Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 130 - 150 °C @Time 10800 sec |
266 - 302 °F @Time 3.00 hour |
|
LATI Larton MDT16-02 PPS Polyphenylene Sulfide (PPS) based compound. Magnetic detectable filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & M.. |
|||
Drying Temperature | 130 - 150 °C @Time 10800 sec |
266 - 302 °F @Time 3.00 hour |
|
LATI Laticonther 80 CPG/700 PPS, Glass Fiber Reinforced High thermal conductivity product based on Polyphenylene Sulfide (PPS). Special filler. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation.. |
|||
Drying Temperature | 130 °C | 266 °F | |
A. Schulman SCHULADUR® A GB20 20% Glass Bead Reinforced PBT Information provided by A. Schulman. |
|||
Drying Temperature | 130 °C | 266 °F | |
A. Schulman ComAlloy® E-13370 Lubricated Reinforced Polyester Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Drying Temperature | 130 °C | 266 °F | |
A. Schulman SCHULADUR® A GF15 15% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Drying Temperature | 130 °C | 266 °F | |
A. Schulman VOLOY™ 461 Glass Reinforced, Flame Retardant PBT Alloy Information provided by A. Schulman. |
|||
Drying Temperature | 130 °C | 266 °F | |
A. Schulman SCHULADUR® A GB20 20% Glass Bead Reinforced PBT Information provided by A. Schulman. |
|||
Drying Temperature | 130 °C | 266 °F | |
A. Schulman SCHULADUR® A GB30 30% Glass Bead Reinforced PBT Information provided by A. Schulman. |
|||
Drying Temperature | 130 °C | 266 °F | |
A. Schulman SCHULADUR® A GB20 20% Glass Bead Reinforced PBT Information provided by A. Schulman. |
|||
Drying Temperature | 130 °C | 266 °F | |
A. Schulman SCHULADUR® A GF30 30% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Drying Temperature | 130 °C | 266 °F | |
A. Schulman VOLOY™ 414 30% Glass Fiber Reinforced, Flame Retardant PBT Information provided by A. Schulman. |
|||
Drying Temperature | 130 °C | 266 °F | |
A. Schulman VOLOY™ 462 Hybrid Reinforced PBT Alloy Information provided by A. Schulman. |
|||
Drying Temperature | 130 °C | 266 °F | |
A. Schulman LUBRILON® 432 30% Glass Fiber Reinforced, PTFE Lubricated PBT Alloy Information provided by A. Schulman. |
|||
Drying Temperature | 130 °C | 266 °F | |
Beijing Chemical Industry KAIFA® HN201-G20 PA6 Resin 20% glass fiber reinforced, thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Drying Temperature | 130 °C | 266 °F | |
Beijing Chemical Industry KAIFA® HN301-G10 PA6 Resin 10% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Drying Temperature | 130 °C | 266 °F | |
Beijing Chemical Industry KAIFA® HN301-G30 PA6 Resin 30% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Drying Temperature | 130 - 140 °C | 266 - 284 °F | Temperature can be reduced when using vacuum ovens. |
LATI LARTON GCE/60 60% Mixed Glass Fiber and Special Mineral Filled Polyphenylene sulfide (PPS)
(discontinued Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |
|||
Drying Temperature | 130 - 140 °C | 266 - 284 °F | Temperature can be reduced when using vacuum ovens. |
LATI LARTON G/30 30% Glass Fiber Filled Polyphenylene sulfide (PPS)
(discontinued **) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |
|||
Drying Temperature | 130 - 150 °C @Time 10800 sec |
266 - 302 °F @Time 3.00 hour |
|
LATI Latilub 80-15T K/30 PPS, 30% Carbon Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati .. |
|||
Drying Temperature | 130 - 140 °C | 266 - 284 °F | Temperature can be reduced when using vacuum ovens. |
LATI LATILUB 80-40GRT Polyphenylene sulfide Base (PPS), 40% Graphite and PTFE Self Lubricating Plastic
(U Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Drying Temperature | 130 - 140 °C | 266 - 284 °F | Temperature can be reduced when using vacuum ovens. |
LATI LARTON G/40 40% Glass Fiber Filled Polyphenylene sulfide (PPS)
(Unverified Data**) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |
|||
Drying Temperature | 130 - 140 °C | 266 - 284 °F | Temperature can be reduced when using vacuum ovens. |
LATI LARTON K/30 30% Carbon Fiber Reinforced Polyphenylene sulfide (PPS)
(Unverified Data**) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |