Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
BASF Capron® GR20 HS 20% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron GR20 HS is a heat stabilized 20% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest.. |
|||
Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
BASF Capron® GR40 HS 40% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron GR40 HS is a heat stabilized 40% glass reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensional stabil.. |
|||
Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
BASF Capron® HPN 9233G 33% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron HPN 9233G is a 33% glass reinforced polyamide 6 injection molding compound combining exceptional strength, stiffness and high temperature performance with excellent surface aesthetics. It is.. |
|||
Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
BASF Capron® 8232G 25% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron 8232G is a 25% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. Its resistance to creep under l.. |
|||
Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
BASF Capron® 8232G 25% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8232G is a 25% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. Its resistance to creep under l.. |
|||
Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
BASF Capron® 8232G HS 25% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron 8232G HS is a heat stabilized, 25% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. Its resista.. |
|||
Mold Temperature | 95.0 - 120 °C | 203 - 248 °F | |
Lavergne VYPET VNT 325 PET 25% Glass - Mineral Reinforced Vypet 325 is a 25% glass/mineral reinforced PET injection molding compound designed for electrical and structural applications.Features: High temperature performance; Good balance resilience-stiffne.. |
|||
Mold Temperature | 95.0 - 120 °C | 203 - 248 °F | |
Lavergne VYPET VNT 835 PET 35% Glass-Mineral Reinforced Vypet VNT 835 is a 35% mineral and fiberglass reinforced PET injection molding compound designed for structural applications.Features: High temperature performance; Low warp; Excellent dimensional s.. |
|||
Mold Temperature | 95.0 - 120 °C | 203 - 248 °F | |
Lavergne VYPET VNT 930 PET 30% Glass Reinforced Vypet VNT 930 is a 30% fiberglass reinforced PET injection molding compound designed for structural applications.Features: High temperature performance; Low warp; Excellent dimensional stabilityTypi.. |
|||
Mold Temperature | 95.0 - 140 °C | 203 - 284 °F | |
Akro-Plastic Akromid® T6 GF30 (3501) PPA Dry, 30% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Mold Temperature | 95.0 °C | 203 °F | Injection molding |
BASF Ultramid® 8233G HS BK-102 33% Glass Filled PA6 (Conditioned) Ultramid 8233G HS BK-102 is a heat stabilized, weather resistant, 33% glass fiber reinforced PA6 injection molding compound offering excellent strength, stiffness, high temperature performance and d.. |
|||
Mold Temperature | 95.0 °C | 203 °F | Injection molding |
BASF Ultramid® 8233G HS BK-106 33% Glass Filled PA6 (Conditioned) Ultramid 8233G HS BK-106 is a heat stabilized, weather resistant, 33% glass fiber reinforced PA6 injection molding compound offering excellent strength, stiffness, high temperature
performance and .. |
|||
Mold Temperature | 95.0 °C | 203 °F | Injection molding |
BASF Ultramid® 8233G HS BK-106 33% Glass Filled PA6 (Dry) Ultramid 8233G HS BK-106 is a heat stabilized, weather resistant, 33% glass fiber reinforced PA6 injection molding compound offering excellent strength, stiffness, high temperature
performance and .. |
|||
Mold Temperature | 95.0 °C | 203 °F | Injection molding |
BASF Ultramid® 8260 HS BK-102 40% Mineral Filled PA6 (Conditioned) Ultramid 8260 HS BK-102 is a heat stabilized, pigmented black, 40% mineral reinforced PA6 injection molding resin. It possesses high stiffness, dimensional stability and heat resistance combined wi.. |
|||
Mold Temperature | 95.0 °C | 203 °F | Injection molding |
BASF Ultramid® 8260 HS BK-102 40% Mineral Filled PA6 (Dry) Ultramid 8260 HS BK-102 is a heat stabilized, pigmented black, 40% mineral reinforced PA6 injection molding resin. It possesses high stiffness, dimensional stability and heat resistance combined wi.. |
|||
Mold Temperature | 95.0 °C | 203 °F | Injection molding |
BASF Ultramid® 8262G HS BK-102 7/13% Glass/Mineral Filled PA6 (Dry) Ultramid 8262G HS BK-102 is a heat stabilized, pigmented black, 20% glass and mineral reinforced PA6 injection molding compound resulting in a balance of engineering properties with excellent dimens.. |
|||
Mold Temperature | 95.0 °C | 203 °F | Injection molding |
BASF Ultramid® 8272G HS BK-102 12% Glass Filled PA6 (Dry) Ultramid 8272G HS BK-102 is a 12% glass fiber reinforced, black pigmented, thermally modified, nylon 6 blow molding compound offering an excellent balance of engineering properties combined with the.. |
|||
Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
BASF Capron® 8231G 14% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron 8231G is a 14% glass fiber reinforced polyamide 6 molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also av.. |
|||
Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
BASF Capron® 8260 40% Mineral-Filled Nylon 6 (Dry)
(discontinued **) Capron 8260 is a 40% mineral reinforced polyamide 6 injection molding compound. It possesses high stiffness, dimensional stability and heat resistance combined with excellent processability includi.. |
|||
Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
BASF Capron® 8260 HS BK-102 40% Mineral-Filled Nylon 6 (Conditioned)
(discontinued **) Capron 8260 HS BK-102 is a heat stabilized, pigmented black, 40% mineral reinforced nylon 6 injection molding resin. It possesses high stiffness, dimensional stability and heat resistance combined .. |
|||
Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
BASF Capron® 8331G HS Blend Impact Modified, 14% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8331G HS Blend is a 14% glass fiber reinforced, heat stabilized, polyamide 6 molding compound developed for applications requiring improved toughness in combination with a balance of strength.. |
|||
Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
BASF Capron® 8334G Impact Modified, 40% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8334G is a heat stabilized, 40% glass fiber reinforced polyamide 6 molding compound developed for applications requiring a high level of stiffness combined with excellent impact performance. .. |
|||
Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
BASF Capron® GR15 15% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron GR15 is a 15% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also.. |
|||
Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
BASF Capron® GR20 HS 20% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron GR20 HS is a heat stabilized 20% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest.. |
|||
Mold Temperature | 95.0 °C | 203 °F | See Materials Notes |
BASF Capron® GR30 HS 30% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron GR30 HS is a heat stabilized 30% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest.. |
|||
Mold Temperature | 95.0 °C | 203 °F | DAM; optimum |
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFR52G45BL BK337 is a 45% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont .. |
|||
Mold Temperature | 95.0 - 110 °C | 203 - 230 °F | |
LATI Latigea B02 H6 Bio-Polymer Bio-Polymer (PLA, PHB, ...). Unfilled. Improved thermal stability. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop.. |
|||
Mold Temperature | >= 95.0 °C | >= 203 °F | |
DuPont Performance Polymers Rynite® 530 BK503 PET
(Unverified Data**) Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, .. |
|||
Mold Temperature | >= 95.0 °C | >= 203 °F | |
DuPont Performance Polymers Rynite® 545 BK504 PET
(Unverified Data**) Rynite® 545 BK504 is a 45% glass reinforced modified polyethylene terephthalate with good strength and stiffness, excellent dimensional stability and creep resistance.Information provided by DuPont.. |
|||
Mold Temperature | 95.0 °C | 203 °F | |
Polyram Polytron A40B02 Nylon 66, 40% Long Fiber A 40% LONG FIBER GLASS REINFORCED BLACK NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind. |