Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 193 - 232 °C | 380 - 450 °F | |
Multibase Multi-Pro® 2510 XGW Polypropylene Mineral Filled, 27% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Middle Barrel Temperature | 193 - 232 °C | 380 - 450 °F | |
Multibase Multi-Pro® 3018 XUG Polypropylene Mineral Filled, 30% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingUses:AppliancesFurnitureInformation provided by Multibase |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT1001-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Facias, claddings, and rocker panelsBodyside moldingsStep pads and bumper componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT2500-630UV Thermoplastic Polyolefin, UV Stabilized, 500F Light Charcoal Applications: Air DamsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT2600-00UV Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Interior trimSplash shieldScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT2700-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Air deflectorsFuel filler shieldsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products P102-00 Polypropylene, Black Applications: Consumer goodsIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products P249-01UV General Purpose Polypropylene Copolymer, UV Stabilized, Black Applications: LP bracketsSplash shieldsDoor/trunk scuffInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products P250-00 Polypropylene Copolymer, Natural Applications: ConsolesComponent housingsInterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products P250-00UV Polypropylene Copolymer, UV Stabilized, Natural Applications: ConsolesConsumer goodsInterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products P252-00 Polypropylene Copolymer, Natural Applications: Interior trimUnderhood componentsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products P252-670UV Polypropylene Copolymer, UV Stabilized, 134B Stone Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products P252-674UV Polypropylene Copolymer, UV Stabilized, 447B Fawn Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products P256-00 Polypropylene Copolymer, Natural Applications: Door/trunk scuffUnderhood componentsSplash shieldsElectrical enclosuresInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products P256-01A Polypropylene Copolymer, Black Applications: Lower IP componentsUnderhood clipsGlove box binInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products P256-762 Polypropylene Copolymer, Medium Grey Applications: Misc. ClipsElectrical housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 232 °C | 380 - 450 °F | |
Multibase Multi-Pro® 2510 XG Polypropylene Mineral Filled, 25% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingUses:AppliancesFurnitureInformation provided by Multibase |
|||
Middle Barrel Temperature | 193 - 210 °C | 380 - 410 °F | |
Fiberfil® PP-60/VO Polypropylene Homopolymer, Flame Retardant, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 193 - 210 °C | 380 - 410 °F | |
Fiberfil® PP-60/VO/NH Polypropylene Homopolymer, Flame Retardant, non-halogenated, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 193 - 216 °C | 380 - 420 °F | |
MRC Polymers MAXTELâ„¢ 600T30IM TPO, 30% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityImpact ModifiedCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Pol.. |
|||
Middle Barrel Temperature | 193 °C | 380 °F | |
Multibase Multi-Flex® TEA 4001-35 Natural TPO Thermoplastic Polyolefin Elastomer Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Middle Barrel Temperature | 193 °C | 380 °F | |
Multibase Multi-Flex® TEA 4001-65 TPO Thermoplastic Polyolefin Elastomer Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Middle Barrel Temperature | 193 - 227 °C | 380 - 440 °F | |
CTC SunPro® SP 200 P 3085 Polypropylene Copolymer SunPro® SP 200 P 3085 is a general purpose, medium flow, polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Certifications: GM.PP... |
|||
Middle Barrel Temperature | 193 - 227 °C | 380 - 440 °F | |
CTC SunPro® SP 200 P 5000 Polypropylene Copolymer SunPro® SP 200 P 5000 is a general purpose, medium flow, polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Certifications: MS DB5.. |
|||
Middle Barrel Temperature | 193 - 227 °C | 380 - 440 °F | |
CTC SunPro® SP 200 P4058 Polypropylene Copolymer SunPro® SP 200 P 4058 is a general purpose, medium flow, polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Certifications: Chrysl.. |
|||
Middle Barrel Temperature | 193 - 227 °C | 380 - 440 °F | |
CTC X-PRO CTC PP 2019 Polypropylene Impact Copolymer X-PRO PP 2019 is a high impact, polypropylene copolymer. It has automotive and industrial general purpose applications.Data provided by Composite Technologies (CTC). |
|||
Middle Barrel Temperature | 193 - 227 °C | 380 - 440 °F | |
CTC X-PRO CTC PP2020 Polypropylene Impact Copolymer X-PRO PP 2020 is an impact, polypropylene copolymer. It has automotive and industrial general purpose applications.Data provided by Composite Technologies (CTC). |
|||
Middle Barrel Temperature | 193 - 232 °C | 380 - 450 °F | |
Multibase Multi-Pro® 4007 XGS Polypropylene Mineral, 40% by weight.Features:Gloss, HighScratch ResistantForms:PelletsProcessing Methods:Injection MoldingUses: FurnitureAppliancesInformation provided by Multibase |
|||
Middle Barrel Temperature | 193 - 227 °C | 380 - 440 °F | |
LTL Color Compounds ColorFast® FRPS100 Styrene, High Impact V1-rated high impact styreneAll information provided by LTL Color Compounders, Inc. |