Polymer Property : Drying Temperature = 150 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Drying Temperature 65.6 - 82.2 °C
150 - 180 °F
RheTech Products CC40P100-00EG 40% Calcium Carbonate Reinforced Polypropylene, Natural, Extrusion Grade
Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Drying Temperature 65.6 - 82.2 °C
150 - 180 °F
RheTech Products FT1002-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
Drying Temperature 65.6 - 82.2 °C
150 - 180 °F
RheTech Products FT1002-00A Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
Drying Temperature 65.6 - 82.2 °C
150 - 180 °F
RheTech Products FT2500-01A Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
Drying Temperature 65.6 - 82.2 °C
150 - 180 °F
RheTech Products FT3080-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products.
Drying Temperature 65.6 - 82.2 °C
150 - 180 °F
RheTech Products FT3080-425 Thermoplastic Polyolefin, UV Stabilized, YBWA Platinum
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
Drying Temperature 65.6 - 82.2 °C
150 - 180 °F
RheTech Products FT7011-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Claddings and faciasExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Drying Temperature 65.6 - 82.2 °C
150 - 180 °F
RheTech Products GC20P255-01UV 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, Black
Applications: Durable goodsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Drying Temperature 65.6 - 82.2 °C
150 - 180 °F
RheTech Products HP513-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
Drying Temperature 65.6 - 82.2 °C
150 - 180 °F
RheTech Products HP519-00 26% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Interior trim moldingsSill platesAir ductsInjection molding conditions reported in table.Information provided by RheTech Products.
Drying Temperature 65.6 - 82.2 °C
150 - 180 °F
RheTech Products HP519-01 26% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black
Applications: Interior trim moldingsSill platesAir ductsInjection molding conditions reported in table.Information provided by RheTech Products.
Drying Temperature 65.6 - 82.2 °C
150 - 180 °F
RheTech Products HP520-01 12% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Black
Applications: Interior trimCenter consolesGlove box binsInjection molding conditions reported in table.Information provided by RheTech Products.
Drying Temperature 65.6 - 82.2 °C
150 - 180 °F
RheTech Products HP521-01 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black
Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Drying Temperature 65.6 - 82.2 °C
150 - 180 °F
RheTech Products M40P100-01 40% Mica Reinforced Polypropylene, Black
Applications: Structural componentsAir ducts and dampenersFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
Drying Temperature 65.6 - 82.2 °C
150 - 180 °F
RheTech Products RCC220-01 20% Calcium Carbonate Reinforced Polypropylene Copolymer, Black, Recycled Content
Applications: I/P hush panelsSplash shieldsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Drying Temperature 65.6 - 82.2 °C
150 - 180 °F
RheTech Products T10P250-00 10% Talc Reinforced Polypropylene Copolymer, Natural
Applications: Fan shroudsCenter consolesAir ductsInjection molding conditions reported in table.Information provided by RheTech Products.
Drying Temperature 65.6 - 82.2 °C
150 - 180 °F
RheTech Products T10UP100-01 10% Talc Reinforced Polypropylene Copolymer, General Purpose Black, UL94 HB Rated
Applications: Wire troughElectrical componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Drying Temperature 65.6 - 82.2 °C
150 - 180 °F
RheTech Products T15P100-00 12% Talc Reinforced Polypropylene, Natural
Applications: Component housingConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Drying Temperature 65.6 - 82.2 °C
150 - 180 °F
RheTech Products T20P100-517UV 20% Talc Reinforced Polypropylene, UV Stabilized, Interior DX9 Black
Applications: Center consolesIP componentsClose out panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Drying Temperature 65.6 - 82.2 °C
150 - 180 °F
RheTech Products T20P252-01 20% Talc Reinforced Polypropylene Copolymer, Black
Applications: IP Structural componentsGlove box binWire troughInjection molding conditions reported in table.Information provided by RheTech Products.
Drying Temperature 65.6 - 82.2 °C
150 - 180 °F
RheTech Products T40P108-01 40% Talc Reinforced Polypropylene, Black
Applications: Wire troughBracketsConsolesFan shroudsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Drying Temperature 65.6 - 82.2 °C
150 - 180 °F
RheTech Products HP506-01 20% Talc Reinforced High Performance Polypropylene, Black
Applications: Underhood componentsLamp housingsHVAC ductsInjection molding conditions reported in table.Information provided by RheTech Products.
Drying Temperature 65.6 - 82.2 °C
150 - 180 °F
RheTech Products HP506-01A 21% Talc Reinforced High Performance Polypropylene, UV Stabilized, Black
Applications: Automotive interior applicationsHVAC ductsTail lamp housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Drying Temperature 65.6 °C
150 °F
PolyOne Edgetek® AS-40GF/000 Acrylonitrile Butadiene Styrene (ABS), Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Drying Temperature 65.6 - 82.2 °C
150 - 180 °F
Average value: 77.6 °C Grade Count:13
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini..
Drying Temperature 65.6 °C

@Time 7200 sec
150 °F

@Time 2.00 hour
Styrolution Zylar 960 MBS
ZYLAR 960 is an impact modified styrene acrylic copolymer that provides toughness equivalent to some grades of polycarbonate, good clarity and superior processing characteristics for demanding injec..
Drying Temperature 65.6 - 93.3 °C
150 - 200 °F
Desiccant type
CPT C-Flex® R70-003 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Drying Temperature 65.6 - 93.3 °C
150 - 200 °F
Desiccant type
CPT C-Flex® R70-085 Clear Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Drying Temperature 65.6 - 82.2 °C
150 - 180 °F
RheTech Products HP522-357 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, JA6A Black
Applications: Center consolesAir vents louversInterior trimInjection molding conditions reported in table.Information provided by RheTech Products.
Drying Temperature 65.6 - 90.0 °C
150 - 194 °F
Average value: 77.5 °C Grade Count:7
Overview of materials for Polypropylene with 40% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are..
Copyright © lookpolymers.com All Rights Reserved