Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 12.8 - 32.2 °C | 55.0 - 90.0 °F | |
PolyOne Versaflex™ CL2000X Thermoplastic Elastomer (TPE) Versaflex™ CL2000X is an ultra-soft TPE designed for use in injection molding applications where exceptional clarity and an extremely soft feel are desired. - Tactile Feel - Ultra-Soft - Water Clar.. |
|||
Mold Temperature | 12.8 - 32.2 °C | 55.0 - 90.0 °F | |
PolyOne Versaflex™ CL2003X Thermoplastic Elastomer (TPE) Versaflex™ CL2003X is an ultra-soft TPE designed for use in injection molding applications where exceptional clarity and ultra-soft properties are desired. New Product. Commercial specifications ha.. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
PolyOne Versaflex™ CL2050 Thermoplastic Elastomer (TPE) Versaflex™ CL2050 is an easy processing compound designed for use in applications where clarity and enhanced heat resistance are required. New Product. Commercial specifications have not been estab.. |
|||
Mold Temperature | 12.8 - 32.2 °C | 55.0 - 90.0 °F | |
PolyOne Versaflex™ FFC 2882-50 Thermoplastic Elastomer (TPE) Versaflex™ FFC 2882-50 is designed to pass several fatty food extraction conditions identified in EU Directive 82/711/EEC. Versaflex™ FFC 2882-50 will also overmold and co-extrude to polypropylene.. |
|||
Mold Temperature | 12.8 - 32.2 °C | 55.0 - 90.0 °F | |
PolyOne Versaflex™ HC 2110-57B Thermoplastic Elastomer (TPE) Versaflex™ HC 2110-57B is a TPE designed for use in the healthcare industry offering low stiction and good compression set. New Product. Commercial specifications have not been established. - Bonds.. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
PolyOne Versaflex™ OM 1040X-1 Thermoplastic Elastomer (TPE) The Versaflex™ OM 1040X-1 is a medical compliant overmolding TPE with very good adhesion to PC or ABS-based plastics. - Good Surface Aesthetics - Rubbery Feel - Soft Touch - Very Good Bond to PC, A.. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
PolyOne Versaflex™ OM 1245X-1 Thermoplastic Elastomer (TPE) The Versaflex™ OM 1245X-1 is designed for overmolding onto polycarbonate (PC), ABS, and PC/ABS susbstrates. - Excellent Bond to PC, ABS, PC/ABS - Rubbery Feel - Soft TouchColor concentrates with EV.. |
|||
Mold Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | |
PolyOne Versaflex™ OM 2262 Thermoplastic Elastomer (TPE) Versaflex™ OM 2262 is a performance overmolding grade with general FDA compliance. This product is designed for both insert and two-shot molding onto Eastman Tritan™ copolyester as well as ABS, PC.. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
PolyOne Versollan™ RU 2204X Thermoplastic Elastomer (TPE) Versollan™ RU 2204X is the first of a new class of high performance, injection moldable TPU alloys developed to offer a rubbery feel and appearance, reduced cycle times, combined with the performan.. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
PolyOne Versollan™ RU 2205-1 Thermoplastic Elastomer (TPE) Versollan™ RU 2205-1 is the first of a new class of high performance, injection moldable TPU alloys developed to offer a rubbery feel and appearance, reduced cycle times, combined with the performa.. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
Northstar Polymers MPC-W44A Polyurethane Gel MPC-W44A is a polyurethane gel formulation specifically designed for padding and cushioning application that requires Shore Durometer OOO scale hardness. Produces good rebound characteristics and g.. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
Northstar Polymers MPP-A30A Polyether Prepolymer This room-temperature-curable polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this s.. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
Northstar Polymers MPP-A60A Liquid Castable Polyurethane MPP-A60A is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott.. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
PolyOne Dynaflex™ D3226-1000-03 Thermoplastic Elastomer (TPE) Dynaflex™ D3226-1000-03 is an easy processing TPE designed for general purpose applications. It is suitable for injection molding, extrusion, blow molding and thermoforming processes. - Dry Feel - .. |
|||
Mold Temperature | 15.6 - 32.2 °C | 60.1 - 90.0 °F | |
PolyOne Dynalloy™ OBC8000-T05 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8000-T05 is an ultra-soft TPE utilizing the unique rubber properties of Dows INFUSE™ Olefin Block Copolymers. This product is designed for injection molding applications where excepti.. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
Northstar Polymers MCG-1 OOO Scale Microcellular Gel Elastomer MCG-1 is formulated for making extremely soft products. MCG-1 has unique structure for this class of material. The cured product will be slightly foamed and give a very soft touch, yet faster resp.. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
Northstar Polymers MPP-A65A High Performance Polyether This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex.. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
Northstar Polymers MPP-A80E High Performance Polyether This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex.. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
Northstar Polymers SAI-1 Low Viscosity Variable Ratio Polyurethane Gel SAI-1 is custom formulated polyurethane gel material to yield very soft elastomer gel material from low viscosity components at room temperature. This material is variable mixing ratio so that the .. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
MRC Polymers MAXTELâ„¢ 600T10-BK TPO, 10% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
MRC Polymers MAXTELâ„¢ 600T25 TPO, 25% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
MRC Polymers MAXTELâ„¢ 600T30IM TPO, 30% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityImpact ModifiedCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Pol.. |
|||
Mold Temperature | 21.1 - 32.2 °C | 70.0 - 90.0 °F | |
MRC Polymers MAXTELâ„¢ 600-BK TPO, Black For automotive exterior applications. Excellent process ability and dimensional stability.Unfilled TPOAvailable in black and gray onlyCan be UV StabilizedInternal and external lubricants can be add.. |