Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 3 | 240 - 270 °C | 464 - 518 °F | |
Nilit Nilamid B3 H XB Unfilled, Impact Resistant PA6 Description: Nilamid B3 H XB is a high impact NYLON 6. The product has excellent impact properties above 0°C, combined with good maintaining mechanical characteristics. Application areas include au.. |
|||
Zone 3 | 240 - 270 °C | 464 - 518 °F | |
Nilit Nilamid B3 H ZA Unfilled, Low Temperature Impact Resistant PA6 Description: Nilamid B3 H ZA is a NYLON 6 with a low level of impact modification, allowing parts to be snap fitted in a dry-as-molded condition. It also has improved impact strength and elongation,.. |
|||
Zone 3 | 240 - 270 °C | 464 - 518 °F | |
Nilit Nilamid B3 H ZB Unfilled, Low Temperature Impact Resistant PA6 Description: Nilamid B3 H ZB is a high impact NYLON 6. The product has excellent impact properties, even at minus temperatures, whilst maintaining mechanical characteristics. Application areas inclu.. |
|||
Zone 3 | 240 °C | 464 °F | Injection Molding |
UBE UBESTA® 3020GX9 23% Glass Fiber Reinforced Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: 23% glass fiber reinforced gradeInformation provided by UBE. |
|||
Zone 3 | 240 °C | 464 °F | Injection Molding |
UBE UBESTA® 3035UF Rigid Piping Grade Nylon 12 Description: UBESTA contributes to the field of Utilities such as plastic pipe system evolutionary developed for gas industry. It is used for both burial and for rehabilitation of existing cast iron.. |
|||
Zone 3 | 240 - 260 °C | 464 - 500 °F | |
Eurostar Staramide BG2ST43 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide BG2ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 240 - 260 °C | 464 - 500 °F | |
Eurostar Staramide BG6ST01 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide BG6ST01 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 240 - 270 °C | 464 - 518 °F | |
Eurostar Staramide BG7H PA6, 35% Glass Fiber Filled, Heat Stabilized, Injection Molded Staramide BG7H is a Heat Stabilized, 35% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 240 - 270 °C | 464 - 518 °F | |
Eurostar Staramide BT6 PA6, 30% Mineral Filled, Injection Molded Staramide BT6 is a 30% Mineral Filled, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 240 - 250 °C | 464 - 482 °F | |
Eurostar Staramide P1000IX3 PA6, Impact Modified, Injection Molded Staramide P1000IX3 is an Impact Modified, Polyamide 6 Injection Molding Resin (also known as P1000HI020 or Star X 2020)Information provided by Eurostar. |
|||
Zone 3 | 240 - 270 °C | 464 - 518 °F | |
Eurostar Staramide PF005 PA6, 25% Glass Fiber Filled, Injection Molded Staramide PF005 is an 25% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 240 °C | 464 °F | |
Eurostar Starpylen HT 25 MC PP, Mineral Filled, Injection Molding Starpylen HT 25 MC is a Mineral Filled Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 240 - 260 °C | 464 - 500 °F | |
Eurostar Star L PA6 D36 PA6, Injection Molded Star L PA6 D36 is a MOS2 Lubricated Unreinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 240 - 260 °C | 464 - 500 °F | |
Eurostar Star L PA6 D61 PA6, Injection Molded Star L PA6 D61 is a PTFE/Silicone Oil Lubricated, Unreinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 240 - 270 °C | 464 - 518 °F | |
Eurostar Staramide PF007 PA6, 35% Glass Fiber Filled, Injection Molded Staramide PF007 is a 35% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 240 - 260 °C | 464 - 500 °F | |
Eurostar Star L PA6 D83 PA6, Injection Molded Star L PA6 D83 is a PTFE/Proprietary Additive Lubricated, Unreinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |