Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products CS30P100-01UV 30% Ceramic Sphere Reinforced Polypropylene, UV Stabilized, Black Applications: Consumer goodsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products F37-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: ElectronicsBracketsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products FT2700-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Air deflectorsFuel filler shieldsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products FT3080-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products FT4600-152 Thermoplastic Polyolefin, UV Stabilized, JA6A Black Applications: Scuff platesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products FT4802-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products FT4900-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products FT4900-772UV Thermoplastic Polyolefin, UV Stabilized, RXF Jet Black Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products FT5250-01UV Thermoplastic Polyolefin, UV Stabilized, Black Applications: Cowl vent grillesExterior componentsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products FT7011-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Claddings and faciasExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products FT7013-721UV Thermoplastic Polyolefin, UV Stabilized, XDV Dark Slate Applications: Scuff platesLift gate coversI/P componentsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products G13P100-00 13% Glass Fiber Reinforced Polypropylene, Natural Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products G20P100-599 20% Glass Fiber Reinforced Polypropylene, UV Stabilized, (Ford BJ4A) Medium Dark Parchment Applications: Arm rest insertVacuum canister insertStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 71.1 - 82.2 °C | 160 - 180 °F | |
PolyOne LubriOne™ NN-30GF/10T WHT Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products GC30P100-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: Arm rest insertBattery trayBracketsAir cleaner housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products GC30P200-01UV 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, Black Applications: Interior componentsStructural housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products GC43P250-777 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Ivory Applications: BracketsStructural supportsDurable GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products P102-00 Polypropylene, Black Applications: Consumer goodsIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products P251-01 Polypropylene Copolymer, Black Applications: Splash shieldFuse panel coversCenter consolesDoor panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products T30P200-01BG 30% Talc Reinforced Polypropylene Copolymer, Black, Blow Molding Grade Applications: HVAC ductsSeat backsFlipper panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products T40P100-01 40% Talc Reinforced Polypropylene, Black Applications: Wire troughBracketsConsolesFan shroudsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products T40P100-04 40% Talc Reinforced Polypropylene, White Applications: Automotive componentsConsumer productsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 76.7 - 82.2 °C | 170 - 180 °F | |
Polymer Resources AH-GP1 Acetal Homopolymer, Low Flow, High Melt Strength, Heat Stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 76.7 - 82.2 °C | 170 - 180 °F | |
Polymer Resources AH-GP2-TFE10 Acetal Homopolymer, 10% PTFE Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 76.7 - 82.2 °C | 170 - 180 °F | |
Polymer Resources PC/ABS-GP2 General Purpose PC/ABS Alloy, High Flow PC/ABS Alloy, General Purpose, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by .. |
|||
Drying Temperature | 71.1 - 82.2 °C | 160 - 180 °F | |
Polymer Resources PPX-SF1 Modified-PPO, Structural Foam Grade, Flame Retardant, Easy Flow Modified-Polyphenylene Oxide, Structural Foam Grade, Easy FlowFeatures: • Flame Retardant • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechani.. |
|||
Drying Temperature | 71.1 - 82.2 °C | 160 - 180 °F | |
Polymer Resources PPX-SF2 Modified-PPO, Structural Foam Grade, Flame Retardant Modified-Polyphenylene Oxide, Structural Foam Grade, Standard FlowFeatures: • Flame Retardant • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mec.. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products G20P100-601 20% Glass Fiber Reinforced Polypropylene, UV Stabilized, (Ford ZUA5) Dark Graphite Applications: Arm rest insertVacuum canisterStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products HP513-00A High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Drying Temperature | 65.6 - 82.2 °C | 150 - 180 °F | |
RheTech Products HP522-286 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, ZUCA Medium Graphite Applications: ConsolesClose out panelInjection molding conditions reported in table.Information provided by RheTech Products. |