Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 216 - 238 °C | 420 - 460 °F | |
PlastiComp Complet® LGF30 - TPU Rigid Thermoplastic Polyurethane, 30% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 30% long glass fiber reinforcementInformation provided by Plas.. |
|||
Melt Temperature | 216 - 227 °C | 420 - 441 °F | ASTM D789 |
Niche Polymer PA6GF43N Nylon 6, 43% Glass Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 216 - 227 °C | 420 - 441 °F | ASTM D789 |
Niche Polymer PA6GM40BK Nylon 6, 40% Mineral Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 216 - 238 °C | 421 - 460 °F | |
PolyOne Edgetek® PP-20GF/000 HS Polypropylene, Unspecified (PP, Unspecified) Information provided by PolyOne |
|||
Melt Temperature | 216 - 232 °C | 420 - 450 °F | |
ExxonMobil Santoprene® 273-50 Thermoplastic Elastomer
(discontinued **) A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Melt Temperature | 216 - 238 °C | 420 - 460 °F | |
PlastiComp Complet® LCF50 - TPU Rigid Thermoplastic Polyurethane, 50% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Melt Temperature | 216 - 238 °C | 420 - 460 °F | |
PlastiComp Complet® LGF50 - TPU Rigid Thermoplastic Polyurethane, 50% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 50% long glass fiber reinforcementInformation provided by Plas.. |
|||
Melt Temperature | 216 - 238 °C | 420 - 460 °F | |
PlastiComp Complet® LGF60 - TPU Rigid Thermoplastic Polyurethane, 60% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 60% long glass fiber reinforcementInformation provided by Plas.. |
|||
Melt Temperature | 216 - 238 °C | 421 - 460 °F | |
Ineos Nova 1983 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Extremely high impact strength with good flexural stiffness, Color Stable, Custom colors, UL94 HB at 0.060 for all colorsApplications: Suitable for extrusion or injection molding processes requiring.. |
|||
Melt Temperature | 216 - 238 °C | 421 - 460 °F | |
Ineos Nova 474 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Custom ColorsApplications: Injection molding, Alternative to engineering resinsPerformance grades of polystyrene are engineered to have specific properties. These products can be custom colored. N.. |
|||
Melt Temperature | 216 - 238 °C | 421 - 460 °F | |
Ineos Nova 782 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High flow, Custom colorsApplications: Multi-purpose injection molding where custom color is a requirement, Toys, Appliance, Computer peripheralsPerformance grades of polystyrene are engineered to ha.. |
|||
Melt Temperature | 216 - 238 °C | 421 - 460 °F | |
Ineos Nova 879 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High heat crystal polystyrene, Color stable, Custom colorsApplications: Injection molding, Designed for applications requiring high strength, high heat resistance, and color stabilityPerformance gra.. |
|||
Melt Temperature | 216 °C | 420 °F | |
LyondellBasell Ultrathene® UE672317 Ethylene Vinyl Acetate Copolymer, Film Grade Ultrathene UE672 is an EVA copolymer with excellent impact strength, heat sealability, good toughness and flexibility. Applications may include flexible packaging films for food and healthcare, as w.. |
|||
Melt Temperature | 216 °C | 420 °F | |
Teknor Apex Chemlon® 217 GI Nylon 6, 17% Glass Fiber Reinforced Features: High Impact, 17% Glass Reinforced; Highly toughened compound designed to improve practical toughness and ductility Processing Method: Injection Molding Forms: Pellets Additive: Impact Mod.. |
|||
Melt Temperature | 216 - 232 °C | 421 - 450 °F | |
Styron MAGNUMâ„¢ 347 HP Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositi.. |
|||
Melt Temperature | 216 °C | 421 °F | Injection |
Lubrizol ESTANE® 58149 Ester Based Thermoplastic Polyurethane Features: Low Compression SetUse: Hydraulic Seals and Gaskets Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol. |
|||
Melt Temperature | 216 - 232 °C | 420 - 450 °F | Processing |
ExxonMobil Santoprene® 103-40 Thermoplastic Elastomer A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Melt Temperature | 216 - 232 °C | 420 - 450 °F | Processing |
ExxonMobil Santoprene® 203-40 Thermoplastic Elastomer A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Melt Temperature | 216 - 232 °C | 420 - 450 °F | |
ExxonMobil Santoprene® 273-40 Thermoplastic Elastomer A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Melt Temperature | 216 - 249 °C | 420 - 480 °F | |
Clariant Renol ABS3460 ABS, General Purpose, Low Gloss Data provided by Clariant Masterbatches |
|||
Melt Temperature | 216 - 249 °C | 420 - 480 °F | |
Clariant Renol ABS3470 ABS, High Heat, Low Gloss Data provided by Clariant Masterbatches |
|||
Melt Temperature | 216 - 249 °C | 420 - 480 °F | |
Clariant Renol BR4014BK ABS, High Gloss, Black Data provided by Clariant Masterbatches |
|||
Melt Temperature | 216 °C | 420 °F | |
Teknor Apex Chemlon® 214 GH Nylon 6, 14% Short Glass Fiber Features: Good Creep Resistance; Good Dimensional Stability; Good Processability; Good Toughness; Heat Stabilized; High Strength Processing Method: Injection Molding Forms: Pellets Additive: Heat S.. |
|||
Melt Temperature | 216 - 293 °C | 420 - 560 °F | Average value: 247 °C Grade Count:9 |
Overview of materials for Nylon 6, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Nucleated". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Melt Temperature | 216 - 232 °C | 420 - 450 °F | Processing |
ExxonMobil Santoprene® 123-50 Thermoplastic Elastomer
(discontinued **) A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran.. |