. |
|||
Melt Temperature | 246 - 274 °C | 475 - 525 °F | |
Polymer Resources PC/TP-FR2 Flame Retardant PC/Polyester Alloy Flame Retardant, High Impact, Excellent Chemical ResistanceFeatures: • Flame Retardant • Impact Modified • Self Extinguishing • Good Chemical ResistanceProcess: Injection MoldingNotes: All p.. |
|||
Melt Temperature | 246 - 274 °C | 475 - 525 °F | |
Polymer Resources PC/TP-GP1-HF PC/Polyester Alloy, High Melt Flow High Melt Flow, Good Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by .. |
|||
Melt Temperature | 246 - 274 °C | 475 - 525 °F | |
Polymer Resources PC/TP-GP1-UV PC/Polyester Alloy, UV-stabilized High Impact, Good Chemical Resistance, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Melt Temperature | 246 - 274 °C | 475 - 525 °F | |
Polymer Resources PC/TP-GP2 PC/Polyester Alloy High Impact, Excellent Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b.. |
|||
Melt Temperature | 246 - 274 °C | 475 - 525 °F | |
Polymer Resources PPX-FR1 Modified-PPO, V-0 Flame Retardant Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Melt Temperature | 246 - 274 °C | 475 - 525 °F | |
Polymer Resources PPX-FR1-[color]EN Modified PPO, UL 94 V-0 with HDT of 190 F, Extrusion Grade Process: ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Temperature | 246 - 274 °C | 475 - 525 °F | |
Polymer Resources PPX-FR4 Modified-PPO, V-1 Flame Retardant Modified-Polyphenylene Oxide, V-1 Flame Retardant, 185F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Melt Temperature | 246 - 282 °C | 475 - 540 °F | |
Polymer Resources PPX-MF-FR1 Modified-PPO, V-0 Flame Retardant, Mineral Reinforced Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDT, Mineral ReinforcedFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mecha.. |
|||
Melt Temperature | 246 - 274 °C | 475 - 525 °F | |
Polymer Resources TP-FR IM2 PBT, Impact Modified, Flame Retardant, High Flow Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Temperature | 246 - 274 °C | 475 - 525 °F | |
Polymer Resources TP-FR-IM2 Polybutylene Terephthalate, Impact Modified, Flame Retardant, High Flow Polybutylene Terephthalate, Impact Modified, Flame Retardant, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Melt Temperature | 246 - 279 °C | 475 - 535 °F | |
PTS PCA-30G11-(V) UV Stabilized, Glass Reinforced PC/PBT Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 246 - 274 °C | 475 - 525 °F | |
Polymer Resources PC/TP-GP1 PC/Polyester Alloy High Impact, Good Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Pol.. |
|||
Melt Temperature | 246 - 288 °C | 475 - 550 °F | |
PTS PCA-2010NHV Non-Bromine, Non-Chlorine, Flame Retardant UV PC/ABS Alloy This is a non-halogenated flame retardant, UV stabilized grade. Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 246 - 277 °C | 475 - 531 °F | Average value: 262 °C Grade Count:5 |
Overview of materials for Polycarbonate/Styrenic Alloy This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Styrenic Alloy". Each property range of values reported is minimum and maximum values of a.. |
|||
Melt Temperature | 246 - 260 °C | 475 - 500 °F | |
LyondellBasell Petrothene® KR92828 High Density Polyethylene ApplicationsPETROTHENE KR 92828 is a high molecular weight, high density polyethylene-based compound designed for use in jacketing, conduit or wire insulation. KR 92828 contains a carbon black cont.. |
|||
Melt Temperature | 246 - 274 °C | 475 - 525 °F | Injection Molding |
Ineos ABS Lustran® 633 ABS, Injection Molding Grade Lustran® ABS 633 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It offers a good balance of physical properties, high gloss, and good moldability. Typical .. |
|||
Melt Temperature | 246 - 274 °C | 475 - 525 °F | Injection Molding |
Ineos ABS Lustran® ABS 349 Lustran® ABS 349 is a high-gloss, medium-impact injection molding resin that has been specially formulated for excellent surface lubricity using internal additives. |
|||
Melt Temperature | 246 - 260 °C | 475 - 500 °F | ISO 294 |
Gromax BTE90-DN001N1 Nylon 6 (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 246 - 260 °C | 475 - 500 °F | |
LyondellBasell Petrothene® LR590001 High Density Polyethylene ApplicationsPETROTHENE LR590001 is designed as primary insulation for telephone singles. LR590001 is a high density resin designed for low shrinkback after extrusion. Antioxidant has been added to e.. |
|||
Melt Temperature | 246 - 288 °C | 475 - 550 °F | |
Star Plastics PC/ABSFR9001 Molding Grade PC/ABSFR Information provided by Star Plastics, Inc. |
|||
Melt Temperature | 246 - 288 °C | 475 - 550 °F | |
Star Plastics PC/ABSQX7002 Molding Grade PC/ABS High Flow Information provided by Star Plastics, Inc. |
|||
Melt Temperature | 246 - 302 °C | 475 - 575 °F | |
Calsak CS-72 General Purpose ABS Resin Product Characteristics:High Impact, High GlossInjection molding grade |
|||
Melt Temperature | 246 - 302 °C | 475 - 575 °F | |
Calsak CS-72L General Purpose ABS Resin Product Characteristics:High Impact, High GlossInjection molding grade |
|||
Melt Temperature | 246 °C | 475 °F | |
Chem Polymer Chemlon 206 G Nylon 6, 6% Glass Fiber Reinforced A 6% glass fiber reinforced nylon 6 offering improved creep resistance, stiffness, tensile and dimensional stability over unmodified nylon 6 materials.Data provided by the manufacturer, Chem Polymer.. |
|||
Melt Temperature | 246 °C | 475 °F | |
Chem Polymer Chemlon 218 GV Nylon 6, 18% Glass Reinforced A flame retardant, glass reinforced grade of nylon 6. The material is UL94 V0 rated, completely non-halogenated and phosphorus free. It gives excellent surface appearance and is available in a ran.. |
|||
Melt Temperature | 246 °C | 475 °F | Injection |
Albis Plastics Cellulose Acetate Butyrate B9424-3 , 3% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |