Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eurotec® Tecodur® PB70 GR45 NL100 HS01 PBT/PET, 45% glass fiber reinforced, heat stabilized, natural

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , PBT + PET Blend, Glass Filled , Polybutylene Terephthalate (PBT), Heat Resistant , Polyethylene Terephthalate (PET)
Manufacturer Eurotec
Trade Name Tecodur®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurotec® Tecodur® PB70 GR45 NL100 HS01 PBT/PET, 45% glass fiber reinforced, heat stabilized, natural.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Eurotec®
Physical Properties Metric English Comments
Density 1.68 g/cc
0.0607 lb/in³
ISO 1183
Moisture Absorption 0.100 %

@Temperature 23.0 °C
0.100 %

@Temperature 73.4 °F
50% RH; ISO 960
Mechanical Properties Metric English Comments
Tensile Strength at Break 140 MPa
20300 psi
ISO 527
Elongation at Break 1.5 %
1.5 %
ISO 527
Tensile Modulus 16.0 GPa
2320 ksi
ISO 527
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
8.00 kJ/m²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Thermal Properties Metric English Comments
Melting Point 225 °C
437 °F
[10 K/min], ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 215 °C
419 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 205 °C
401 °F
ISO 75
Flammability, UL94 HB

@Thickness 0.750 mm
HB

@Thickness 0.0295 in
HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
IEC 60093
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
IEC 60093
Processing Properties Metric English Comments
Processing Temperature 260 - 280 °C
500 - 536 °F
Feed Temperature 50.0 - 70.0 °C
122 - 158 °F
Throat
Mold Temperature 60.0 - 110 °C
140 - 230 °F
Drying Temperature 120 °C
248 °F
Dry Time 4.00 - 6.00 hour
4.00 - 6.00 hour
Moisture Content <= 0.080 %
<= 0.080 %
ISO 960
Hold Pressure 40.0 - 80.0 MPa
5800 - 11600 psi
Descriptive Properties Value Comments
Back Pressure Low
Injection Speed Fast
Users viewing this material also viewed the following: