Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 180 - 220 °C | 356 - 428 °F | |
PolyOne OnFlex™ S EF 50A-3S1965 Thermoplastic Elastomer (TPE) OnFlex™-S EF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver good mechanical properties together with excell.. |
|||
Melt Temperature | 180 - 220 °C | 356 - 428 °F | |
PolyOne OnFlex™ S EF 80A-3S1977 Thermoplastic Elastomer (TPE) OnFlex™-S EF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver good mechanical properties together with excell.. |
|||
Melt Temperature | 180 - 220 °C | 356 - 428 °F | |
NOVA Chemicals Novapol® HB-W952-A HDPE Extrusion Resin Molded Plaque Properties. Features: High molecular weight, excellent ESCR, impact strength, high rigidity.Applications: large-part blow-molding, trash cans, drums, jerry cans, fuel tanks.Data provi.. |
|||
Melt Temperature | 180 - 220 °C | 356 - 428 °F | |
Polykemi AB POLYfill PPH 30030DNH Polypropylene Homopolymer, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
Melt Temperature | 180 - 200 °C | 356 - 392 °F | |
Lotte Chemical Titan TITANEX® LF1043 Linear low density polyethylene resin
(discontinued **) LF1043 is a pelleted linear low density polyethylene resin formulated with antioxidant, and antiblock agent. This product is used for blown film extrusion which offers outstanding toughness, extrud.. |
|||
Melt Temperature | 180 - 200 °C | 356 - 392 °F | |
Lotte Chemical Titan TITANEX® LF1051 Linear low density polyethylene Hexene-1 resin
(discontinued **) LF1051 is a pelleted linear low density polyethylene Hexene-1 resin formulated with antioxidant, high antiblock and slip agent. This product is used for blown film extrusion which offers outstandin.. |
|||
Melt Temperature | 180 - 200 °C | 356 - 392 °F | |
LATI LATILUB 73/13-01M Polyoxymethylene Base (POM), 1% Molybdenum Disulfide Self Lubricating Plastic
(Unv Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Melt Temperature | 180 - 200 °C | 356 - 392 °F | |
LATI LATILUB 73/13-10ST Polyoxymethylene Base (POM), 10% Mixed PTFE/Silicone Self Lubricating Plastic
(Un Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Melt Temperature | 180 - 280 °C | 356 - 536 °F | Molding |
Ineos Styrenics 496N High-Impact Polystyrene Resin (NAFTA) Description: High-impact, lower flow grades for food packaging, dairy containers, lids, plates, appliance components and housings.Information provided by BASF.Ineos Styrenics purchased this product .. |
|||
Melt Temperature | 180 - 210 °C | 356 - 410 °F | |
Iran Petrochemical (PCC) LH0075 Low Density Polyethylene LH0075 is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties.Applications: carrier bags, shrink film, industria.. |
|||
Melt Temperature | 180 - 225 °C | 356 - 437 °F | |
Iran Petrochemical (PCC) LL0209AA Linear Low Density Polyethylene LL 0209AA is a LLDPE copolymer with butene as comonomer which contains anti-oxidant. It is recommended for general purpose applications.Information provided by Iran Petrochemical Commercial Co. |
|||
Melt Temperature | 180 - 220 °C | 356 - 428 °F | |
Lotte Chemical Titan TITANEX® HF1881 High density polyethylene Hexene-1 resin HF1881 is a pelleted medium molecular weight, high density polyethylene Hexene-1 resin for tubular film extrusion.Applications: Grocery sacks, shopping bags, liners and thin films.Advantages: Speci.. |
|||
Melt Temperature | 180 - 230 °C | 356 - 446 °F | Extrusion |
Stellarchem AB-860LG TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Melt Temperature | 180 - 280 °C | 356 - 536 °F | Injection Molding |
Styrolution Polystyrol 168 N GR 2 PS Description: Polystyrol 168 N is a high molecular, heat grade used where high strength is required. Suitable for physically or chemically expanded extruded sheet. As blend component with high impact.. |
|||
Melt Temperature | 180 - 250 °C | 356 - 482 °F | Injection |
Styrolution Styrolux® 3G46 SBC Description: Styrolux® 3G 46 is a clear styrene-butadiene copolymer (SBC) developed specifically for sheet- and film extrusion and for thermoformed articles. Styrolux® 3G 46 is designed for im.. |
|||
Melt Temperature | 180 - 210 °C | 356 - 410 °F | |
Styron EMERGEâ„¢ 5710 Acrylonitrile Butadiene Styrene (ABS) EMERGEâ„¢ ABS 5710 advanced resin is an ignition resistant ABS resin with an excellent balance of flow and impact strength. Applications: Monitor Enclosures Surge Protectors and UPS Enclosures .. |
|||
Melt Temperature | 180 - 260 °C | 356 - 500 °F | |
Supreme Petrochem SP6432 9690 Medium Impact Polystyrene Characteristics High flow Good toughness Available in various colors Processing Injection moldingApplications Air conditioner and cooler grills Refrigerator parts Washing machine components Mate.. |
|||
Melt Temperature | 180 °C | 356 °F | Extrusion |
Total Lumicene® mPE M 5220 High Density Polyethylene, Blow Molding Lumicene® mPE M 5220 is a high density polyethylene with outstanding organoleptic properties, stress-cracking resistance and processability.Lumicene® mPE M 5220 is especially suited for the produc.. |
|||
Melt Temperature | 180 °C | 356 °F | |
Carmel Olefins IPETHENE® 113 Low Density Polyethylene IPETHENE® 113 is a general purpose low density polyethylene film extrusion grade. It contains medium level of anti-blocking and slip additives. It is BHT free. It exhibits a good balance between me.. |
|||
Melt Temperature | 180 - 280 °C | 356 - 536 °F | Average value: 231 °C Grade Count:5 |
Overview of materials for Polystyrene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Melt Temperature | 180 - 260 °C | 356 - 500 °F | Average value: 215 °C Grade Count:49 |
Overview of materials for Polypropylene with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in.. |