Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
Polymer Resources PC-FR2-D Polycarbonate, Improved Flame Retardant, Medium Flow Polycarbonate, Improved Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted.. |
|||
Front Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
Polymer Resources PC-FR-IM1 Polycarbonate, Preliminary Data Sheet, Low Temperature Impact and Flame Retardant Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
Polymer Resources PC-GP2-D Polycarbonate, General Purpose, Medium Flow Polycarbonate, General Purpose, Medium FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on.. |
|||
Front Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
Polymer Resources PC-GP2-D-[color]-1 Polycarbonate, General Purpose, Medium Flow with Mold Release Polycarbonate, General Purpose, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf.. |
|||
Front Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
Polymer Resources PC-IM1 Polycarbonate, Impact Modified, Low Flow Polycarbonate, Impact Modified, Low FlowProcess: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided .. |
|||
Front Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
Polymer Resources PC-IM1-UV Polycarbonate, Impact Modified, Low Flow, UV-stabilized Polycarbonate, Impact Modified, Low Flow, UV-stabilizedProcess: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Front Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
Polymer Resources PC-UV2-D-[color]-1 Polycarbonate, UV-stabilized, Medium Flow with Mold Release Polycarbonate, UV-stabilized, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Front Barrel Temperature | 282 - 316 °C | 540 - 600 °F | |
Polymer Resources PPX-FR6 Modified-PPO, V-0 Flame Retardant Modified-Polyphenylene Oxide, V-0 Flame Retardant, 300F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Front Barrel Temperature | 282 - 316 °C | 540 - 600 °F | |
Polymer Resources PPX-G10HF Modified-PPO, 10% Glass Reinforced, High Flow Modified-Polyphenylene Oxide, 10% Glass Reinforced, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf.. |
|||
Front Barrel Temperature | 282 - 316 °C | 540 - 600 °F | |
Polymer Resources PPX-G30 Modified-PPO, 30% Glass Reinforced Modified-Polyphenylene Oxide, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Front Barrel Temperature | 282 - 316 °C | 540 - 600 °F | |
Polymer Resources PPX-GP5 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 270F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Front Barrel Temperature | 282 - 316 °C | 540 - 600 °F | |
Polymer Resources PPX-GP6 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 290F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Front Barrel Temperature | 282 - 316 °C | 540 - 600 °F | |
Polymer Resources PPX-GP7 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 300F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Front Barrel Temperature | 282 - 316 °C | 540 - 600 °F | |
Polymer Resources PPX-MF-FRG20 Modified-PPO, 40% Glass/Mineral Reinforced, Flame Retardant Modified-Polyphenylene Oxide, 40% Glass/Mineral Reinforced, Flame RetardantFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanica.. |
|||
Front Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
Polymer Resources PC-FD2 Polycarbonate, FDA-compliant Feedstocks, Medium Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Medium Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Front Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
Polymer Resources PC-UV2-D Polycarbonate, UV-stabilized, Medium Flow Polycarbonate, UV-stabilized, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Front Barrel Temperature | 288 - 316 °C | 550 - 600 °F | |
Star Plastics PC1212FR Molding Grade PC FR Information provided by Star Plastics, Inc. |
|||
Front Barrel Temperature | 288 - 316 °C | 550 - 600 °F | |
Star Plastics PC1212FRR Molding Grade PC FR Information provided by Star Plastics, Inc. |
|||
Front Barrel Temperature | 288 - 316 °C | 550 - 600 °F | |
Star Plastics PC1212FRRUV Molding Grade PC FR Information provided by Star Plastics, Inc. |
|||
Front Barrel Temperature | 288 - 316 °C | 550 - 600 °F | |
Star Plastics PC1212FRUV Molding Grade PC FR Information provided by Star Plastics, Inc. |
|||
Front Barrel Temperature | 288 - 316 °C | 550 - 600 °F | |
Star Plastics PC1510R Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Front Barrel Temperature | 288 - 316 °C | 550 - 600 °F | |
Star Plastics PC1510R Molding Grade PC with Release Information provided by Star Plastics, Inc. |
|||
Front Barrel Temperature | 288 - 316 °C | 550 - 600 °F | |
Star Plastics PC703 Molding Grade PC with release Information provided by Star Plastics, Inc. |
|||
Front Barrel Temperature | 282 - 316 °C | 540 - 600 °F | |
Polymer Resources PPX-FR6 Modified PPO, UL 94 V-0 with HDT of 300 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 282 - 316 °C | 540 - 600 °F | |
Polymer Resources PPX-G20 Modified PPO, 20% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 282 - 316 °C | 540 - 600 °F | |
Polymer Resources PPX-GP5 Modified PPO, General Purpose with HDT of 270 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 282 - 316 °C | 540 - 600 °F | |
Polymer Resources PPX-GP6 Modified PPO, General Purpose with HDT of 290 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 282 - 316 °C | 540 - 600 °F | |
Polymer Resources PPX-GP7 Modified PPO, General Purpose with HDT of 300 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
LTL Color Compounds ColorFast® FRPC300 Polycarbonate, Flame-Retarded V2-rated polycarbonateAll information provided by LTL Color Compounders, Inc. |
|||
Front Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
LTL Color Compounds ColorFast® FRPC400 Polycarbonate, Flame-Retarded Flame-retarded V0, high impact injection molding polycarbonateAll information provided by LTL Color Compounders, Inc. |