Material Notes:
OnFlex™-S EF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver good mechanical properties together with excellent processability, in addition to typical OnFlex™-S properties such as a wide hardness range, low compression set, good colourability and a wide temperature operating range. OnFlex™-S EF compounds are semi-filled, making them opaque and with a medium density.Properties are measured using injection molded plaques.Information provided by PolyOne
Physical Properties Metric English Comments
Density 0.980 g/cc
0.0354 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
ISO 868
Tensile Strength at Break 6.30 MPa
914 psi
ISO 37
Tensile Stress 1.50 MPa

@Strain 100 %
218 psi

@Strain 100 %
ISO 37
2.30 MPa

@Strain 300 %
334 psi

@Strain 300 %
ISO 37
Elongation at Break 680 %
680 %
ISO 37
Tear Strength 25.0 kN/m
143 pli
ISO 34-1
Compression Set 15 %

@Temperature 23.0 °C,
Time 259000 sec
15 %

@Temperature 73.4 °F,
Time 72.0 hour
ISO 815
63 %

@Temperature 70.0 °C,
Time 79200 sec
63 %

@Temperature 158 °F,
Time 22.0 hour
ISO 815
95 %

@Temperature 100 °C,
Time 79200 sec
95 %

@Temperature 212 °F,
Time 22.0 hour
ISO 815
Processing Properties Metric English Comments
Melt Temperature 180 - 220 °C
356 - 428 °F
Mold Temperature 30.0 - 60.0 °C
86.0 - 140 °F
Descriptive Properties Value Comments
Features High Flow
Forms Pellets
Generic Material TPE
Generic Material Type Styrenic Thermoplastic Elastomer (TES)
Generic Name Thermoplastic Elastomer (TPE)
Injection Rate Fast
Manufacturer / Supplier GLS Thermoplastic Elastomers
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
RoHS Compliance RoHS Compliant
Uses Appliances
Automotive Applications
Consumer Applications
General Purpose
Industrial Applications
Users viewing this material also viewed the following: