Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | |
PolyOne Gravi-Tech™ GRV-PB-069-BMX Natural Polyether Block Amide (PEBA-Ether) Information provided by PolyOne |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | |
Oxford Polymers PEEK 20GF-Natural PEEK, 20% Glass Fiber Reinforced Product Description: Glass Fiber (20% Reinforced), PEEK, Polyetheretherketone injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Glass fiber Special Chara.. |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | |
Polymer Resources PC/TP-GP3-G20 PC/Polyester Alloy, 20% Glass Reinforced Superior Chemical Resistance, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | |
Polymer Resources PC/TP-GP3-G30 PC/Polyester Alloy, 30% Glass Reinforced Superior Chemical Resistance, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | DAM; Extrusion |
DuPont Performance Polymers Zytel® FG42A NC010 Nylon 66
(Unverified Data**) Zytel® FG42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion. It has been developed for consideration into applications such as parts for the food industry.Informat.. |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | Injection Molding |
LG Chemical LUPOY GP5008A PC/ABS Description: Injection Molding, PC/ABS, General Purpose, High FlowApplication: Miscellaneous GoodsCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Dry Time | 2.00 - 6.00 hour | 2.00 - 6.00 hour | |
Gromax CFG33-RN13N1 Nylon 6 33% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Dry Time | 2.00 - 6.00 hour @Temperature 80.0 °C |
2.00 - 6.00 hour @Temperature 176 °F |
|
Lanxess Durethan® BC 30 S 000000 Nylon 6 PA 6, non-reinforced, injection moldingInformation provided by LANXESS. |
|||
Dry Time | 2.00 - 6.00 hour | 2.00 - 6.00 hour | |
Gromax BFG20-DN00N1 Nylon 6 20% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Dry Time | 2.00 - 6.00 hour | 2.00 - 6.00 hour | |
Gromax BFG30-DN00N1 Nylon 6 30% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Dry Time | 2.00 - 6.00 hour | 2.00 - 6.00 hour | |
Gromax BTE45-DN00N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Dry Time | 2.00 - 6.00 hour | 2.00 - 6.00 hour | |
Gromax CFG45-PN11N1 Nylon 6 46% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | |
Eurostar Staramide AG10K PA66, 50% Glass Filled, Injection Molded AG10 is a Heat and Hydrolytically Stabilized, 50% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl.. |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | |
Eurostar Staramide AG6K PA66, 30% Glass Filled, Injection Molded AG6 is a Heat and Hydrolytically Stabilized, 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | |
Eurostar Staramide AST03 PA66, Impact Modified, Injection Molded AST03 is an Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | |
Eurostar Staramide PF004EUC PA6, 20% Glass Filled, Injection Molded PF004EUC is a 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | |
Eurostar Starflam AFR450X2 PA66, 25% Glass Filled, Injection Molded AFR450X2 is a Red Phosphorous, Flame Retardant, 25% Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive su.. |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | |
Eurotec® Tecodur® PB70 GR50 BK009 MX01 PBT/PET, 50% glass fiber reinforced, heat & UV stabilized, improved impact, natural Information provided by Eurotec® |
|||
Dry Time | 3.00 - 6.00 hour | 3.00 - 6.00 hour | |
Eurotec® Tecoform® PO20 GR25 NL HS POM, 25% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | |
Eurotec® Tecodur® PB70 GR45 NL100 HS01 PBT/PET, 45% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Dry Time | 3.00 - 6.00 hour | 3.00 - 6.00 hour | |
Eurotec® Tecoform® PO20 NL RM POM, MoS2 modified, natural Information provided by Eurotec® |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | |
Arkema Group Pebax® 4033 SA 01 MED Polyether Block Amide (PEBA) Polyether block amide PEBAX® 4033 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t.. |
|||
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | |
Arkema Group Pebax® 4033 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 4033 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema .. |
|||
Dry Time | 2.00 - 6.00 hour | 2.00 - 6.00 hour | |
Gromax CFG30-SN31N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |