Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 82.0 - 93.0 °C | 180 - 199 °F | |
PolyOne Lubri-Tech™ PS-000/15T Polyester (PBT) - 15% PTFE Lubricated
(discontinued **) Data provided by PolyOne. |
|||
Drying Temperature | 82.0 - 93.0 °C | 180 - 199 °F | |
PolyOne Lubri-Tech™ PS-000/15T-2S Polyester (PBT) - 15% PTFE Lubricated - 2% Silicone Lubricated
(discontinue Data provided by PolyOne. |
|||
Drying Temperature | 82.0 - 93.0 °C | 180 - 199 °F | |
PolyOne Lubri-Tech™ PS-000/20T Polyester (PBT) - 20% PTFE Lubricated
(discontinued **) Data provided by PolyOne. |
|||
Drying Temperature | 82.0 - 93.0 °C | 180 - 199 °F | |
PolyOne Stat-Tech™ AS-15CP/000 ABS - 15% Carbon Powder
(discontinued **) Data provided by PolyOne. |
|||
Drying Temperature | 82.0 - 93.0 °C @Time 10800 - 14400 sec |
180 - 199 °F @Time 3.00 - 4.00 hour |
|
Ineos ABS Lustran® 256 Extrusion Blending Grade Lustran® ABS 256 resin is a natural, medium-flow, medium-impact, low-gloss, low-gel extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It is used for blending with other Lustran® ABS vi.. |
|||
Drying Temperature | 82.0 - 93.0 °C @Time 7200 sec |
180 - 199 °F @Time 2.00 hour |
|
Ineos ABS Lustran® 720 ABS, Molding Grade Lustran® ABS 720 resin is a black, virgin injection molding grade of ABS (acrylonitrile butadiene styrene). It is supplied as salt-and-pepper pellets with color concentrate 901802 black. Designed.. |
|||
Drying Temperature | 82.0 - 93.0 °C @Time 7200 sec |
180 - 199 °F @Time 2.00 hour |
|
Ineos ABS Lustran® 750 ABS, Molding Grade Lustran® 750 resin is a black, virgin injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It is designed for molded drain, waste, and vent (DWV) fittings. Lustran® 750 (901802 bl.. |
|||
Drying Temperature | 82.0 - 93.0 °C @Time 7200 sec |
180 - 199 °F @Time 2.00 hour |
|
Ineos ABS Lustran® 786 ABS, Extrusion Grade Lustran® ABS 786 resin is a black, virgin extrusion grade of ABS (acrylonitrile butadiene styrene). It is designed for extruded drain, waste, and vent (DWV) pipe. Lustran® ABS 786 (901046 blac.. |
|||
Drying Temperature | 82.0 - 93.0 °C @Time 7200 sec |
180 - 199 °F @Time 2.00 hour |
|
Ineos ABS Lustran® ABS 241 ABS, Blending Grade Lustran® ABS 241 resin is a natural, stiffer-flow, virgin blending grade of ABS (acrylonitrile butadiene styrene). It is designed for use with other high-impact ABS resins for drain, waste, and v.. |
|||
Drying Temperature | 82.0 - 93.0 °C @Time 10800 - 14400 sec |
180 - 199 °F @Time 3.00 - 4.00 hour |
|
Ineos ABS Lustran® LK197 ABS, Extrusion Grade Lustran® ABS LK197 resin is a high-gloss, medium-impact extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It provides a superior balance between rigidity and impact strength, as well as e.. |
|||
Drying Temperature | 82.0 - 93.0 °C @Time 7200 sec |
180 - 199 °F @Time 2.00 hour |
|
Ineos ABS Lustran® 261 ABS, High-Impact Blending Grade Lustran® ABS 261 resin is a natural, stiffer-flow, virgin blending grade of ABS (acrylonitrile butadiene styrene). It is designed for use with other high-impact ABS resins for drain, waste, and v.. |
|||
Drying Temperature | 82.0 - 93.0 °C @Time 7200 - 10800 sec |
180 - 199 °F @Time 2.00 - 3.00 hour |
|
Ineos ABS Lustran® SMA 2171 SMA, Injection Molding Grade Lustran® SMA 2171 is a high heat injection molding grade of impact-modified SMA (styrene/maleic anhydride) terpolymer offering an exceptional balance of processability and performance. Lustran®.. |
|||
Drying Temperature | 82.0 - 93.0 °C | 180 - 199 °F | air dew point <-40°C |
Lubrizol Pellethane® 2363-80A Thermoplastic Polyurethane Elastomer Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Drying Temperature | 82.0 - 93.0 °C | 180 - 199 °F | air dew pint <-40°C |
Lubrizol Estane® 2102-80A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Low compression setAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 20.. |
|||
Drying Temperature | 82.0 - 93.0 °C | 180 - 199 °F | air dew point <-40°C |
Lubrizol Estane® 2103-70A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: High MVTRAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Drying Temperature | 82.0 - 93.0 °C | 180 - 199 °F | air dew point <-40°C |
Lubrizol Estane® 2103-80AE Thermoplastic Polyurethane Elastomer Formerly PellethaneAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Drying Temperature | 82.0 - 93.0 °C | 180 - 199 °F | air dew point <-40°C |
Lubrizol Estane® 2103-80AEN Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: NSF Standard 61 certified, FDA complianceAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane produ.. |
|||
Drying Temperature | 82.0 - 93.0 °C | 180 - 199 °F | |
Lubrizol Estane® 2103-80PF Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Film and profile resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in.. |
|||
Drying Temperature | 82.0 - 93.0 °C | 180 - 199 °F | air dew point <-40°C |
Lubrizol Estane® 2103-84AEN Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Contains UV Stabilizer, NSF Standard 61 certifiedAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pelletha.. |
|||
Drying Temperature | 82.0 - 93.0 °C | 180 - 199 °F | air dew point <-40°C |
Lubrizol Estane® 2103-85AE Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Film and profile resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in.. |
|||
Drying Temperature | 82.0 - 93.0 °C | 180 - 199 °F | air dew point <-40°C |
Lubrizol Estane® 2355-75A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Memory and elasticity, Impact modificationAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane pro.. |
|||
Drying Temperature | 82.0 - 93.0 °C | 180 - 199 °F | air dew point <-40°C |
Lubrizol Estane® 2355-80AE Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Damping capacityAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009... |
|||
Drying Temperature | 82.0 - 93.0 °C | 180 - 199 °F | air dew point <-40°C |
Lubrizol Estane® 2355-85ABR Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: FDA and USDA compliance, Blend resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product l.. |
|||
Drying Temperature | 82.0 - 93.0 °C | 180 - 199 °F | |
PolyOne Edgetek® NL-45GF/000 Nylon 6/12 - 45% Glass Fiber
(discontinued **) Data provided by PolyOne. |
|||
Drying Temperature | 82.0 - 93.0 °C | 180 - 199 °F | air dew point <-40°C |
Lubrizol Estane® 2102-75A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Memory, elasticity and impact modificationAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane prod.. |
|||
Drying Temperature | 82.0 - 93.0 °C | 180 - 199 °F | air dew point <-40°C |
Lubrizol Estane® 2103-80AEF Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Film resin for injection blow moldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product l.. |