Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 300 - 325 °C | 572 - 617 °F | |
LATI LAESTRA E01 G/30 30% Glass Fiber Reinforced, Elastomer Modified Syndiotactic Polystyrene (SPS)
(disconti Description: Laestra compounds are syndiotactic polystyrene (SPS) products. SPS is a polymer offering a combination of properties unavailable with other materials. It exhibits a melting point of 270.. |
|||
Melt Temperature | 300 - 340 °C | 572 - 644 °F | |
LG Chemical LUPOY GN-2151F Halogen Free Modified PC, 15% Glass Fiber Reinforced, Flame Retardant, Green Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Melt Temperature | 300 - 320 °C | 572 - 608 °F | Injection Molding |
LG Chemical LUPOY GP1000L PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, High FlowApplication: IT/OA, E&E Housing and Components Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical |
|||
Melt Temperature | 300 - 340 °C | 572 - 644 °F | Injection Molding |
LG Chemical LUPOY GP2300 PC+GF30%, Heat Resistance Description: Injection Molding, PC+GF30%, General Purpose, Heat ResistanceApplication: IT/OA, E&E Housing and Components, Automotive (Interior)CAS: 103598-77-2 and 65997-17-3Information provided by .. |
|||
Melt Temperature | 300 - 340 °C | 572 - 644 °F | |
LG Chemical LUPOY GP-2401F General Purpose Modified PC, 40% Glass Fiber Reinforced, Flame Retardant Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Melt Temperature | 300 - 340 °C | 572 - 644 °F | Injection Molding |
LG Chemical LUPOY GN2101F PC+GF10%, Halogen Free, Flame Retardant, Heat Resistance Description: Injection Molding, PC+GF10%, Halogen Free Flame Retardant, Heat ResistanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information prov.. |
|||
Melt Temperature | 300 - 320 °C | 572 - 608 °F | Injection Molding |
LG Chemical LUPOY GP1000M PC, Transparent Description: Injection Molding, PC, General Purpose, TransparencyApplication: IT/OA, Electric & Electronic Housing and Components, Automotive Exterior and InteriorCAS: 103598-77-2Information provide.. |
|||
Melt Temperature | <= 300 °C | <= 572 °F | Processing Temperature |
Teknor Apex Beetle® MDF50 Nylon 6, 50% Short Glass Fiber Filler Notes: MDF50 is a 50% glass fiber reinforced nylon 6 that offers excellent mechanical performance coupled with good surface finish Features: Good Surface FinishProcessing Method: Injection molding F.. |
|||
Melt Temperature | 300 - 310 °C | 572 - 590 °F | |
Samyang Trirex® 3025GRU10 Polycarbonate, 10% Glass Reinforced TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Melt Temperature | 300 - 310 °C | 572 - 590 °F | |
Samyang Trirex® 3500G20 Polycarbonate, 20% Glass Reinforced TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Melt Temperature | 300 °C | 572 °F | Injection Molding; ISO 294 |
Covestro Makrolon® 2856 Polycarbonate ISO 7391-PC,MR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 9.5 cm3/10 minFood contact qualityMedium viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAva.. |
|||
Melt Temperature | 300 °C | 572 °F | Injection molding; ISO 294 |
Covestro Makrolon® ET UV110 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• PC/UV absorber concent.. |
|||
Melt Temperature | 300 °C | 572 °F | Injection molding; ISO 294 |
Covestro Makrolon® FU4007 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Furniture applications.. |
|||
Melt Temperature | 300 °C | 572 °F | Injection Molding; ISO 294 |
Covestro Makrolon® LQ3147 Polycarbonate ISO 7391-PC,MLR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minOptical lensHigh viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in clear tints .. |
|||
Melt Temperature | 300 - 330 °C | 572 - 626 °F | |
E-Polymers SEPAZ® V330HS 30% Glass Fiber Reinforced Heat Stabilized PPA Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s.. |
|||
Melt Temperature | 300 °C | 572 °F | Injection Molding; ISO 294 |
Covestro Makrolon® DP1-1825* Polycarbonate, Impact Grade Developmental productISO 7391-PC,MP,(,,)-09-9MVR (300 °C/1.2 kg) 6.0 cm3/10 minImpact modifiedHigh viscosityInjection molding - Melt temperature 280 - 320 °CAvailable in opaque colors onlyPreproce.. |
|||
Melt Temperature | 300 °C | 572 °F | Optimal |
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Conditioned) Description: 50% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness as well as for electric insulating parts.Information provided by BASF |
|||
Melt Temperature | 300 - 330 °C | 572 - 626 °F | |
LATI Latilub 95-25GR CE/10 PSU, Mineral Fiber Reinforced, Graphite Filled Self-lubricating product based on Polysulfone (PSU). Graphite. Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu.. |
|||
Melt Temperature | 300 - 325 °C | 572 - 617 °F | |
LATI LAESTRA G/40 40% Glass Fiber Reinforced Syndiotactic Polystyrene (SPS)
(discontinued **) Description: Laestra compounds are syndiotactic polystyrene (SPS) products. SPS is a polymer offering a combination of properties unavailable with other materials. It exhibits a melting point of 270.. |