| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Drying Temperature | 65.0 - 80.0 °C | 149 - 176 °F | |
|
Multibase TPSiV® 3111-60A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Hydrolysis resistant; FDA 21 CFR 177.2600 CompliantAPPLICATIONS: Solution for soft touc..
|
|||
| Drying Temperature | 65.0 - 80.0 °C | 149 - 176 °F | |
|
Multibase TPSiV® 4000-50A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mob..
|
|||
| Drying Temperature | 65.0 - 80.0 °C | 149 - 176 °F | |
|
Multibase TPSiV® 4000-60A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mob..
|
|||
| Drying Temperature | 65.0 - 80.0 °C | 149 - 176 °F | |
|
Multibase TPSiV® 4000-70A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mob..
|
|||
| Drying Temperature | 65.0 - 80.0 °C | 149 - 176 °F | |
|
Multibase TPSiV® 4000-80A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mob..
|
|||
| Drying Temperature | 65.0 - 80.0 °C | 149 - 176 °F | |
|
Multibase TPSiV® 4100-60A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Low compression setAPPLICATIONS: Solution for soft touch overmolding on consumer electr..
|
|||
| Drying Temperature | 65.0 - 80.0 °C | 149 - 176 °F | |
|
Multibase TPSiV® 4100-70A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Low compression setAPPLICATIONS: Solution for soft touch overmolding on consumer electr..
|
|||
| Drying Temperature | 65.0 - 80.0 °C | 149 - 176 °F | |
|
Multibase TPSiV® 4200-50A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e..
|
|||
| Drying Temperature | 65.0 - 80.0 °C | 149 - 176 °F | |
|
Multibase TPSiV® 4200-60A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e..
|
|||
| Drying Temperature | 65.0 - 80.0 °C | 149 - 176 °F | |
|
Multibase TPSiV® 4200-70A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e..
|
|||
| Drying Temperature | 65.0 - 80.0 °C | 149 - 176 °F | |
|
Multibase TPSiV® 4200-80A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e..
|
|||
| Drying Temperature |
65.0
°C <br>@Time 14400 sec
|
149
°F <br>@Time 4.00 hour
|
Pre-drying |
|
Premix Thermoplastics PRE-ELEC® PET 1451
PRE-ELEC PET 1451 is a conductive thermoplastic compound based on PETG. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PET 14..
|
|||
| Drying Temperature | <= 65.0 °C | <= 149 °F | Pre-drying |
|
Premix Thermoplastics PRE-ELEC® TPE 1501 Conductive Thermoplastic Compound
PRE-ELEC® TPE 1501 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electri..
|
|||
| Drying Temperature | <= 65.0 °C | <= 149 °F | Pre-drying |
|
Premix Thermoplastics PRE-ELEC® TPE 1502 Conductive Thermoplastic Compound
PRE-ELEC® TPE 1502 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electri..
|
|||
| Drying Temperature | <= 65.0 °C | <= 149 °F | Pre-drying |
|
Premix Thermoplastics PRE-ELEC® TPE 1503 Conductive Thermoplastic Compound
PRE-ELEC® TPE 1503 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electri..
|
|||
| Drying Temperature | 65.0 - 102 °C | 149 - 216 °F | Average value: 71.5 °C Grade Count:7 |
|
Overview of materials for PETG Copolyester
This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M..
|
|||
| Drying Temperature | 65.0 °C | 149 °F | Injection Molding |
|
LG Chemical LUMID GP1300AP PA6, Plasticized
Feature: Injection Molding, PA6, PlasticizedApplication: Automotive PartsInformation provided by LG Chemical
|
|||
| Drying Temperature | 65.0 °C | 149 °F | |
|
SK Chemicals SKYGREEN® PETG 2008 Specially Formulated PET Copolymer Resin
SKYGREEN PETG is an amorphous copolyester in which a certain amount of ethylene glycol is replaced with 1,4-cyclohexane dimethanol (CHDM), which prevent crystallization, leading to improved processa..
|
|||
| Drying Temperature | 65.0 - 75.0 °C | 149 - 167 °F | |
|
Arkema Group Pebax® 5533 SA 01 MED Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 5533 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t..
|
|||
| Drying Temperature | 65.0 - 75.0 °C | 149 - 167 °F | |
|
Arkema Group Pebax® 5533 SA 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 5533 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema ..
|
|||
| Drying Temperature | 65.0 - 75.0 °C | 149 - 167 °F | |
|
Arkema Group Pebax® 5533 SP 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 5533 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide..
|
|||
| Drying Temperature | 65.0 - 75.0 °C | 149 - 167 °F | |
|
Arkema Group Pebax® 6333 SA 01 MED Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 6333 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t..
|
|||
| Drying Temperature | 65.0 - 75.0 °C | 149 - 167 °F | |
|
Arkema Group Pebax® 6333 SA 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 6333 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema ..
|
|||
| Drying Temperature | 65.0 - 75.0 °C | 149 - 167 °F | |
|
Arkema Group Pebax® 6333 SP 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 6333 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide..
|
|||
| Drying Temperature | 65.0 - 75.0 °C | 149 - 167 °F | |
|
Arkema Group Pebax® Rnew 55R53 SP 01 Polyether Block Amide (PEBA)
Polyether block amide Pebax® 55R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV..
|
|||
| Drying Temperature | 65.0 - 75.0 °C | 149 - 167 °F | |
|
Arkema Group Pebax® Rnew 63R53 SP 01 Polyether Block Amide (PEBA)
Polyether block amide Pebax® 63R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV..
|
|||