Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | |
Polymer Resources PC/TP-GP3-G10 PC/Polyester Alloy, 10% Glass Reinforced Superior Chemical Resistance, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | DAM; Extrusion |
DuPont Performance Polymers Zytel® 7304 NC010 Nylon 6
(Unverified Data**) Zytel® 7304 NC010 is a medium viscosity, unlubricated polyamide 6 resin for extrusion applications.Information provided by DuPont Performance Polymers |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | Injection Molding |
LG Chemical LUPOY EC5000AF PC/ABS, Flame Residence Description: Injection Molding, PC/ABS, Flame Residence, Anti-StaticApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9 and 68928-70-1Information provided by LG Chemical |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | Injection Molding |
LG Chemical LUPOY GP5006BH PC/ABS, Heat Resistance, Impact Strength Description: Injection Molding, PC/ABS, Heat Resistance, Impact Strength, High ToughnessApplication: Miscellaneous GoodsCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical.. |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | Injection Molding |
LG Chemical LUPOY HR5007AE PC/ABS, High Impact Description: Injection Molding, PC/ABS, High Flow, High ImpactApplication: E&E (Housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical |
|||
Dry Time | 2.00 - 6.00 hour | 2.00 - 6.00 hour | |
Gromax BFG30-FN00N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Dry Time | 2.00 - 6.00 hour | 2.00 - 6.00 hour | |
Gromax BFG30-FU00B3 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Dry Time | 2.00 - 6.00 hour | 2.00 - 6.00 hour | |
Gromax BFM30-EL04B2 Nylon 6 30% Mineral Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Dry Time | 2.00 - 6.00 hour | 2.00 - 6.00 hour | |
Gromax BTG30-DN03N1 Nylon 6 30% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Dry Time | 2.00 - 6.00 hour | 2.00 - 6.00 hour | |
Gromax CFG33-RN13N1 Nylon 6 33% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Dry Time | 2.00 - 6.00 hour @Temperature 80.0 °C |
2.00 - 6.00 hour @Temperature 176 °F |
|
Lanxess Durethan® AKV 15 FN 00 000000 Nylon 66, 12% Glass Fiber PA 66, 12% glass fiber, injection molding, halogen free flame retardantInformation provided by LANXESS. |
|||
Dry Time | 2.00 - 6.00 hour | 2.00 - 6.00 hour | |
Gromax ATE90-FN01N1 Nylon 6 (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Dry Time | 2.00 - 6.00 hour | 2.00 - 6.00 hour | |
Gromax BFG30-EN04B2 Nylon 6 36% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | |
Eurostar Staramide AG3K PA66, 15% Glass Filled, Injection Molded AG3K is a Heat and Hydrolytically Stabilized, 15% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl.. |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | |
Eurostar Staramide AG4K PA66, 20% Glass Filled, Injection Molded AG4K is a Heat and Hydrolytically Stabilized, 20% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl.. |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | |
Eurostar Staramide BG6ST43 PA6, 30% Glass Fiber Filled, Impact Modified, Injection Molded BG6ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | |
Eurostar Staramide AG3 PA66, 15% Glass Filled, Injection Molded AG3 is a 15% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | |
Eurotec® Tecodur® PB70 GR45 NL100 HS01 PBT/PET, 45% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Dry Time | 3.00 - 6.00 hour | 3.00 - 6.00 hour | |
Eurotec® Tecoform® PO20 NL RM POM, MoS2 modified, natural Information provided by Eurotec® |
|||
Dry Time | 3.00 - 6.00 hour | 3.00 - 6.00 hour | |
Eurotec® Tecoform® PO20 NL RW POM, surface modified, natural Information provided by Eurotec® |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | |
Arkema Group Pebax® 5533 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 5533 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema .. |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | |
Arkema Group Rilsan® Clear G170 Polyamide Rilsan® Clear G170 is a high performance transparent polyamide with outstanding thermal resistance. This grade has been designed for extrusion and injection molding applications and for medical use.. |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | |
Arkema Group Rilsan® PA 11 BESNO MED Nylon 11 Rilsan® PA 11 BESNO MED is a polyamide produced from a renewable source. This grade dedicated to extrusion offers the highest quality and it is specially designed to meet the stringent requirements.. |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | DAM; Injection Molding |
DuPont Performance Polymers Zytel® RS 3261TL NC010 Nylon 610
(Unverified Data**) Zytel® RS 3261TL NC010 is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by weight. It is an unreinforced and toughened resin for injection molding.. |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | |
Eurostar Staramide BG3H PA6, 15% Glass Filled, Injection Molded BG3H is a Heat Stabilized, 15% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Dry Time | 2.00 - 6.00 hour | 2.00 - 6.00 hour | |
Gromax CFG35-R113N1 Nylon 6 36% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |