Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 240 °C | 464 °F | Die |
Premix Thermoplastics PRE-ELEC® ABS 1415 Conductive Thermoplastic Compound PRE-ELEC® ABS 1415 is a conductive thermoplastic compound based on ABS. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® ABS.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | hopper |
Nilit Nilamid B G6 FR C4 30% Glass Fiber Reinforced, Flame Retardant PA6 Description: Nilamid B G6 FR C4 combines excellent mechanical performance with flame retardancy. The halogenated flame retardant system used in this product allows a wide range of colors. This produ.. |
|||
Zone 1 | 240 - 270 °C | 464 - 518 °F | hopper |
Nilit Nilamid B3 H G10 50% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G10 is a product that combines outstanding strength and stiffness with good moldability and good impact strength. It is widely used for structural applications.Key characte.. |
|||
Zone 1 | 240 - 270 °C | 464 - 518 °F | hopper |
Nilit Nilamid B3 H G3 15% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 6. These products combine good overall mechanical performance and impact strength with ease of processing. Key cha.. |
|||
Zone 1 | 240 - 270 °C | 464 - 518 °F | hopper |
Nilit Nilamid B3 H G6 30% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G6 is a general purpose, 30% glass fiber reinforced NYLON 6 with a combination of good mechanical performance, impact strength and processability. It is one of the most wid.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850/GF/30/TF/13/SI/2 PBT, with glass fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850-7431 PBT, with carbon fiber and glass spheres Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Low warpage.Low waterabsorbtion, for dimensional stable precision parts.Par.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850-7692 PBT, with glass spheres and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850-7692/BK PBT, with glass spheres and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850-7783 PBT, with glass fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850-8197 PBT, lubricant modified, easy flowing, demolding aid Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Parts for electric and electro.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850-8322 PBT, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850/CF/10/GF/10/BK PBT, with carbon fiber and glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Zone 1 | 240 - 260 °C | 464 - 500 °F | |
Lehmann & Voss LUVOCOM® 1850/PL/15/BK PBT, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Parts for electric and electro.. |
|||
Zone 1 | 240 - 290 °C | 464 - 554 °F | |
Solvay Specialty Polymers Hyflon® MFA® F1530 Perfluoropolymer Hyflon® MFA is a family of perfluoro polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistanc.. |
|||
Zone 1 | 240 - 250 °C | 464 - 482 °F | |
Eurostar Star L PA6 30V D31 PA6, Glass Filled, Injection Molding Star L PA6 30V D31 is a Molybdenum Disulfide Lubricated, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 240 - 250 °C | 464 - 482 °F | |
Eurostar Star L PA6 30V D51 PA6, Glass Filled, Injection Molding Star L PA6 30V D51 is a PTFE Lubricated, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 240 - 250 °C | 464 - 482 °F | |
Eurostar Star L PA6 30V D61 PA6, Glass Filled, Injection Molding Star L PA6 30V D61 is a PTFE/Silicone Oil Lubricated, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 240 - 250 °C | 464 - 482 °F | |
Eurostar Starflam BFR552Y3 PA6, Mineral/Glass Fiber Filled, Flame Retardant, Injection Molded Starflam BFR552Y3 is a Halogen and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Mineral Filled, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 240 - 250 °C | 464 - 482 °F | |
Eurostar Starflam PF0023E PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PF0023E is a Mineral Flame Retardant, Halogen Free, Red Phosphorous Free, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 240 - 250 °C | 464 - 482 °F | |
Eurostar Starflam PK0049 PA6, Mineral Fiber Filled, Flame Retardant, Injection Molded Starflam PK0049 is a Free Flame Retardant Mineral Filled Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 240 - 250 °C | 464 - 482 °F | |
Eurostar Starflam PX05003 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PX05003 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 240 - 250 °C | 464 - 482 °F | |
Eurostar Starflam EXCP0132 PA, Mineral Filled, Injection Molding Starflam EXCP0132 is a Halogen Free and Red Phosphorous Free, Mineral Filled, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 240 - 250 °C | 464 - 482 °F | |
Eurostar Starflam PF0069 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PF0069 is a Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 240 °C | 464 °F | Feeding zone |
BASF Ultradur® B 4300 K4 20% Glass Bead Filled PBT Description: Is a PBT + ASA, Injection-molding grades containing 20% of glass beads for industrial parts with low warpage.Applications: Precision parts for optical instruments, fuel tank sensor unit.. |