Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 238 - 249 °C | 460 - 480 °F | |
Ravago Manufacturing Americas Hybrid S464 ABS + Polycarbonate Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Middle Barrel Temperature | 238 - 249 °C | 460 - 480 °F | |
Firestone C200-001 Nylon 6 Natural color. Not heat stabilized, modified, or lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone |
|||
Middle Barrel Temperature | 238 - 249 °C | 460 - 480 °F | |
Firestone CL200-001 Nylon 6 Natural color. Not heat stabilized or modified. Lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone |
|||
Middle Barrel Temperature | 238 - 249 °C | 460 - 480 °F | |
Entec Hylox® 9020 PBT, 20% Glass Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Middle Barrel Temperature | 238 - 249 °C | 460 - 480 °F | |
Entec Hylox® 9030 PBT, 30% Glass Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Middle Barrel Temperature | 238 - 249 °C | 460 - 480 °F | |
Entec Hylox® 9015 PBT, 15% Glass Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Middle Barrel Temperature | 235 - 249 °C | 455 - 480 °F | |
A. Schulman ComAlloy Hiloy® 414 Polyester - PBT, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.45% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Middle Barrel Temperature | 235 - 249 °C | 455 - 480 °F | |
A. Schulman ComAlloy Hiloy® 415 Polyester - PBT, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Middle Barrel Temperature | 235 - 249 °C | 455 - 480 °F | |
A. Schulman ComAlloy Hiloy® 419 Polyester - PBT, Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.40% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Middle Barrel Temperature | 235 - 249 °C | 455 - 480 °F | |
A. Schulman ComAlloy Hiloy® 420 Polyester - PBT, Glass/Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.30% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Middle Barrel Temperature | 235 - 249 °C | 455 - 480 °F | |
A. Schulman ComAlloy Hiloy® 421 Polyester - PBT, Glass/Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.45% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Middle Barrel Temperature | 235 - 249 °C | 455 - 480 °F | |
A. Schulman ComAlloy Hiloy® 422 Heavy Mineral Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.40% Heavy Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Middle Barrel Temperature | 235 - 249 °C | 455 - 480 °F | |
A. Schulman ComAlloy Hiloy® 435 Glass/Mineral Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.50% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Middle Barrel Temperature | 235 - 249 °C | 455 - 480 °F | |
A. Schulman ComAlloy Hiloy® 436 Glass/Mineral Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.20% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Middle Barrel Temperature | 235 - 249 °C | 455 - 480 °F | |
A. Schulman ComAlloy Voloy® 413 Polyester - PBT, Glass Reinforced, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Middle Barrel Temperature | 235 - 249 °C | 455 - 480 °F | |
A. Schulman ComAlloy Voloy® 415 Polyester - PBT, Glass/Mineral Reinforced, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.30% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Middle Barrel Temperature | 235 - 249 °C | 455 - 480 °F | |
A. Schulman ComAlloy Voloy® 417 Polyester - PBT, Glass/Mineral Reinforced, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.43% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Middle Barrel Temperature | 235 - 249 °C | 455 - 480 °F | |
A. Schulman ComAlloy Voloy® 462 Glass/Mineral Reinforced, PBT Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.35% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Middle Barrel Temperature | 232 - 249 °C | 450 - 480 °F | |
Polymer Resources PC/TP-GP3 PC Polyester, High Impact, Superior Chemical Resistance
(Unverified Data**)&l Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |