Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
BASF Capron® GR15 HS 15% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron GR15 HS is a heat stabilized 15% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest.. |
|||
Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
BASF Capron® GR20 20% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron GR20 is a 20% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also.. |
|||
Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
BASF Capron® HPN 9333G HS Impact Modified, 33% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron HPN 9333G HS is a heat stabilized, 33% glass reinforced, impact modified polyamide 6 injection molding compound combining exceptional strength, stiffness and high temperature performance with.. |
|||
Mold Temperature | >= 95.0 °C | >= 203 °F | |
DuPont Performance Polymers Rynite® 940 NC010 PET
(Unverified Data**) Information provided by DuPont Performance Polymers |
|||
Mold Temperature | >= 95.0 °C | >= 203 °F | |
DuPont Performance Polymers Rynite® RE15022 NC010 PET
(Unverified Data**) Rynite® RE15022 NC010 is a 36% glass reinforced product designed for applications that need high burst strength.Information provided by DuPont Performance Polymers |
|||
Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
BASF Capron® 8230G HS 6% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron 8230G HS is a heat stabilized, 6% nylon 6 molding compound offering improved stiffness and dimensional stability in thin sections. It exhibits a combination of strength, stiffness and perfor.. |
|||
Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
BASF Capron® 8231G 14% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8231G is a 14% glass fiber reinforced polyamide 6 molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also av.. |
|||
Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
BASF Capron® 8232G HS 25% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron 8232G HS is a heat stabilized, 25% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. Its resista.. |
|||
Mold Temperature | 95.0 - 120 °C | 203 - 248 °F | |
Lavergne VYPET VNT 335 PET 35% Glass - Mineral Reinforced Vypet VNT 335 is a 35% glass/mineral reinforced PET injection molding compound designed for structural applications.Features: High temperature performance; Low warp; Excellent dimensional stabilityT.. |
|||
Mold Temperature | 95.0 - 120 °C | 203 - 248 °F | |
Lavergne VYPET VNT 635A PET 35% Glass Reinforced Vypet 635A is a 35 % glass reinforced PET injection molding compound designed for electrical and structural applications with a very glossy surface.Features: High temperature performance, Excellent.. |
|||
Mold Temperature | 95.0 - 125 °C | 203 - 257 °F | |
Topas Advanced Polymers TOPAS® 5013S-04 Cyclic Olefin Copolymer (COC) TOPAS® 5013S-04 is a high flow injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high .. |
|||
Mold Temperature | >= 95.0 °C | >= 203 °F | |
DuPont Performance Polymers Rynite® 408 BK515 PET Rynite® 408 BK515 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness and temperature resistance.Info.. |
|||
Mold Temperature | 95.0 °C | 203 °F | Injection molding |
BASF Ultramid® 8231G HS 14% Glass Filled PA6 (Conditioned) Ultramid 8231G HS is a heat stabilized, 14% glass fiber reinforced nylon 6 injection molding compound. It is also available in non-heat stabilized (Ultramid 8231) and/or pigmented versions. The gla.. |
|||
Mold Temperature | 95.0 °C | 203 °F | Injection molding |
BASF Ultramid® 8231G HS BK-102 14% Glass Filled PA6 (Dry) Ultramid 8231G HS BK-102 is a black pigmented heat stabilized, 14% glass fiber reinforced PA6 injection molding compound.The glass fiber reinforcement enhances performance such as strength, stiffnes.. |
|||
Mold Temperature | 95.0 °C | 203 °F | Injection molding |
BASF Ultramid® 8233G HS BK-102 33% Glass Filled PA6 (Conditioned) Ultramid 8233G HS BK-102 is a heat stabilized, weather resistant, 33% glass fiber reinforced PA6 injection molding compound offering excellent strength, stiffness, high temperature performance and d.. |
|||
Mold Temperature | 95.0 °C | 203 °F | Injection molding |
BASF Ultramid® 8233G HS BK-106 33% Glass Filled PA6 (Conditioned) Ultramid 8233G HS BK-106 is a heat stabilized, weather resistant, 33% glass fiber reinforced PA6 injection molding compound offering excellent strength, stiffness, high temperature
performance and .. |
|||
Mold Temperature | 95.0 °C | 203 °F | Injection molding |
BASF Ultramid® 8260 40% Mineral Filled PA6 (Conditioned) Ultramid 8260 is a 40% mineral reinforced PA6 injection molding compound. It possesses high stiffness, dimensional stability and heat resistance combined with excellent processability including low.. |
|||
Mold Temperature | 95.0 °C | 203 °F | Injection molding |
BASF Ultramid® 8260 HS PA6 (Conditioned) |
|||
Mold Temperature | 95.0 °C | 203 °F | Injection molding |
BASF Ultramid® 8260 HS PA6 (Dry) |
|||
Mold Temperature | 95.0 °C | 203 °F | Injection molding |
BASF Ultramid® 8262G HS BK-102 7/13% Glass/Mineral Filled PA6 (Dry) Ultramid 8262G HS BK-102 is a heat stabilized, pigmented black, 20% glass and mineral reinforced PA6 injection molding compound resulting in a balance of engineering properties with excellent dimens.. |
|||
Mold Temperature | 95.0 °C | 203 °F | Injection molding |
BASF Ultramid® 8272G HS BK-102 12% Glass Filled PA6 (Dry) Ultramid 8272G HS BK-102 is a 12% glass fiber reinforced, black pigmented, thermally modified, nylon 6 blow molding compound offering an excellent balance of engineering properties combined with the.. |
|||
Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
BASF Capron® 8234G 44% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron 8234G is a 44% glass fiber reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensional stability. It is .. |
|||
Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
BASF Capron® 8260 HS BK-102 40% Mineral-Filled Nylon 6 (Conditioned)
(discontinued **) Capron 8260 HS BK-102 is a heat stabilized, pigmented black, 40% mineral reinforced nylon 6 injection molding resin. It possesses high stiffness, dimensional stability and heat resistance combined .. |
|||
Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
BASF Capron® 8260 HS BK-102 40% Mineral-Filled Nylon 6 (Dry)
(discontinued **) Capron 8260 HS BK-102 is a heat stabilized, pigmented black, 40% mineral reinforced nylon 6 injection molding resin. It possesses high stiffness, dimensional stability and heat resistance combined .. |
|||
Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
BASF Capron® 8332G Impact Modified, 25% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8332G is a 25% glass reinforced, impact modified polyamide 6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a balance of .. |
|||
Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
BASF Capron® 8333G HI Impact Modified, 33% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron 8333G HI is a 33% glass reinforced, impact modified polyamide 6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a balance .. |
|||
Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
BASF Capron® 8333G HI Impact Modified, 33% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8333G HI is a 33% glass reinforced, impact modified polyamide 6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a balance .. |
|||
Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
BASF Capron® 8334G Impact Modified, 40% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8334G is a heat stabilized, 40% glass fiber reinforced polyamide 6 molding compound developed for applications requiring a high level of stiffness combined with excellent impact performance. .. |
|||
Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
BASF Capron® GR15 15% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron GR15 is a 15% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also.. |
|||
Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
BASF Capron® GR40 40% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron GR40 is a 40% glass reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensional stability. It is also ava.. |