Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 210 - 220 °C | 410 - 428 °F | |
Huntsman AVALON® 98 AB Thermoplastic Polyurethane Introduction: AVALON 98 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 98 AB is part of the AVALON Performance Range and offers a premium soling ma.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical AF312A ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical AF312B ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical ER460 ABS, Medium Heat Resistance, High Flowability Feature: Injection Molding, Medium Heat Resistance, High FlowabilityApplication: Automobile, Motor Cycle, Electric & Electronic GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical HF380I ABS, High Flow Feature: Injection Molding, High Flow, Good PaintabilityApplication: Painting Products of Motor Cycle)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical HG173 ABS, High Surface Gloss Feature: Injection Molding, High Surface GlossApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical HI100 ABS, High Impact Feature: Injection Molding, High ImpactApplication: Helmet, Pipe & Fittings, Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
LG Chemical LUCEL EC-610B Electrically Conductive POM, 10% Carbon Black Filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical LUCEL GC210 POM+GF10%, High Rigidity Feature: Injection Molding, POM+GF10%, High RigidityApplication: Casings of Pump and Pivot BearingsCAS No. 66455-31-0 and 65997-17-3Information provided by LG Chemical |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical LUCEL GC225 POM+GF25%, High Rigidity Feature: Injection Molding, POM+GF25%, High RigidityApplication: Casings of Pump and Pivot BearingsCAS No. 66455-31-0 and 65997-17-3Information provided by LG Chemical |
|||
Front Barrel Temperature | 180 - 220 °C | 356 - 428 °F | Extrusion |
Inno-Comp INNOPOL® CS 2-7120 20% Talc Filled Polypropylene Copolymer INNOPOL® CS 2-7120 is a 20 % talc-filled polypropylene block-copolymer compound /PP-B TD20 (ISO 1043)/. This grade is available in natural and custom colored form.INNOPOL® CS 2-7120 is recomme.. |
|||
Front Barrel Temperature | 210 - 220 °C | 410 - 428 °F | |
Lavergne VYTEEN ABS 2901 Acrylonitrile Butadiene Styrene Vyteen ABS 2901 is a black recycled general purpose ABS terpolymer with balanced impact/stiffness properties designed for injection molding applications.Features: -Good resilience -Good processabi.. |
|||
Front Barrel Temperature | 210 - 220 °C | 410 - 428 °F | |
Huntsman AVALON® 90 AK Thermoplastic Polyurethane Introduction: AVALON 90 AK is a part of the AVALON Crystal Range and offers a specially designed, flexible material wit a higher degree of transparency compared with conventional TPU at the same har.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical AF308 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
Stellarchem AB835EM TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
Stellarchem DIOSHY® GP-935-UB2 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
Stellarchem GP-860HD TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
Stellarchem GP-9401 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
Stellarchem LP-845 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
Stellarchem LP-855 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
Stellarchem MP-8001 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
Samyang Tribit® 1503 Polybutylene Terephthalate Characteristics:High flow & processabilityApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll information provid.. |
|||
Front Barrel Temperature | 180 - 220 °C | 356 - 428 °F | Injection |
Samyang Triel® 5400 Thermoplastic Polyether Ester Elastomer TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor r.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
Borealis BorECO™ BA212E Polypropylene Block Copolymer for Non-Pressure Pipes BorECO BA212E is a high molecular weight, low melt flow rate polypropylene block copolymer with very high stiffness and impact strength.BorECO BA212E is recommended for solid wall and structured wal.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
Borealis BorECO™ BA222E Polypropylene Block Copolymer for Non-Pressure Pipes BorECO BA222E is a high molecular weight, low melt flow rate polypropylene block copolymer with superior stiffness and excellent impact properties. BorECO BA222E fulfills the requirements according.. |
|||
Front Barrel Temperature | 180 - 220 °C | 356 - 428 °F | |
Unitika TERRAMAC TE-1030 Polylactic Acid (PLA) High-Impact grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Front Barrel Temperature | 180 - 220 °C | 356 - 428 °F | |
Unitika TERRAMAC TE-1070 Polylactic Acid (PLA) High-Impact grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | |
Chi Mei Acryrex® CM-207 PMMA Features:General PurposeGood Weather ResistanceHigh GlossHigh Heat ResistanceHigh StrengthMedium ViscosityUses: Automotive Interior PartsBathroom AccessoriesContainersCosmeticsHousehold GoodsKnobsRo.. |
|||
Front Barrel Temperature | 180 - 220 °C | 356 - 428 °F | Injection |
Samyang Triel® 5300 Thermoplastic Polyether Ester Elastomer TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor rec.. |
|||
Front Barrel Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
LG Chemical SG175G ABS, Super Surface Gloss, High Flow Feature: Injection Molding, Super Surface Gloss, High FlowApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical |