| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Drying Temperature | 65.0 - 80.0 °C | 149 - 176 °F | |
| Multibase TPSiV® 3111-60A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Hydrolysis resistant; FDA 21 CFR 177.2600 CompliantAPPLICATIONS: Solution for soft touc.. |
|||
| Drying Temperature | 65.0 - 80.0 °C | 149 - 176 °F | |
| Multibase TPSiV® 4000-50A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mob.. |
|||
| Drying Temperature | 65.0 - 80.0 °C | 149 - 176 °F | |
| Multibase TPSiV® 4000-60A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mob.. |
|||
| Drying Temperature | 65.0 - 80.0 °C | 149 - 176 °F | |
| Multibase TPSiV® 4000-70A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mob.. |
|||
| Drying Temperature | 65.0 - 80.0 °C | 149 - 176 °F | |
| Multibase TPSiV® 4000-80A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mob.. |
|||
| Drying Temperature | 65.0 - 80.0 °C | 149 - 176 °F | |
| Multibase TPSiV® 4100-60A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Low compression setAPPLICATIONS: Solution for soft touch overmolding on consumer electr.. |
|||
| Drying Temperature | 65.0 - 80.0 °C | 149 - 176 °F | |
| Multibase TPSiV® 4100-70A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Low compression setAPPLICATIONS: Solution for soft touch overmolding on consumer electr.. |
|||
| Drying Temperature | 65.0 - 80.0 °C | 149 - 176 °F | |
| Multibase TPSiV® 4200-50A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e.. |
|||
| Drying Temperature | 65.0 - 80.0 °C | 149 - 176 °F | |
| Multibase TPSiV® 4200-60A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e.. |
|||
| Drying Temperature | 65.0 - 80.0 °C | 149 - 176 °F | |
| Multibase TPSiV® 4200-70A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e.. |
|||
| Drying Temperature | 65.0 - 80.0 °C | 149 - 176 °F | |
| Multibase TPSiV® 4200-80A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e.. |
|||
| Drying Temperature | 65.0 °C @Time 14400 sec |
149 °F @Time 4.00 hour |
Pre-drying |
| Premix Thermoplastics PRE-ELEC® PET 1451 PRE-ELEC PET 1451 is a conductive thermoplastic compound based on PETG. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PET 14.. |
|||
| Drying Temperature | <= 65.0 °C | <= 149 °F | Pre-drying |
| Premix Thermoplastics PRE-ELEC® TPE 1501 Conductive Thermoplastic Compound PRE-ELEC® TPE 1501 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electri.. |
|||
| Drying Temperature | <= 65.0 °C | <= 149 °F | Pre-drying |
| Premix Thermoplastics PRE-ELEC® TPE 1502 Conductive Thermoplastic Compound PRE-ELEC® TPE 1502 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electri.. |
|||
| Drying Temperature | <= 65.0 °C | <= 149 °F | Pre-drying |
| Premix Thermoplastics PRE-ELEC® TPE 1503 Conductive Thermoplastic Compound PRE-ELEC® TPE 1503 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electri.. |
|||
| Drying Temperature | 65.0 - 102 °C | 149 - 216 °F | Average value: 71.5 °C Grade Count:7 |
| Overview of materials for PETG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
| Drying Temperature | 65.0 °C | 149 °F | Injection Molding |
| LG Chemical LUMID GP1300AP PA6, Plasticized Feature: Injection Molding, PA6, PlasticizedApplication: Automotive PartsInformation provided by LG Chemical |
|||
| Drying Temperature | 65.0 °C | 149 °F | |
| SK Chemicals SKYGREEN® PETG 2008 Specially Formulated PET Copolymer Resin SKYGREEN PETG is an amorphous copolyester in which a certain amount of ethylene glycol is replaced with 1,4-cyclohexane dimethanol (CHDM), which prevent crystallization, leading to improved processa.. |
|||
| Drying Temperature | 65.0 - 75.0 °C | 149 - 167 °F | |
| Arkema Group Pebax® 5533 SA 01 MED Polyether Block Amide (PEBA) Polyether block amide PEBAX® 5533 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t.. |
|||
| Drying Temperature | 65.0 - 75.0 °C | 149 - 167 °F | |
| Arkema Group Pebax® 5533 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 5533 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema .. |
|||
| Drying Temperature | 65.0 - 75.0 °C | 149 - 167 °F | |
| Arkema Group Pebax® 5533 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 5533 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide.. |
|||
| Drying Temperature | 65.0 - 75.0 °C | 149 - 167 °F | |
| Arkema Group Pebax® 6333 SA 01 MED Polyether Block Amide (PEBA) Polyether block amide PEBAX® 6333 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t.. |
|||
| Drying Temperature | 65.0 - 75.0 °C | 149 - 167 °F | |
| Arkema Group Pebax® 6333 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 6333 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema .. |
|||
| Drying Temperature | 65.0 - 75.0 °C | 149 - 167 °F | |
| Arkema Group Pebax® 6333 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 6333 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide.. |
|||
| Drying Temperature | 65.0 - 75.0 °C | 149 - 167 °F | |
| Arkema Group Pebax® Rnew 55R53 SP 01 Polyether Block Amide (PEBA) Polyether block amide Pebax® 55R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV.. |
|||
| Drying Temperature | 65.0 - 75.0 °C | 149 - 167 °F | |
| Arkema Group Pebax® Rnew 63R53 SP 01 Polyether Block Amide (PEBA) Polyether block amide Pebax® 63R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV.. |
|||