Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 90.0 - 110 °C | 194 - 230 °F | Preferred |
Nilit Nilamid A3 H G3 15% Glass Reinforced PA66 Description: Nilamid A3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 66. This product combines good overall mechanical performance and impact strength with ease of processing.Key char.. |
|||
Mold Temperature | 90.0 - 110 °C | 194 - 230 °F | Preferred |
Nilit Nilamid B3 H G7 35% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G7 is a general purpose, 35% glass fiber reinforced NYLON 6. It has high mechanical performance, and also excellent moldability. Its impact performance is outstanding, so i.. |
|||
Mold Temperature | 82.2 - 110 °C | 180 - 230 °F | |
PolyOne Edgetek® PS-20CF/000 Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Mold Temperature | 82.2 - 110 °C | 180 - 230 °F | |
PolyOne Stat-Tech™ PS-NX 102902 CM Black Polybutylene Terephthalate (PBT)
(discontinued **) Preliminary Data SheetPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Mold Temperature | 80.0 - 110 °C | 176 - 230 °F | |
DuPont Performance Polymers Sorona® FG3015G NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data** Sorona® FG3015G NC010 is a 15% glass fiber reinforced polytrimethylene terephthalate resin containing 31% renewably sourced ingredients by weight (37% based on polymer only) formulated to be food c.. |
|||
Mold Temperature | 70.0 - 110 °C | 158 - 230 °F | |
Lehmann & Voss LUVOCOM® 3-7901 Polyamide 6, with glass fiber and carbon fiber Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressElectrically conductive, suitable for continuous discharging of staticall.. |
|||
Mold Temperature | 70.0 - 110 °C | 158 - 230 °F | |
Lehmann & Voss LUVOCOM® 3-8437 Polyamide 6, with glass fiber Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts with low creep.Emergency running property.Suitable for metall inserts.Control.. |
|||
Mold Temperature | 70.0 - 110 °C | 158 - 230 °F | |
Lehmann & Voss LUVOCOM® 6-8438-1 Polyamide 12, with glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Suitable for discharging of statically generated electricity.Dynamic stressed parts.Low waterab.. |
|||
Mold Temperature | 80.0 - 110 °C | 176 - 230 °F | Injection Molding |
LG Chemical LUCEL FW720F Modified POM, Friction Resistance, Abrasion Resistance Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0 and 9002-84-2Information provided by LG.. |
|||
Mold Temperature | 80.0 - 110 °C | 176 - 230 °F | Injection Molding |
LG Chemical LUCEL HI515W POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: Gears, Automobile ClipCAS No. 66455-31-0 and 155123-66-3Information provided by LG Chemical |
|||
Mold Temperature | 80.0 - 110 °C | 176 - 230 °F | Injection Molding |
LG Chemical LUMID GP2101BF PA66+GF10%, Halogen Free Flame Retardant Feature: Injection Molding, PA66+GF10%, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG.. |
|||
Mold Temperature | 80.0 - 110 °C | 176 - 230 °F | Injection Molding |
LG Chemical LUMID GP2130B(W) PA66+GF13%, General Purpose Feature: Injection Molding, PA66+GF13%, General PurposeApplication: Valve CoversCAS No. 32131-17-2, 65997-17-3 and 9010-79-9Information provided by LG Chemical |
|||
Mold Temperature | 80.0 - 110 °C | 176 - 230 °F | Injection Molding |
LG Chemical LUMID GP3300B(W) PA66+MF30%, General Purpose Feature: Injection Molding, PA66+MF30%, General PurposeApplication: Automotive (Engine Cover))CAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical |
|||
Mold Temperature | 90.0 - 110 °C | 194 - 230 °F | |
LATI Latiohm 87/28-07 CNT PC Semiconductive/dissipative product based on Polycarbonate (PC). Carbon nanotubes. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Mold Temperature | 71.1 - 110 °C | 160 - 230 °F | |
Samyang Trirex® PC-3025N2 10 MFI Flame Retardant Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Mold Temperature | 90.0 - 110 °C | 194 - 230 °F | |
A. Schulman SCHULADUR® B GF25LB 25% Glass Fiber Reinforced, Lubricated PET Information provided by A. Schulman. |
|||
Mold Temperature | 90.0 - 110 °C | 194 - 230 °F | |
A. Schulman SCHULADUR® B GF25LB 25% Glass Fiber Reinforced, Lubricated PET Information provided by A. Schulman. |
|||
Mold Temperature | 100 - 110 °C | 212 - 230 °F | actual surface temp |
Unitika TERRAMAC TE-8300 Polylactic Acid (PLA) High-durability, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Mold Temperature | 60.0 - 110 °C | 140 - 230 °F | |
Eurotec® Tecodur® PB70 GR15 BK002 XA21 PBT, 15% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Mold Temperature | 60.0 - 110 °C | 140 - 230 °F | |
Eurotec® Tecodur® PB70 GR17 BK002 FA20 PBT, 17% glass fiber reinforced, flame retardant - halogen (RoHS compliant), black Information provided by Eurotec® |
|||
Mold Temperature | 60.0 - 110 °C | 140 - 230 °F | |
Eurotec® Tecodur® PB70 GR50 BK002 CA01 PBT/PET, 50% glass fiber reinforced, heat & UV stabilized, natural Information provided by Eurotec® |
|||
Mold Temperature | 70.0 - 110 °C | 158 - 230 °F | |
Eurotec® Tecomid® NA40 GB30 NL HS PA6.6, 30% glass bead reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Mold Temperature | 90.0 - 110 °C | 194 - 230 °F | |
E-Polymers TEKAMID® TB120G45 , 45% Glass Fiber Reinforced PA6, DAM 45% Glass Fiber Reinforced, High Strength.Information provided by E-Polymers Co. Ltd. |
|||
Mold Temperature | 54.4 - 110 °C | 130 - 230 °F | Average value: 76.3 °C Grade Count:16 |
Overview of materials for Nylon 6, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, PTFE Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Mold Temperature | 80.0 - 110 °C | 176 - 230 °F | |
DuPont Performance Polymers Sorona® 3301 BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)&l Sorona® 3301 BK001 is an unreinforced black polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight with superior surface appearance in ambient temperature condi.. |
|||
Mold Temperature | 70.0 - 110 °C | 158 - 230 °F | |
LATI Latiohm 75/4-08 PD01 G/30 PBT, 30% Glass Fiber Reinforced Semiconductive/dissipative product based on Polybutylene Terephthalate (PBT). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |