Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
Plastcom SLOVALEN EH 96 FRD 2 PP, flame retardant FeaturesDetermined for environment, where contact with water is possible, because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machin.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
NOVA Chemicals Novapol® LF-0323-A LDPE Film Resin Film Properties. Features: General purpose clarity, good heat sealing latitude, easy processability, good drawdown.Applications: Food wrap, consumer packaging, liners, blends with LLDPE.Data provid.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
NOVA Chemicals Novapol® LF-Y819-D LDPE Film Resin Film Properties. Features: Good strength and toughness, excellent shrink film characteristics, excellent processability.Applications: Industrial packaging, liners, shrink film, blends with LLDPE.Da.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
LATI LASTIROL R-V2 Polystyrene (PS) (UL94 V-2)
(discontinued **) Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
NOVA Chemicals Novapol® LA-0218-AB LDPE Foam Resin
(discontinued **) Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Specifically designed for foam process, Blends with LLDPEAdditives: Good heat sealing latitude, Moderate toughness, E.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
NOVA Chemicals Novapol® LA-0218-AF LDPE Foam Resin
(discontinued **) Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Specifically designed for foam process, Blends with LLDPEAdditives: Base resinFilm properties are typical of blown fi.. |
|||
Melt Temperature | 175 - 190 °C | 347 - 374 °F | |
Huntsman IROGRAN® A 92 E 4246 Polyester-Based TPU-High Performance Grade Introduction: IROGRAN A 92 E 4246 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e.. |
|||
Melt Temperature | 160 - 190 °C | 320 - 374 °F | |
Lotte Chemical Titan TITANLENE® LDF250YZ Low density polyethylene LDF250YZ is a low density polyethylene resin for film extrusion. LDF250YZ has no slip and anti-block additives. LDF250YZ meets the U.S. Food and Drug Administration (FDA) criteria for food contact u.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
LATI Latigea B01 F1 Bio-Polymer Bio-Polymer (PLA, PHB, ...). Unfilled. Potentially suitable for food/medical contact application. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pr.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
LATI Latilub 37 B01-02S Bio-Polymer Self-lubricating product based on Bio-Polymer (PLA, PHB, ...). Silicone.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Melt Temperature | 160 - 190 °C | 320 - 374 °F | |
Borealis FA5223 Low Density Polyethylene FA5223 is a Low Density Polyethylene for Film Extrusion. Contains antioxidant and antiblock additive. This grade is developed to give strong film for medium duty applications. Applications FA5223.. |
|||
Melt Temperature | 160 - 190 °C | 320 - 374 °F | |
Borealis FA5224 Low Density Polyethylene FA5224 is a Low Density Polyethylene for Film Extrusion. Contains Antioxidant, Anti-block and Medium Slip additives. This grade is developed to give strong film for medium duty applications. Appl.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
Tisan TISOPLEN® 10% Talc Filled Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
Tisan TISOPLEN® 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
Tisan TISOPLEN® 30% Talc Filled Heat Stabilized Homopolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
Tisan TISOPLEN® 40% Calcite Filled Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
Tisan TISOPLEN® 40% Calcite Filled Heat Stabilized Homopolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
Tisan TISOPLEN® 40% Talc Filled Heat Stabilized Homopolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
Tisan TISOPLEN® 30% Calcite Filled Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Melt Temperature | 150 - 190 °C | 302 - 374 °F | Blown Film Coextrusion |
DuPont™ Appeel® 20D875 Ethylene Acrylate Appeel® 20D875 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide strong peelable seals over a broad tempe.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
Tisan TISOPLEN® 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Melt Temperature | 170 - 190 °C | 338 - 374 °F | |
NOVA Chemicals Novapol® LF-0218-AF LDPE Extrusion Resin
(discontinued **) Film Properties. Features: Good heat sealing latitude, moderate toughness, easy processability.Applications: Specifically designed for foam process, blends with LLDPE.Data provided by the manufactu.. |
|||
Melt Temperature | 140 - 190 °C | 284 - 374 °F | |
Polyplastic TechnoTep A® 65 A Thermoplastic Elastomer, Mineral Filled Low mineral filled, good flexibilityInformation provided by PolyPlastic Group. |