| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
| Polymer Resources PC-BR1-UV Polycarbonate, Branched for Extrusion and Blow Molding, UV-stabilized Polycarbonate, Branched for Extrusion and Blow Molding, UV-stabilizedFeatures: • Ultra High Impact Resistance • Ultra High ViscosityProcess: Extrusion/Blow MoldingNotes: All physical, mechanical.. |
|||
| Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
| Polymer Resources PC-FD2-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold Release, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p.. |
|||
| Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
| Polymer Resources PC-FD3-[color]-1 Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold Release, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
| Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
| Polymer Resources PC-FD4-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
| Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
| Polymer Resources PC-FR3A-D Polycarbonate, Flame Retardant, High Flow Polycarbonate, Flame Retardant, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
| Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
| Polymer Resources PC-FR3-D Polycarbonate, Improved Flame Retardant, High Flow Polycarbonate, Improved Flame Retardant, High FlowFeatures: • High Impact Resistance • Self Extinguishing • Low ViscosityProcess: Injection MoldingNotes: All physical, mechanical and thermal t.. |
|||
| Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
| Polymer Resources PC-FR3-D-[color]-3 Polycarbonate, Improved Flame Retardant, High Flow, UV-stabilized Polycarbonate, Improved Flame Retardant, High Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
| Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
| Polymer Resources PC-G10 Polycarbonate, 10% Glass Reinforced Polycarbonate, 10% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p.. |
|||
| Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
| Polymer Resources PC-G20 Polycarbonate, 20% Glass Reinforced Polycarbonate, 20% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p.. |
|||
| Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
| Polymer Resources PC-G40 Polycarbonate, 40% Glass Reinforced Polycarbonate, 40% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p.. |
|||
| Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
| Polymer Resources PC-G5-IM Polycarbonate, 5% Glass Reinforced, Impact Modified, Foamable Polycarbonate, 5% Glass Reinforced, Impact Modified, FoamableProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf.. |
|||
| Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
| Polymer Resources PC-GP1-D Polycarbonate, General Purpose, Low Flow Polycarbonate, General Purpose, Low FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/.. |
|||
| Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
| Polymer Resources PC-GP1-TFE5 Polycarbonate, 5% PTFE, Wear Resistant, Low Flow Polycarbonate, 5% PTFE, General Purpose, Wear Resistant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
| Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
| Polymer Resources PC-GP2-D-[color]-1 Polycarbonate, General Purpose, Medium Flow with Mold Release Polycarbonate, General Purpose, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf.. |
|||
| Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
| Polymer Resources PC-GP2-D-[color]-6 Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold Release Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
| Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
| Polymer Resources PC-GP2-TFE5 Polycarbonate, 5% PTFE, Wear Resistant, Medium Flow Polycarbonate, 5% PTFE, General Purpose, Medium Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samp.. |
|||
| Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
| Polymer Resources PC-GP4-[color]-4 Polycarbonate, UV-stabilized, Easy Flow with Mold Release Polycarbonate, UV-stabilized, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
| Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
| Polymer Resources PC-GP4-[color]-6 Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samp.. |
|||
| Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
| Polymer Resources PC-HM-FR1-[color]-4 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold Release Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
| Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
| Polymer Resources PC-IM3 Polycarbonate, Impact Modified, High Flow Polycarbonate, Impact Modified, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
| Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
| Polymer Resources PC-BR1-[color]-5 Polycarbonate, Branched, Food Contact Polycarbonate, Branched for Extrusion and Blow MoldingFeatures: • Ultra High Impact Resistance • Ultra High Viscosity • Food Contact AcceptableProcess: Extrusion/Blow MoldingNotes: All physica.. |
|||
| Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
| Polymer Resources PC-FD2 Polycarbonate, FDA-compliant Feedstocks, Medium Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Medium Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
| Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
| Polymer Resources PC-FR1A-D-[color]-3 Polycarbonate, Flame Retardant, Low Flow, UV-stabilized Polycarbonate, Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
| Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
| Polymer Resources PC-HM-FR1-[color]-TFE Polycarbonate, 10% Glass Reinforced, PTFE, Flame Retardant, Wear Resistant Polycarbonate, 10% Glass Reinforced, PTFE, Flame Retardant, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, tes.. |
|||
| Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
| Polymer Resources PC-HM-FR2 Polycarbonate, 10% Glass Reinforced, Flame Retardant Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
| Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
| Polymer Resources PC-UV2-D Polycarbonate, UV-stabilized, Medium Flow Polycarbonate, UV-stabilized, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
| Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
| Polymer Resources PC-UV3-D Polycarbonate, UV-stabilized, High Flow Polycarbonate, UV-stabilized, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
| Drying Temperature | 118 - 124 °C | 245 - 255 °F | Average value: 121 °C Grade Count:8 |
| Overview of materials for Polycarbonate, Gamma Radiation Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum.. |
|||
| Drying Temperature | 118 - 127 °C | 245 - 260 °F | Average value: 123 °C Grade Count:9 |
| Overview of materials for Polycarbonate, Foam Grade, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Foam Grade, Glass Filled". Each property range of values reported is minimum and maximum .. |
|||
| Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
| Polymer Resources PCSF-FRG20 Polycarbonate, 20% Glass Reinforced Structural Foam Grade Polycarbonate, 20% Glass Reinforced Structural Foam GradeFeatures: • Flame Retardant • Foamable • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechanical and thermal testing con.. |
|||