| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Front Barrel Temperature | 193 - 224 °C | 379 - 435 °F | |
| PolyOne Versalloy™ HC 9220-70 Thermoplastic Elastomer (TPE) Versalloy™ HC 9220-70 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr.. |
|||
| Front Barrel Temperature | 193 - 224 °C | 379 - 435 °F | |
| PolyOne Versalloy™ HC 9220-80 Thermoplastic Elastomer (TPE) Versalloy™ HC 9220-80 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr.. |
|||
| Front Barrel Temperature | 210 - 224 °C | 410 - 435 °F | |
| Ravago Manufacturing Americas Hylac® GP74G20 ABS, 20% Glass Fiber Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
| Front Barrel Temperature | 191 - 224 °C | 376 - 435 °F | |
| Ineos Nova Zylar® 220 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features:High clarity Good elongation Styrenic processing advantages Excellent property retention after gamma and ETO sterilization Meets USP XXIII specifications for Class VI plasticsApplications:D.. |
|||
| Front Barrel Temperature | 184 - 224 °C | 364 - 436 °F | |
| Teknor Apex Uniprene® 7010-64NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
| Front Barrel Temperature | 184 - 224 °C | 364 - 436 °F | |
| Teknor Apex Uniprene® UN-1140A Thermoplastic Elastomer Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
| Front Barrel Temperature | 184 - 224 °C | 364 - 436 °F | |
| Teknor Apex Uniprene® UN-2012-L3 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
| Front Barrel Temperature | 184 - 224 °C | 364 - 436 °F | |
| Teknor Apex Uniprene® UN-2028A UMB Thermoplastic Elastomer Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
| Front Barrel Temperature | 184 - 224 °C | 364 - 436 °F | |
| Teknor Apex Uniprene® UN-2420D Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
| Front Barrel Temperature | 184 - 224 °C | 364 - 436 °F | |
| Teknor Apex Uniprene® UN-2598A Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
| Front Barrel Temperature | 184 - 224 °C | 364 - 436 °F | |
| Teknor Apex Uniprene® UN-2598D Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
| Front Barrel Temperature | 184 - 224 °C | 364 - 436 °F | |
| Teknor Apex Uniprene® UN-2598E Thermoplastic Vulcanizate Alloy Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
| Front Barrel Temperature | 184 - 224 °C | 364 - 436 °F | |
| Teknor Apex Uniprene® UN-2640S Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
| Front Barrel Temperature | 184 - 224 °C | 364 - 436 °F | |
| Teknor Apex Uniprene® UN-2678C Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
| Front Barrel Temperature | 184 - 224 °C | 364 - 436 °F | |
| Teknor Apex Uniprene® UN-7010-45NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin.. |
|||
| Front Barrel Temperature | 184 - 224 °C | 364 - 436 °F | |
| Teknor Apex Uniprene® UN-7010-73NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin.. |
|||
| Front Barrel Temperature | 184 - 224 °C | 364 - 436 °F | |
| Teknor Apex Uniprene® UN-7010-80NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin.. |
|||
| Front Barrel Temperature | 184 - 224 °C | 364 - 436 °F | |
| Teknor Apex Uniprene® UN-7010-87NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin.. |
|||
| Front Barrel Temperature | 184 - 224 °C | 364 - 436 °F | |
| Teknor Apex Uniprene® UN-7100-55 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
| Front Barrel Temperature | 184 - 224 °C | 364 - 436 °F | |
| Teknor Apex Uniprene® UN-7100-87 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
| Front Barrel Temperature | 184 - 224 °C | 364 - 436 °F | |
| Teknor Apex Uniprene® 7010-73NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
| Front Barrel Temperature | 184 - 224 °C | 364 - 436 °F | |
| Teknor Apex Uniprene® UN-2420H Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
| Front Barrel Temperature | 184 - 224 °C | 364 - 436 °F | |
| Teknor Apex Uniprene® UN-2533A Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
| Front Barrel Temperature | 184 - 224 °C | 364 - 436 °F | |
| Teknor Apex Uniprene® UN-7100-40D Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
| Front Barrel Temperature | 184 - 224 °C | 364 - 436 °F | |
| Teknor Apex Uniprene® UN-7100-45 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
| Front Barrel Temperature | 184 - 224 °C | 364 - 436 °F | |
| Teknor Apex Uniprene® UN-7100-80 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
| Front Barrel Temperature | 191 - 224 °C | 376 - 435 °F | |
| Ineos Nova Zylar® 530 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features:High clarityStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationMeets USP XXIII specifications for Class VI plasticsUL94 HB @ 1.5 mm for uncolored ma.. |
|||
| Front Barrel Temperature | 191 - 224 °C | 376 - 435 °F | |
| Ineos Nova Zylar® 535 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features: High clarity, strength and toughnessStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationAnti-stat packageEnhanced mold releaseUL 94HB @ 1.5 mm for a.. |
|||
| Front Barrel Temperature | 191 - 224 °C | 376 - 435 °F | |
| Ineos Nova Zylar® 631 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features:Outstanding practical toughness and ductilityStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationUSP Class VI compliantCustom colors and enhancement .. |
|||
| Front Barrel Temperature | 210 - 224 °C | 410 - 435 °F | |
| Ravago Manufacturing Americas Hylac® GP30G ABS, 30% Glass Fiber Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||