Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0080 - 0.012 cm/cm
0.0080 - 0.012 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore D 50
50
ASTM D2240
Tensile Strength at Break 20.0 MPa
2900 psi
510 mm/min; ASTM D638
Tensile Strength 12.4 MPa

@Strain 100 %
1800 psi

@Strain 100 %
510 mm/min; ASTM D638
Elongation at Break 350 %
350 %
510 mm/min; ASTM D638
Tear Strength 84.1 kN/m
480 pli
Die C, 510 mm/min; ASTM D624
Compression Set 45 %

@Temperature 23.0 °C,
Time 79200 sec
45 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
Clash Berg Modulus 0.558 GPa
80.9 ksi
ASTM D1043
0.310 GPa

@Temperature -25.0 °C
45.0 ksi

@Temperature -13.0 °F
ASTM D1043
Thermal Properties Metric English Comments
Brittleness Temperature -27.8 °C
-18.0 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 179 - 185 °C
354 - 365 °F
196 - 207 °C
385 - 405 °F
Descriptive Properties Value Comments
Features Medium Gloss
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Furniture
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved