Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Albis Plastics Cellulose Acetate Propionate CP808 (FDA), 17% Plasticizer  (discontinued **)

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Cellulosic , Cellulose Acetate Propionate, Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Albis Plastics Cellulose Acetate Propionate CP808 (FDA), 17% Plasticizer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and ContainersProcessing: Injection Molding (Melt Temperature: 405°F, Mold Temperature: 110°F)Data supplied by Albis Plastics Corporation.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Water Absorption 1.4 %
1.4 %
(24 hr); ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 29.0 MPa
4210 psi
ASTM D638
Tensile Strength, Yield 23.4 MPa
3390 psi
ASTM D638
Flexural Yield Strength 33.1 MPa
4800 psi
ASTM D790
Izod Impact, Notched 4.48 J/cm
8.39 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 72.0 °C
162 °F
ASTM D648
Vicat Softening Point 91.0 °C
196 °F
ASTM D1525
Processing Properties Metric English Comments
Melt Temperature 207 °C
405 °F
Injection
Mold Temperature 43.0 °C
109 °F
Users viewing this material also viewed the following: