Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 0.500 - 1.50 MPa | 72.5 - 218 psi | |
Polykemi AB POLYblend 45FS GK25 PC/ABS-Blend, Glass Fiber reinforced Information provided by Polykemi AB |
|||
Back Pressure | 0.500 - 1.50 MPa | 72.5 - 218 psi | |
Polykemi AB POLYblend 45H PC/ABS-blend, Flame Retardant Information provided by Polykemi AB |
|||
Back Pressure | 0.500 - 1.50 MPa | 72.5 - 218 psi | |
Polykemi AB POLYblend 85E PC/ABS-Blend Information provided by Polykemi AB |
|||
Back Pressure | 0.500 - 1.50 MPa | 72.5 - 218 psi | |
Polykemi AB POLYblend 85H PC/ABS-Blend Information provided by Polykemi AB |
|||
Back Pressure | 0.500 - 1.50 MPa | 72.5 - 218 psi | |
Polykemi AB POLYblend 90VB PC/ABS-Blend, Flame Retardant Information provided by Polykemi AB |
|||
Back Pressure | 0.500 - 1.50 MPa | 72.5 - 218 psi | |
Polykemi AB POLYelast TPE S902A Thermoplastic Elastomer, SBS-based Information provided by Polykemi AB |
|||
Back Pressure | 0.500 - 1.50 MPa | 72.5 - 218 psi | |
Polykemi AB POLYelast TPE Z400 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Back Pressure | 0.500 - 1.50 MPa | 72.5 - 218 psi | |
Polykemi AB POLYelast TPE Z406 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | |
Polykemi AB POLYfill PPH 150DNH Polypropylene Homopolymer, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
Back Pressure | 0.500 - 2.00 MPa | 72.5 - 290 psi | Injection molding |
Hexion Bakelite™ EP 8414 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage
(dis Epoxy molding compound, inorganically filled, glass fiber reinforced, highly heat resistant, good electrical even at higher temperatures, very slight post shrinkage, increased media resistance, UL l.. |
|||
Back Pressure | 0.500 - 2.00 MPa | 72.5 - 290 psi | Injection molding |
Hexion Bakelite™ PF 2774 Phenolic Formaldehyde Resin, Dishwasher Proof, Improved Electrical Properties, Low Shrinkage, UL Listed Phenolic molding compound, inorganically filled, glass fiber reinforced, increased dimensional stability, averaged notched impact strength, average heat resistance, improved electrical properties, U.. |
|||
Back Pressure | 0.500 - 2.00 MPa | 72.5 - 290 psi | Injection molding |
Hexion Bakelite™ PF 14694 Phenolic Formaldehyde Resin, High Surface Quality
(discontinued **) Phenolic molding compound, mainly organically filled, very soft flow for large molds.Application areas: Housing parts, heat shields, cookware fittings.Information provided by Bak AGBak AG became a p.. |
|||
Back Pressure | 0.500 - 2.00 MPa | 72.5 - 290 psi | Injection molding |
Hexion Bakelite™ X30 Phenolic Formaldehyde Resin
(discontinued **) Phenolic molding compound, reinforced with cotton and sisal fibers, increased notched impact strength.Application areas: Covers for electrical and electromagnetic devices.Information provided by Bak.. |
|||
Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection Molding |
Stellarchem DIOSHY® GP-935-UB2 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection Molding |
Stellarchem GP-930 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection Molding |
Stellarchem MP-8001 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Back Pressure | 0.500 - 0.848 MPa | 72.5 - 123 psi | Injection |
Alliance Polymers Viprene™ G80A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G80A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Back Pressure | 0.500 - 2.00 MPa | 72.5 - 290 psi | Injection molding |
Hexion Bakelite™ PF 2874 Phenolic Formaldehyde Resin, Low Shrinkage, Improved Electrical Properties, UL Listed, High Mechanical Strength Phenolic molding compound, inorganically filled, glass fiber reinforced, increased mechanical strength, increased temperature stability, low water absorption, good dimensional stability, UL listed m.. |
|||
Back Pressure | 0.500 - 2.00 MPa | 72.5 - 290 psi | Injection molding |
Hexion Bakelite™ PF 8052 Phenolic Formaldehyde Resin, Resistant to High Temperatures
(discontinued **) Phenolic molding compound, glass fiber reinforced and inorganically filled. Excellent heat resistance with respect to surface finish and mechanical properties.Application areas: Pan handles, heat r.. |
|||
Back Pressure | 0.500 - 2.00 MPa | 72.5 - 290 psi | Injection molding |
Hexion Bakelite™ PF 2855 Phenolic Formaldehyde Resin, High Surface Quality, Low Shrinkage, For Electrostatic Coating, Dishwasher Proof, UL Listed Phenolic molding compound, inorganically/organically filled, heat resistant up to 250°C, hot steam and hot water resistant, high surface quality, for electrostatic coating, UL listed molding compou.. |