Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50/CF/10/GF/20/BK Polycarbonate, with carbon fiber and glass fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50/CF/10/TF/15/BK 100 Polycarbonate, with carbon fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50/CF/15/TF/15/SI/2/BK Polycarbonate, with carbon fiber, PTFE, lubricant modified Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50/CF/15/TF/15/SI/2/BK-HB Polycarbonate, with carbon fiber, PTFE, lubricant modified Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50/CF/30 Polycarbonate, with carbon fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50/TF/15/BK-1 Polycarbonate, with PTFE, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50/TF/15/GY04 Polycarbonate, with PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50/TF/15/NAT Polycarbonate, with PTFE, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50-7154 Polycarbonate, with carbon fiber, low-warpage Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Reduced moment of inertia compared with me.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50-7154/V0 Polycarbonate, with carbon fiber, low-warpage Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Reduced moment of inertia compared with me.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50-7216 Polycarbonate, with PTFE, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50-7224/V0 Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Reduced moment of inertia compared with metal parts.Improved f.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50-7228 Polycarbonate, with carbon fiber, glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Electrically conductive, suitable for cont.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50-7317 Polycarbonate, with PTFE, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50-7644 Polycarbonate, with carbon fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Electrically conductive, suitable for cont.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50-7814/EM Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50-7856/FR/BK Polycarbonate, with carbon fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50-8076 Polycarbonate, with carbon fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts with low warpage and.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50-8376 Polycarbonate, unreinforced Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical engineering.Antistatic.Isotropic shrinkage characteristics.Reduced moment.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50-8479/BL-1 Polycarbonate, unreinforced Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Isotropic shrinkage characteristics.Reduced moment of inertia .. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss ELECTRAFIL M-2386 Polycarbonate, with carbon fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Electrically conductive, suitable for cont.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss LUVOCOM® 50/GF/20/TF/20/GY Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Zone 3 | 300 - 320 °C | 572 - 608 °F | |
Lehmann & Voss PLASLUBE J-50/10/TF/15/BK Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts, even at elevated te.. |