Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 93.3 °C | 200 °F | |
Multibase Multi-Pro® 1004 R Polypropylene Features: Scratch Resistance, GoodHeat Resistance, HighStiffness, GoodForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Drying Temperature | 93.3 °C | 200 °F | |
Multibase Multi-Pro® 1008 T Polypropylene Talc Filler, 10% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Drying Temperature | 93.3 °C | 200 °F | |
Multibase Multi-Pro® 1505 R Polypropylene Glass Fiber Reinforced, 15% by weight.Features:Heat Resistance, HighScratch ResistantStiffness, GoodForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Drying Temperature | 93.3 °C | 200 °F | |
Multibase Multi-Pro® 2005 RCI Polypropylene Glass Fiber Reinforced, 20% by weight.Features:Heat Resistance, HighScratch ResistantStiffness, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided .. |
|||
Drying Temperature | 93.3 °C | 200 °F | |
Multibase Multi-Pro® 2516 CU Polypropylene Calcium Carbonate Filler, 25% by weight.Features:Gloss, High UV Resistance, Good Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureLawn and Garden EquipmentInformation provided by Mult.. |
|||
Drying Temperature | 93.3 °C | 200 °F | |
Multibase Multi-Pro® 2518 CU Polypropylene Calcium Carbonate Filler, 25% by weight.Features:Gloss, High Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Drying Temperature | 93.3 °C | 200 °F | |
Multibase Multi-Pro® 4005 M Polypropylene Mica Filled, 40% by weight.Features:Rigidity, HighImpact Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided by Multibase |
|||
Drying Temperature | 93.3 °C | 200 °F | |
PolyOne Trilliant™ HC HC3220-0030 RS Natural Polycarbonate (PC) The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead.. |
|||
Drying Temperature | 93.3 - 107 °C | 200 - 225 °F | |
Polymer Resources PPX/NY G10 PPO/Nylon 66 Alloy , 10% Glass Reinforced Polyphenylene Oxide/Nylon 66 Alloy , 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Drying Temperature | 93.3 - 107 °C | 200 - 225 °F | |
PolyOne Lubri-Tech™ PS-15GB/10T Polybutylene Terephthalate (PBT), Glass Bead Filled, PTFE Lubricated
(discont Description/Features:Glass Bead FilledPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 93.3 - 104 °C | 200 - 220 °F | |
PolyOne Edgetek® PS-15GF-25MN/000 Polybutylene Terephthalate (PBT), Glass/Mineral Filled
(discontinued **)< Description/Features:Glass/Mineral ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 93.3 °C | 200 °F | |
PolyOne Edgetek® PS-40GF/000 Polybutylene Terephthalate (PBT), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 93.3 °C | 200 °F | |
PolyOne Edgetek® BB-20GF/000 PC/ABS Blend, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 93.3 °C | 200 °F | then reduce to 160°F |
Ecomass® 4703TU95 Tungsten Filled Polyurethane Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsHigh Specific GravityTungsten Powder Filled Polyurethane (TPU)FlexibleInformation provided by Technical Po.. |
|||
Drying Temperature | 93.3 °C | 200 °F | then reduce to 160°F |
Ecomass® 4703ZD84 Tungsten Filled Polyurethane Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsModerate Specific GravityTungsten Powder Filled Polyurethane (TPU)FlexibleInformation provided by Technica.. |
|||
Drying Temperature | 93.3 °C | 200 °F | |
PolyOne Lubri-Tech™ MP-20CF/15T Modified Polyphenylene Oxide (mPPO), Carbon Fiber Reinforced, PTFE Lubricated
  Description/Features:Carbon Fiber ReinforcedPTFE LubricatedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Drying Temperature | 93.3 - 98.9 °C | 200 - 210 °F | |
Polymer Resources PPX-FR5 Modified PPO, UL 94 V-0 with HDT of 225 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |