Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | |
PolyOne OnFlex™ BIO 5170D-E0010 Thermoplastic Elastomer (TPE) OnFlex™ BIO 5100 series thermoplastic elastomer compounds are glass reinforced thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% renewab.. |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | |
PolyOne OnFlex™ BIO 5180D-E0014 Thermoplastic Elastomer (TPE) OnFlex™ BIO 5100 series thermoplastic elastomer compounds are glass reinforced thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% renewab.. |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | |
PolyOne OnFlex™ BIO 5370A-E0004 Thermoplastic Elastomer (TPE) OnFlex™-Bio 5300 series thermoplastic elastomer compounds are soft thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% of renewable materi.. |
|||
Dry Time | 1.00 - 3.00 hour | 1.00 - 3.00 hour | |
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA)
(Unverified Data**) Ixef 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance. - Black: Ixef 15.. |
|||
Dry Time | 1.00 - 3.00 hour | 1.00 - 3.00 hour | |
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 43% Filler by Weight Additive:Nucleating AgentLubricant Features:Fast Molding CycleGeneral PurposeGood Mold Release Good.. |
|||
Dry Time | 1.00 - 3.00 hour | 1.00 - 3.00 hour | |
Ascend Performance Materials Vydyne® 21SPG1 Nylon 66, DAM Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit.. |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP3015-GR High Temperature Protective Coating Inorganic, Mixed Oxides Filled These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Gray-ceramic inorganic coating to 1400°F. |
|||
Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4000 High Temperature Protective Silicone Coating, Metal Oxide Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4010S High Temperature Protective Coating Silicone-Polyester |
|||
Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4010-S1 High Temperature Protective Coating, Silicone |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4070-S High Temperature Protective Coating, Silicone-Polyester |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4070-S1 High Temperature Protective Coating, Silicone |
|||
Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4070-S1 High Temperature Protective Coating, Silicone |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4080-S High Temperature Protective Coating, Silicone-Polyester |
|||
Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4080-S High Temperature Protective Coating, Silicone-Polyester |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4090-S1 High Temperature Protective Coating, Silicone |
|||
Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4090-S1 High Temperature Protective Coating, Silicone |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4095-S High Temperature Protective Coating, Silicone-Polyester |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP5000 High Temperature Protective Coating Inorganic, Zinc Filled CP5000 is a two part, water-based, inorganic zinc rich primer which provides superior resistance to salt-fog, immersion, impact and abrasion. This primer system is compatible with all CP-Series prod.. |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP3015-AL High Temperature Protective Coating Inorganic, Mixed Oxides Filled These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Aluminum-ceramic filled coating to 1200°F. |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4000-S High Temperature Protective Coating Silicone-Polyester |
|||
Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4010 High Temperature Protective Silicone Coating, Aluminum Filled Single part, silicone-based, low viscosity, heat-curable, aluminum-filled sealer offering exceptional moisture resistance to 1100°F (593°C). |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4020 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4010 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4020-S1 High Temperature Protective Coating, Silicone |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4050-S High Temperature Protective Coating Silicone-Polyester |
|||
Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4050-S1 High Temperature Protective Coating, Silicone |
|||
Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
Aremco Corr-Paint™ CP4090-S High Temperature Protective Coating, Silicone-Polyester |
|||
Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
Aremco Corr-Paint™ CP4095-S1 High Temperature Protective Coating, Silicone |
|||
Dry Time | 1.00 - 3.00 hour | 1.00 - 3.00 hour | |
Ascend Performance Materials Vydyne® 21SPF1 Nylon 66, DAM Vydyne® 21SPF1 is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding applications with the added benefits of improved flow during the molding .. |