Processing Properties Metric English Comments
Melt Temperature 255 - 270 °C
491 - 518 °F
Parker Chomerics PREMIER™ A240-HTHF EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Melt Temperature 255 - 270 °C
491 - 518 °F
Parker Chomerics PREMIER™ A230-FRHF EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Melt Temperature 255 - 270 °C
491 - 518 °F
Parker Chomerics PREMIER™ A230-HTHF EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Melt Temperature 255 - 285 °C
491 - 545 °F
PolyOne Edgetek® ET3500-5001 colored Acrylonitrile Styrene Acrylate + PC (ASA+PC)
The Edgetek™ Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Melt Temperature 255 - 260 °C
491 - 500 °F
Extrusion
LG Chemical AT-553 Transparent ABS, Permanent Antistatic, Natural and Colored Pellets
LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron..
Melt Temperature 255 - 265 °C
491 - 509 °F
Injection Molding
LG Chemical Lupox® SG5150 PBT+PET+GF15%
Description: Injection Molding, PBT+PET+GF15%, Good SurfaceApplication: E&E, Automotive (Door Latch)CAS No. 65997-17-3, 25038-59-9 and 24968-12-5Information provided by LG Chemical
Melt Temperature 255 - 265 °C
491 - 509 °F
Injection Molding
LG Chemical Lupox® SG5200 PBT+PET+GF20%
Description: Injection Molding, PBT+PET+GF20%, Good Surface Application: E&E (Microwave Oven Door Gasket)CAS No. 65997-17-3, 25038-59-9 and 24968-12-5Information provided by LG Chemical
Melt Temperature 255 - 265 °C
491 - 509 °F
Injection Molding
LG Chemical Lupox® SG5300 PBT+PET+GF30%
Description: Injection Molding, PBT+PET+GF30%, Good Surface Application: E&E, Automotive (Switch)CAS No. 65997-17-3, 24968-12-5 and 25038-59-9Information provided by LG Chemical
Melt Temperature 255 - 285 °C
491 - 545 °F
Injection Molding
LG Chemical LUPOY GN1006FT PC, Halogen Free, Flame Retardant
Description: Injection Molding, PC, Halogen Free Flame Retardant, Good FlowApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical
Melt Temperature 255 - 285 °C
491 - 545 °F
Injection Molding
LG Chemical LUPOY HP5004A PC/ABS
Description: Injection Molding, PC/ABS, General Purpose, Good Weld Properties, High Impact (at Low Temperature), Heat ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2, 9003-56-9 and 18102..
Melt Temperature 255 °C
491 °F
LCL-PR29
Intercontinental Polymers 216 PET Polymer Type - Semi-Dull, Polyester Pellets
Applications: UV Block Filament SpecialtiesInformation provided by Intercontinental Polymers.
Melt Temperature 255 °C
491 °F
LCL-PR29
Intercontinental Polymers 728-01 PET Polymer Type - Clear, Polyester Pellets
Applications: Filament YarnInformation provided by Intercontinental Polymers.
Melt Temperature 255 - 260 °C
491 - 500 °F
Extrusion
LG Chemical TR-558 Transparent ABS, Humidity Resistance, Natural and Colored Pellets
LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron..
Melt Temperature 255 °C
491 °F
LCL-PR29
Intercontinental Polymers HoPET 741-01 HoPET Polymer Type - Semi-Dull, Polyester Pellets
Applications: Filament Yarn Information provided by Intercontinental Polymers.
Melt Temperature 255 - 285 °C
491 - 545 °F
Start Point: 265°C
Kingfa CPA-6 Toughened PA6
Features:High impactLow tendency to wrapApplications:Injection moldingSport applianceAutomobile partsPower toolsInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Melt Temperature 255 - 285 °C
491 - 545 °F
Start Point: 265°C
Kingfa PA6-M25G20 20% Glass & 25% Mineral Filled PA6
Features:Low tendency to wrapExcellent size stabilityLow abrasionOutstanding surfaceApplications:Injection moldingAutomobile partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Melt Temperature 255 - 265 °C
491 - 509 °F
Injection Molding
LG Chemical Lupox® SG5500 PBT+PET+GF50%
Description: Injection Molding, PBT+PET+GF50%, Good Surface, High StiffnessApplication: E&E, Automotive (Switch)CAS No. 65997-17-3, 24968-12-5 and 25038-59-9Information provided by LG Chemical
Melt Temperature 255 °C
491 °F
LCL-PR29
Intercontinental Polymers HoPET 720 HoPET Polymer Type - Film Grade Resin, Clear, Polyester Pellets
Applications: FilmInformation provided by Intercontinental Polymers.
Melt Temperature 255 °C
491 °F
LCL-PR29
Intercontinental Polymers HoPET 741-02 HoPET Polymer Type - Semi-Dull, Polyester Pellets
Applications: FiberInformation provided by Intercontinental Polymers.
Melt Temperature 255 - 260 °C
491 - 500 °F
Extrusion
LG Chemical TR-558NS Transparent ABS, Antistatic, Natural and Colored Pellets
LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron..
Melt Temperature 255 - 275 °C
491 - 527 °F
Styron PULSEâ„¢ GX50 PC/ABS Engineering Resin
Overview: PULSE GX50 engineering resins give exceptional impact strength even at low temperature and have sufficient heat resistance for the majority of automotive interior components. This resin pr..
Melt Temperature 255 - 265 °C
491 - 509 °F
Toyobo VYLOPET® EMC307 Injection Molding Polyester Resin, High Cycles
Applications: Coiled bobbinsMouthpiecesFeatures: High cyclesInformation provided by Toyobo.
Melt Temperature 255 - 265 °C
491 - 509 °F
Toyobo VYLOPET® EMC310 Injection Molding Polyester Resin
Applications: Coiled bobbinsMouthpiecesFeatures: High cyclesInformation provided by Toyobo.
Melt Temperature 255 - 265 °C
491 - 509 °F
Toyobo VYLOPET® EMC310TU Injection Molding Polyester Resin, Warpageless, High cycles
Applications: Coiled bobbinsMouthpiecesFeatures: High cyclesWarpagelessInformation provided by Toyobo.
Melt Temperature 255 - 265 °C
491 - 509 °F
Toyobo VYLOPET® EMC317A Injection Molding Polyester Resin, Warpageless
Applications: Iron's heat insulation plateChair framesHousingsFeatures: WarpagelessInformation provided by Toyobo.
Melt Temperature 255 - 270 °C
491 - 518 °F
Toyobo VYLOPET® EMC341 Injection Molding Polyester Resin, Hydrolysis Resistant
Applications: Electric rice cooker partsBathroom appliancesFeatures: Good hydrolysis resistanceInformation provided by Toyobo.
Melt Temperature 255 - 270 °C
491 - 518 °F
Toyobo VYLOPET® EMC545 Injection Molding Polyester Resin, Glass Reinforced
Applications: Auto-partsFeatures: Ultrasonic weldabilityGlass fiber reinforcementInformation provided by Toyobo.
Melt Temperature 255 - 270 °C
491 - 518 °F
Toyobo VYLOPET® EMC330 Injection Molding Polyester Resin, Hydrolysis Resistant
Applications: Electric rice cooker partsBathroom appliancesFeatures: Good hydrolysis resistanceInformation provided by Toyobo.
Melt Temperature 255 °C
491 °F
Eastman DURASTAR DS1010 Natural PCTA Copolyester
DURASTAR DS1010 polymer contains a mold release. It has excellent appearance and clarity. Its most outstanding features are chemical resistance and excellent processing characteristics. Exposure to ..
Melt Temperature 255 °C
491 °F
Eastman Eastar Copolyester BR003, Natural PCTA Copolyester
EASTAR BR003 Copolyester contains a mold release additive. It has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabiliti..