Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 71.0 °C | 160 °F | |
Eastman Eastar GN125 Copolyester, Natural
(discontinued **) Eastar Copolyester GN125 is a glycol modified polyethylene terephthalate (PET) that contains an ultraviolet light inhibitor. This product is recommended for indoor applications requiring enhanced co.. |
|||
Drying Temperature | 71.0 - 82.0 °C | 160 - 180 °F | |
PolyOne Stat-Tech™ AS-7SS/000 ABS - 7% Stainless Steel Fiber
(discontinued **) Data provided by PolyOne. |
|||
Drying Temperature | 71.0 °C | 160 °F | |
PolyOne Lubri-Tech™ AT-15GP/05T Acetal With Graphite - 5% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Drying Temperature | 71.0 °C | 160 °F | |
PolyOne Lubri-Tech™ ATH-000/02T Homopolymer - 2% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Drying Temperature | 71.0 °C | 160 °F | |
PolyOne Lubri-Tech™ ATH-000/05M Acetal Homopolymer - 5% MoS2
(discontinued **) Data provided by PolyOne. |
|||
Drying Temperature | 71.0 °C | 160 °F | |
Styrolution PS-168M Polystyrene Description: Polystyrene 168M is a high heat, high molecular weight general purpose polystyrene with excellent clarity and high stiffness. Due to its high melt strength and high stiffness. PS-168M i.. |
|||
Drying Temperature | 71.0 °C | 160 °F | |
Eastman Drystar 0325 Copolyester This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Drying Temperature | 71.0 °C | 160 °F | |
Eastman Drystar 0603 Copolyester This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Drying Temperature | 71.0 °C | 160 °F | |
Eastman DuraStar MN611 Polymer, Natural Durastar Polymer MN611 contains a mold release. It has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing char.. |
|||
Drying Temperature | 71.0 °C | 160 °F | |
Eastman Eastar 5011 Copolyester Eastar Copolyester 5011 is a glycol modified polyethylene terephthalate(PET). The modification is made by adding a second glycol, cyclohexanedimethanol (CHDM) during the polymerization stages. The s.. |
|||
Drying Temperature | 71.0 °C | 160 °F | |
Eastman Eastar DN001HF Copolyester Applications:DisplaysPersonal care and CosmeticsProduct Description: Eastar Copolyester DN001HF has excellent flow characteristics while maintaining superior mechanical properties. It is easy to p.. |
|||
Drying Temperature | 71.0 °C | 160 °F | |
Eastman Eastar DN004HF Copolyester Applications:DisplaysPersonal care and CosmeticsProduct Description: Eastar Copolyester DN004HF has excellent flow characteristics while maintaining superior mechanical properties. It is easy to p.. |
|||
Drying Temperature | 71.0 °C | 160 °F | |
Eastman Eastar DN010 Copolyester Eastar Copolyester DN010 is a brilliantly clear polymer having excellent impact strength, chemical resistance, and low shrinkage rates. Eastar Copolyester DN010 contains no mold release.Applications.. |
|||
Drying Temperature | 71.0 °C | 160 °F | |
Eastman Eastar DN011 Copolyester Eastar Copolyester DN011 is a brilliantly clear polymer having excellent impact strength, chemical resistance, and low shrinkage rates. Eastar Copolyester DN011 contains a mold release.Applications/.. |
|||
Drying Temperature | 71.0 °C | 160 °F | |
Eastman Eastar DN114 Copolyester, Natural Applications:LightingProduct Description: Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage. DN1.. |
|||
Drying Temperature | 71.0 °C | 160 °F | |
Eastman Eastar GN119 Copolyester Applications:Personal care and CosmeticsProduct Description: Eastar GN119 Copolyester is a low-I.V. PETG, for sale only in Asia as a high-flow formulation. This product has been GREENGUARD INDOOR .. |
|||
Drying Temperature | 71.0 °C | 160 °F | |
Eastman Eastar GN120 Copolyester Applications:AppliancesConsumer electronicsPersonal care and cosmeticsStationary suppliesKey Attributes:High clarity and transparencyHigh flow copolyesterToughProduct Description: Eastar GN120 Cop.. |
|||
Drying Temperature | 71.0 °C | 160 °F | |
Eastman Eastar MN006 Copolyester Eastar Copolyester MN006 is a brilliantly clear polymer having excellent impact strength, chemical resistance, and low shrinkage rates. Eastar Copolyester MN006 contains a mold release.Applications/.. |
|||
Drying Temperature | 71.0 °C | 160 °F | |
Eastman Eastar MN200 Copolyester Eastar Copolyester MN200 is an amorphous copolyester with excellent flow characteristics as well as radiation resistance and chemical resistance.Applications/UsesMedical |
|||
Drying Temperature | 71.0 °C | 160 °F | |
Eastman Eastar MN210 Copolyester, Natural Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates.Applications/UsesMedical |
|||
Drying Temperature | 71.0 °C | 160 °F | |
Eastman Eastar MN211 Copolyester, Natural Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. MN211 contains a mold release.Application.. |
|||
Drying Temperature | 71.0 °C | 160 °F | |
Eastman Eastar GN046 Copolyester, Natural Eastar Copolyester GN046 is a very high melt strength copolyester targeted for extrusion blow molding applications. Blow molding of large parts (up to several pounds) are possible with this material.. |
|||
Drying Temperature | 71.0 °C | 160 °F | |
Eastman Eastar GN071 Natural PETG Copolyester EASTAR GN071 Copolyester is used for injection molding applications. It is sparkling clear, tough, chemical resistant, odor free, versatile, easy to work with and affordable. Cleaning solutions wi.. |
|||
Drying Temperature | 71.0 - 110 °C | 160 - 230 °F | Average value: 86.4 °C Grade Count:11 |
Overview of materials for Nylon 66, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu.. |
|||
Drying Temperature | 71.0 - 121 °C | 160 - 250 °F | Average value: 104 °C Grade Count:62 |
Overview of materials for Acetal Copolymer, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Drying Temperature | 71.0 - 121 °C | 160 - 250 °F | Average value: 97.7 °C Grade Count:14 |
Overview of materials for Acetal Homopolymer, PTFE-Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Drying Temperature | 71.0 °C | 160 °F | |
PolyOne Lubri-Tech™ AT-000/02T Acetal - 2% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Drying Temperature | 71.0 °C | 160 °F | |
PolyOne Edgetek® AT-000/07SS Copolymer Acetal - 7% Stainless Steel Fiber
(discontinued **) Data provided by PolyOne. |