| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.23 g/cc | 1.23 g/cc | ASTM D792 |
| Linear Mold Shrinkage | 0.0020 - 0.0050 cm/cm | 0.0020 - 0.0050 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 105 | 105 | ASTM D785 |
| Tensile Strength at Break | 54.0 MPa | 7830 psi | ASTM D638 |
| Tensile Strength, Yield | 44.0 MPa | 6380 psi | ASTM D638 |
| Elongation at Break | 330 % | 330 % | ASTM D638 |
| Elongation at Yield | 4.0 % | 4.0 % | ASTM D638 |
| Tensile Modulus | 1.80 GPa | 261 ksi | ASTM D638 |
| Flexural Strength | 66.0 MPa | 9570 psi | ASTM D790 |
| Flexural Modulus | 1.80 GPa | 261 ksi | ASTM D790 |
| Izod Impact, Notched | 0.770 J/cm @Temperature -40.0 °C |
1.44 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
| NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
ASTM D256 | |
| Izod Impact, Unnotched | NB | NB | ASTM D4812 |
| NB @Temperature -40.0 °C |
NB @Temperature -40.0 °F |
ASTM D4812 | |
| Puncture Energy | 46.0 J | 33.9 ft-lb | Puncture Resistance @Max Load, 23°C; ASTM D3763 |
| 46.0 J @Temperature -40.0 °C |
33.9 ft-lb @Temperature -40.0 °F |
Puncture Resistance at Max Load; ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 73.0 °C | 163 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 64.0 °C | 147 °F | ASTM D648 |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Haze | 1.4 % | 1.4 % | ASTM D1003 |
| Transmission, Visible | 89 % | 89 % | Regular Transmittance; ASTM D1003 |
| 92 % | 92 % | Total Transmittance; ASTM D1003 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 249 - 271 °C | 480 - 520 °F | |
| Mold Temperature | 16.0 - 38.0 °C | 60.8 - 100 °F | |
| Drying Temperature | 71.0 °C | 160 °F | |
| Dry Time | 6 hour | 6 hour |