Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 149 °C | 300 °F | |
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK)
(Unverified Data**) AV-722 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding wea.. |
|||
Drying Temperature | 149 °C | 300 °F | |
LNP ULTEM® SMU6303 Polyetherimide, 5% Glass Fiber Reinforcement, 5% PTFE Lubricant
(discontinued **) Will be UNTW05.Features: Lubricated, High Heat Resistance, Good Wear Resistance, Low to None Ion Content, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provide.. |
|||
Drying Temperature | 149 °C @Time 14400 sec |
300 °F @Time 4.00 hour |
|
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK) AV-755 SL45 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like th.. |
|||
Drying Temperature | 149 °C @Time 14400 sec |
300 °F @Time 4.00 hour |
|
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK) KetaSpire® KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provide.. |
|||
Drying Temperature | 149 °C | 300 °F | |
Solvay Specialty Polymers Radel® R-5500 Polyphenylsulfone (PPSU) Radel® R-5500 is a general purpose extrusion grade of polyphenylsulfone (PPSU), offering exceptional hydrolytic stability and better toughness than most commercially available high-temperature po.. |