Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 215 - 240 °C | 419 - 464 °F | Start Point: 225°C |
Kingfa FRHIPS-960PC Flame Retardant Polystyrene Features:UL 94 V-0 @ 3.2mmNon-DPO, UV stabilityExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV and audio housingElectrical appliance housingInforma.. |
|||
Front Barrel Temperature | 215 - 240 °C | 419 - 464 °F | Start Point: 225°C |
Kingfa HIPS-5197 High Impact Polystyrene Features:UL 94 HB @ 1.6mmExcellent balance propertiesHigh mechanical strengthGood heat stabilityColor tailor-made for clientsApplications:Injection moldingGas assistant moldingTV & Audio housingElec.. |
|||
Front Barrel Temperature | 230 - 240 °C | 446 - 464 °F | Injection Molding |
LG Chemical ER451 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica.. |
|||
Front Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical KEYFLEX BT 1055D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Front Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical LG704W ABS, Low Gloss, Heat Resistance Feature: Injection Molding, Low Gloss, Heat ResistanceApplication: Automobiles Interior Housing (Column Cover, Filllar Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by LG Chem.. |
|||
Front Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical LG709W ABS, Low Gloss, Heat Resistance Injection Molding, Low Gloss, Heat ResistanceApplication: Automobiles Interior Housing (Column Cover, Pilllars, Etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG.. |
|||
Front Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical LI951 Heat Resistant ASA Description: High Heat ASAApplication: Automotive Part (Radiator Grill, Side Mirror)CAS: 26299-47-8Information provided by LG Chemical |
|||
Front Barrel Temperature | 210 - 240 °C | 410 - 464 °F | Injection |
Kolon DIAMAT® EH Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Front Barrel Temperature | 210 - 240 °C | 410 - 464 °F | Injection |
Kolon DIAMAT® EM Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Front Barrel Temperature | 210 - 240 °C | 410 - 464 °F | Injection |
Kolon DIAMAT® IH Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Front Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical LUPOS GP2100 ABS+GF10%, General Purpose Feature: Injection Molding, ABS+GF10%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7 and 65997-17-3Information provided by LG Chemical |
|||
Front Barrel Temperature | 210 - 240 °C | 410 - 464 °F | Injection |
Inno-Comp INNOPOL® CS 2-2130 30% Talc Filled Polypropylene Copolymer INNOPOL® CS 2-2130 is a 30 % talc-filled polypropylene compound /PP-B TD30 (ISO 1043)/. This grade is available in natural and custom colored form.INNOPOL® CS 2-2130 is recommended for produci.. |
|||
Front Barrel Temperature | 190 - 240 °C | 374 - 464 °F | Injection |
Inno-Comp INNOPOL® CS 3-9120 SR5 17% Talc Filled Polypropylene Blend INNOPOL® CS 3-9120 SR5 is a 17% talc-filled compound based on blend of polypropylene block copolymer and homopolymer. This grade is available in natural and custom colored form.INNOPOL® CS 3-9.. |
|||
Front Barrel Temperature | 230 - 240 °C | 446 - 464 °F | Injection Molding |
LG Chemical XR401B ABS, High Flow, Heat Resistance Feature: Injection Molding, High Flow, Heat ResistanceApplication: Automotives Exterior Housing (Side Mirror Housing, Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information p.. |
|||
Front Barrel Temperature | 230 - 240 °C | 446 - 464 °F | Injection Molding |
LG Chemical XR409HJ ABS, Heat Resistance, Curl Fit Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior & Exterior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by .. |
|||
Front Barrel Temperature | 215 - 240 °C | 419 - 464 °F | Start Point: 225°C |
Kingfa FRHIPSV-0 Flame Retardant Polystyrene Features:UL 94 V-0 @ 1.6mm, V-0 @ 3.2mmExcellent balance propertiesHigh mechanical strengthGood heat stabilityColor tailor-made for clientApplications:Injection moldingGas assistant moldingTV or aud.. |
|||
Front Barrel Temperature | 230 - 240 °C | 446 - 464 °F | Injection Molding |
LG Chemical XR401 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (lamp housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 .. |
|||
Front Barrel Temperature | 230 - 240 °C | 446 - 464 °F | Injection Molding |
LG Chemical XR404 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Inf.. |
|||
Front Barrel Temperature | 230 - 240 °C | 446 - 464 °F | |
Solvay TECHNYL® C 206 PA6, DRY Description: Unreinforced Polyamide PA6, standard for fast cycling, for injection molding.Available in: EuropeProduct Applications: TECHNYL® C 206 has fluidity and a good mould release, favored b.. |
|||
Front Barrel Temperature | 230 - 240 °C | 446 - 464 °F | |
Solvay TECHNYL® C 216 PA6, DRY Description: Unreinforced polyamide PA6, standard nucleation for fast cycling, for injection molding.Available in: Asia PacificProduct Applications: This grade has a high fluidity and good mould rel.. |
|||
Front Barrel Temperature | 230 - 240 °C | 446 - 464 °F | |
Solvay Technyl® C206F Unfilled, Fast Cycle Nylon 6 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Front Barrel Temperature | 220 - 240 °C | 428 - 464 °F | H3 |
Samsung Cheil Industries Starex® WR-9140 General Purpose ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Pre-3. Region Temperature |
Tisan TISLAMID® 6 30% Glass Fiber Reinforced Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Front Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Pre-3. Region Temperature |
Tisan TISLAMID® 6 Flame Retardant (V0) Heat Stabilized Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Front Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Pre-3. Region Temperature |
Tisan TISLAMID® 6 UNR Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Front Barrel Temperature | 210 - 240 °C | 410 - 464 °F | Tube Extrusion |
Arkema Group KYNAR FLEX® 2800-01 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical s.. |
|||
Front Barrel Temperature | 210 - 240 °C | 410 - 464 °F | Tube Extrusion |
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Front Barrel Temperature | 210 - 240 °C | 410 - 464 °F | Tube Extrusion |
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Front Barrel Temperature | 210 - 240 °C | 410 - 464 °F | Tube Extrusion |
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Front Barrel Temperature | 210 - 240 °C | 410 - 464 °F | Tube Extrusion |
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low.. |