Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products FT4650-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products FT4702-715UV Thermoplastic Polyolefin, UV Stabilized, ZSP Deep Grey Applications: Exterior componentsGrillesBumper trimDoor componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products FT5100-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: IP structural componentBody side moldingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products FT7011-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Claddings and faciasExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products GC20P255-01UV 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, Black Applications: Durable goodsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products HP517-00 23% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trim moldingsSill platesTire coverInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products HP531-00 22% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: IP structural componentsAir ducts - distributionA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products HP531-680UV 22% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Medium Scratch Resistant, BJAA Light Parchment Applications: I/P componentsInterior trimA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products HP532-01 20% Talc Reinforced High Performance Polypropylene, Non-UV Stabilized, Black Applications: Close out panelSpeaker grilleInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products T10P100-01 10% Talc Reinforced Polypropylene, Black Applications: Consumer goodsAir ductsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products T20P100-01 20% Talc Reinforced Polypropylene, Black Applications: Electronic housingsIP componentsHVAC ducts - air distributionClose out panelDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products T20P100-01UV 20% Talc Reinforced Polypropylene, UV Stabilized, General Purpose Black Applications: Durable goodsElectronics housingsIP componentsClose out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products T20P250-00 20% Talc Reinforced Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Air ductsHush panelsWire troughBracketsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 210 - 230 °C | 410 - 446 °F | |
LG Chemical AT-553 Transparent ABS, Permanent Antistatic, Natural and Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Front Barrel Temperature | 210 - 240 °C | 410 - 464 °F | Injection |
Kolon DIAMAT® IH Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Front Barrel Temperature | 210 - 230 °C | 410 - 446 °F | |
LG Chemical LUPOL GP-1000FA General Purpose Polypropylene, High Impact, Flame Retardant, Non-Bleed LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Front Barrel Temperature | 210 - 230 °C | 410 - 446 °F | |
LG Chemical TR-558 Transparent ABS, Humidity Resistance, Natural and Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Front Barrel Temperature | 210 - 230 °C | 410 - 446 °F | |
LG Chemical LUPOL GP-3154F General Purpose Polypropylene, 15% Mineral Fillers, High Modulus, Flame Retardant LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Front Barrel Temperature | 210 - 230 °C | 410 - 446 °F | |
LG Chemical LUPOL HF-3202D High Flow Polypropylene, 20% Mineral Fillers, High Impact LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Front Barrel Temperature | 210 - 230 °C | 410 - 446 °F | |
LG Chemical LUPOL LW-4407 Low Warpage Polypropylene, 40% Glass Fiber/Mineral Filler Reinforced, Heat Resistant LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Front Barrel Temperature | 210 - 230 °C | 410 - 446 °F | |
LG Chemical LUPOL TE-5102 Thermoplastic Elastomer Alloy, 10% Polymer Alloy, High Impact LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Front Barrel Temperature | 210 - 230 °C | 410 - 446 °F | |
LG Chemical LUPOS GP-2200H General Purpose ABS, 20% Glass Fiber Reinforced, High Heat Resistance LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Front Barrel Temperature | 210 - 220 °C | 410 - 428 °F | |
Solvay TECHNYL® C 442 Black V PA6, DRY Description: Unreinforced polyamide PA6, high viscosity, with high flexibility and very high impact resistance even at low temperature, for extrusion.Available in: Europe Product Applications: It ha.. |
|||
Front Barrel Temperature | 210 - 230 °C | 410 - 446 °F | |
Samsung Cheil Industries Starex® SD-0150GP High Impact Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 210 - 230 °C | 410 - 446 °F | |
Borealis Borcoat™ EA165E Elastomer Modified Polypropylene for Extrusion Borcoat EA165E is an elastomer modified compound, based on a high molecular weight copolymer. The elastomer modification gives excellent low temperature impact resistance.Borcoat EA165E is recommen.. |
|||
Front Barrel Temperature | 210 - 240 °C | 410 - 464 °F | Tube Extrusion |
Arkema Group KYNAR FLEX® 3120-15 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness.. |
|||
Front Barrel Temperature | 210 - 240 °C | 410 - 464 °F | Tube Extrusion |
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Front Barrel Temperature | 210 - 224 °C | 410 - 435 °F | |
Ravago Manufacturing Americas Hylac® GP30G ABS, 30% Glass Fiber Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products GC20P255-01 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: BracketsUnderhood componentsElectrical housingsHeadlamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products GC20P600-01UV 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, Black Applications: Sun roof trimFan shroudInjection molding conditions reported in table.Information provided by RheTech Products. |