Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 188 - 207 °C | 370 - 405 °F | |
PolyOne Geon™ Vinyl Packaging VEO-111 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Melt Temperature | 199 - 207 °C | 390 - 405 °F | |
PolyOne Geon™ CPVC MC100 Polyvinyl Chloride, Chlorinated (CPVC) Geon MC100 CPVC is an Injection molding fitting compound. It is listed under NSF Std 14 and 61 and meets or exceeds ASTM D-1784 Cell Class 23447. MC100 is designed for CTS applications where enhance.. |
|||
Melt Temperature | 200 - 207 °C | 392 - 405 °F | |
PolyOne Geon™ CPVC MC550 Polyvinyl Chloride, Chlorinated (CPVC) Information provided by PolyOne |
|||
Melt Temperature | 202 - 207 °C | 396 - 405 °F | |
PolyOne Geon™ HTX M6307 Polyvinyl Chloride Alloy (PVC Alloy) Information provided by PolyOne |
|||
Melt Temperature | 196 - 207 °C | 385 - 405 °F | |
PolyOne Geon™ Vinyl Flexible B4D01 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 196 - 207 °C | 385 - 405 °F | |
PolyOne Geon™ Vinyl Flexible B5DU0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 196 - 207 °C | 385 - 405 °F | |
PolyOne Geon™ Vinyl Flexible B5DW2 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 196 - 207 °C | 385 - 405 °F | |
PolyOne Geon™ Vinyl Flexible P502 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 196 - 207 °C | 385 - 405 °F | |
PolyOne Geon™ Vinyl Flexible R5185A Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 196 - 207 °C | 385 - 405 °F | |
PolyOne Geon™ Vinyl Flexible B4DC1 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 196 - 207 °C | 385 - 405 °F | |
PolyOne Geon™ Vinyl Flexible B5D00 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 196 - 207 °C | 385 - 405 °F | |
PolyOne Geon™ Vinyl Flexible B5D01 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 196 - 207 °C | 385 - 405 °F | |
PolyOne Geon™ Vinyl Flexible B5D02 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 196 - 207 °C | 385 - 405 °F | |
PolyOne Geon™ Vinyl Flexible B5D05 Polyvinyl Chloride, Flexible (PVC, Flexible) A flexible PVC Compound, designed primarily for extruded sheet and tile applications.Information provided by PolyOne |
|||
Melt Temperature | 196 - 207 °C | 385 - 405 °F | |
PolyOne Geon™ Vinyl Flexible B5DG1 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 196 - 207 °C | 385 - 405 °F | |
Kleerdex Kydex® IM62 Acrylic/PVC injection Molding Compound
(discontinued **) High impact injection molding compoundApplications: Appliances, office equipment, electrical products, tools, medical equipment, computer equipmentFeatures: IM62 has a Notched Izod impact resistance.. |
|||
Melt Temperature | 196 - 207 °C | 385 - 405 °F | |
Kleerdex Kydex® IM90 Acrylic/PVC injection Molding Compound
(discontinued **) Low heat release aviation gradeApplications: Kydex IM90 is designed for injection molded parts each need to meet the highest flammability requirements of the FAA (FAR 25.853d) for vertical burn, rat.. |
|||
Melt Temperature | 160 - 207 °C | 320 - 405 °F | Average value: 188 °C Grade Count:25 |
Overview of materials for PVC, Transparent This property data is a summary of similar materials in the MatWeb database for the category "PVC, Transparent". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Melt Temperature | 157 - 207 °C | 315 - 405 °F | Average value: 182 °C Grade Count:6 |
Overview of materials for PVC/Acrylic Alloy This property data is a summary of similar materials in the MatWeb database for the category "PVC/Acrylic Alloy". Each property range of values reported is minimum and maximum values of appropriate .. |