Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 249 - 268 °C | 480 - 515 °F | |
Polymer Resources NY6-G13-[color]H Nylon, 13% Glass Reinforced, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Melt Temperature | 249 - 268 °C | 480 - 515 °F | |
Polymer Resources NY6-G20 Nylon 6, 20% Glass Reinforced Nylon 6, 20% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Melt Temperature | 249 - 268 °C | 480 - 515 °F | |
Polymer Resources NY6-G30 Nylon 6, 30% Glass Reinforced Nylon 6, 30% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Melt Temperature | 249 - 277 °C | 480 - 530 °F | |
Polymer Resources PC/ABS-FRG5 Flame Retardant PC/ABS Alloy, 5% Glass Reinforced PC/ABS Alloy, Flame Retardant, 5% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Melt Temperature | 249 - 266 °C | 480 - 510 °F | Molding |
PolyOne Edgetek® PS-30GF/000 Polybutylene Terephthalate (PBT), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 249 - 266 °C | 480 - 511 °F | |
LNP VALOX® SMV5845 PBT + PET Alloy, 16% Carbon Fiber Reinforcement
(discontinued **) ESD Applications. Will be VC1600.Features: Good Chemical Resistance, High Flow, Flame RetardantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.Th.. |
|||
Melt Temperature | 249 - 266 °C | 480 - 511 °F | |
LNP VALOX® SMV5847 PBT + PET Alloy, 30% Carbon Fiber Reinforcement
(discontinued **) ESD Applications. VC3000.Features: Good Chemical Resistance, High Flow, Flame RetardantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data .. |
|||
Melt Temperature | 249 - 268 °C | 480 - 515 °F | |
Polymer Resources NY6-G13-[color]-H Nylon 6, 13% Glass Reinforced, Heat Stabilized Nylon 6, 13% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon.. |
|||
Melt Temperature | 249 - 260 °C | 480 - 500 °F | |
Firestone CLM200-001 Nylon 6 Used for monofiliament extrusion. Natural color. Not heat stabilized or modified. Lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone |
|||
Melt Temperature | 249 - 282 °C | 480 - 540 °F | |
Styron EMERGEâ„¢ 9500CR Polycarbonate (PC) / Polyethylene Terephthalate (PET) Overview: EMERGEâ„¢ PC/PET 9500 CR advanced resin is a polycarbonate blend with excellent chemical resistance and ignition resistance properties. This grade was designed for use in medical equipm.. |
|||
Melt Temperature | 249 - 271 °C | 480 - 520 °F | |
Eastman Eastar 5011 Copolyester Eastar Copolyester 5011 is a glycol modified polyethylene terephthalate(PET). The modification is made by adding a second glycol, cyclohexanedimethanol (CHDM) during the polymerization stages. The s.. |
|||
Melt Temperature | 249 - 277 °C | 480 - 530 °F | |
Clariant Renol 60G13HSP Black Nylon 6, 13% Glass Fiber Reinforced, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Melt Temperature | 249 - 282 °C | 480 - 540 °F | |
Clariant Renol BR2065 Nylon 66, Mineral/Glass Reinforced Data provided by Clariant Masterbatches |
|||
Melt Temperature | 249 - 288 °C | 480 - 550 °F | |
Ecomass® 705ZD70 Tungsten Filled ABS Nontoxic Alternative to Lead (Pb) for radiation shielding applicationsHigh specific GravityTungsten Filled ABS compoundRigidGood ToughnessInformation provided by Technical Polymers |
|||
Melt Temperature | 249 - 266 °C | 480 - 510 °F | Processing Temperature |
Teknor Apex Chemlon® 214 GH Nylon 6, 14% Short Glass Fiber Features: Good Creep Resistance; Good Dimensional Stability; Good Processability; Good Toughness; Heat Stabilized; High Strength Processing Method: Injection Molding Forms: Pellets Additive: Heat S.. |
|||
Melt Temperature | 249 - 316 °C | 480 - 600 °F | Average value: 287 °C Grade Count:11 |
Overview of materials for Polyphenylene Ether, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu.. |