Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Drying Temperature = 180 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Drying Temperature 150 - 180 °C
302 - 356 °F
Not necessary for reinforced materials. Temperature can be reduced when using vacuum ovens.
LATI LAPEX A Polyethersulfone (PES) (UL94 V-0)  (Unverified Data**)
Description: Lapex A compounds are polyethersulfone (PES) products. They are high temperature compounds offering an interesting combination of properties. Lapex A provides outstanding thermal resist..
Drying Temperature 150 - 180 °C
302 - 356 °F
Not necessary for reinforced materials. Temperature can be reduced when using vacuum ovens.
LATI LAPEX A G/10 10% Glass Fiber Reinforced Polyethersulfone (PES) (UL94 V-0)  (Unverified Data**)
Description: Lapex A compounds are polyethersulfone (PES) products. They are high temperature compounds offering an interesting combination of properties. Lapex A provides outstanding thermal resist..
Drying Temperature 150 - 180 °C
302 - 356 °F
Not necessary for reinforced materials. Temperature can be reduced when using vacuum ovens.
LATI LAPEX A G/20 20% Glass Fiber Reinforced Polyethersulfone (PES) (UL94 V-0)  (Unverified Data**)
Description: Lapex A compounds are polyethersulfone (PES) products. They are high temperature compounds offering an interesting combination of properties. Lapex A provides outstanding thermal resist..
Drying Temperature 150 - 180 °C
302 - 356 °F
Not necessary for reinforced materials. Temperature can be reduced when using vacuum ovens.
LATI LAPEX A G/30 30% Glass Fiber Reinforced Polyethersulfone (PES) (UL94 V-0)  (Unverified Data**)
Description: Lapex A compounds are polyethersulfone (PES) products. They are high temperature compounds offering an interesting combination of properties. Lapex A provides outstanding thermal resist..
Drying Temperature 150 - 180 °C

@Time 10800 sec
302 - 356 °F

@Time 3.00 hour
LATI Lapex A G/10 PES, 10% Glass Fiber Reinforced
Polyether Sulfone (PES) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ..
Drying Temperature 150 - 180 °C

@Time 10800 sec
302 - 356 °F

@Time 3.00 hour
LATI Lapex A G/20 PES, 20% Glass Fiber Reinforced
Polyether Sulfone (PES) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ..
Drying Temperature 140 - 180 °C

@Time 10800 sec
284 - 356 °F

@Time 3.00 hour
LATI Lapex A PES
Polyether Sulfone (PES). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInf..
Drying Temperature 140 - 180 °C

@Time 10800 sec
284 - 356 °F

@Time 3.00 hour
LATI Lapex R G/10 PPSU, 10% Glass Reinforced
Polyphenylene Sulfone (PPSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A..
Drying Temperature 140 - 180 °C

@Time 10800 sec
284 - 356 °F

@Time 3.00 hour
LATI Lapex R G/20 PPSU, 20% Glass Reinforced
Polyphenylene Sulfone (PPSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A..
Drying Temperature 140 - 180 °C

@Time 10800 sec
284 - 356 °F

@Time 3.00 hour
LATI Lapex R PPSU
Polyphenylene Sulfone (PPSU). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ameri..
Drying Temperature 150 - 180 °C

@Time 10800 sec
302 - 356 °F

@Time 3.00 hour
LATI Latilub 85-10T G/30 PES, 30% Glass Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polyether Sulfone (PES). PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu..
Drying Temperature 150 - 180 °C

@Time 10800 sec
302 - 356 °F

@Time 3.00 hour
LATI Latiohm 85-06 PD01 G/15 PES, 15% Glass Fiber Reinforced
Semiconductive/dissipative product based on Polyether Sulfone (PES). Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..
Drying Temperature 149 - 180 °C
300 - 356 °F
Average value: 151 °C Grade Count:14
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a..
Drying Temperature 135 - 180 °C
275 - 356 °F
Average value: 151 °C Grade Count:15
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m..
Drying Temperature 149 - 180 °C
300 - 356 °F
Average value: 156 °C Grade Count:10
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% ..
Drying Temperature 70.0 - 180 °C
158 - 356 °F
Average value: 98.7 °C Grade Count:14
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyether Grade". Each property range of values reported is minimum a..
Drying Temperature 150 - 180 °C

@Time 10800 sec
302 - 356 °F

@Time 3.00 hour
LATI Lapex A G/30 PES, 30% Glass Fiber Reinforced
Polyether Sulfone (PES) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ..
Copyright © lookpolymers.com All Rights Reserved